Effect of down surface energy density on surface roughness and microstructure of pure titanium fabricated by selective laser melting
Source abstract
Abstract
Pure titanium (Ti), known for its exceptional corrosion resistance, high specific strength, and biocompatibility, is increasingly employed in patient-specific biomedical components and aerospace applications. While Selective Laser Melting (SLM) offers superior design flexibility and near-net-shape capabilities for fabricating complex geometries, the process still faces challenges in controlling the surface quality of down surface regions, where incomplete melting, powder adhesion, and steep thermal gradients often result in surface roughness and microstructural heterogeneity. In this study, we investigated the correlation between down surface microstructure and mechanical properties of SLM-fabricated pure Ti as a function of laser power and scan speed across various energy densities, and optimized the down surface process parameters. The results showed that surface roughness deteriorated under high power and high scan speed conditions due to insufficient energy input and rapid solidification. In contrast, an appropriate energy density at low power and low scan speed promoted the formation of a uniform equiaxed microstructure and more consistent surface morphology. The lowest roughness (Ra = 19.88 μm) and highest hardness (242.85 HV) were achieved under the optimal condition of 100 W power and 700 mm/s scan speed. This study confirms that energy-density-based control of process parameters plays a critical role in determining the surface quality and mechanical performance of pure Ti produced by the SLM process, and highlights the importance of process optimization for reducing post-processing requirements and enhancing functional performance.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. A reviwe on biomedical titanium alloys: recent progress and prospect
2. Bioactive Ti metal analogous to human cancellous bone: fabrication by selective laser melting and chemical treatments10.1016/j.actbio.2010.09.034 ↗
3. Reilly, porous titanium for dental implant applications metals10.3390/met5041902 ↗
4. Densification behavior, microstructure evolution, and wear performance of selective laser melting processed commercially pure titanium10.1016/j.actamat.2012.04.006 ↗
5. Effect on microstructural and mechanical properties of selective laser melted pure Ti parts using stress relief heat-treatment process10.1016/j.jmrt.2023.09.288 ↗
6. Mechanical properties of SLM-printed aluminium alloys
7. Metal fabrication by additive manufacturing using laser and electron beam melting technologies10.1016/S1005-0302(12)60016-4 ↗
8. Fabrication of porous pure titanium via selective laser melting under low-energy-density process conditions
9. Surface roughness analysis, modelling and prediction in selective laser melting10.1016/j.jmatprotec.2012.11.011 ↗
10. Joaquim Ciurana, influence of process parameters on surface quality of CoCrMo produced by selective laser melting10.1007/s00170-015-7040-3 ↗
11. Optimized build orientation of additive manufactured parts for improved surface quality and build time
12. Parameter optimization of selective laser melting fabricated titanium alloy using skin-core and triple contour scanning strategy10.2351/7.0000180 ↗
13. Surface quality improvement by parameters analysis, optimization and heat treatment of AlSi10Mg parts manufactured by SLM additive manufacturing
14. CoCr alloy processed by selective laser melting (SLM): effect of laser energy density on microstructure, surface morphology, and hardness10.1016/j.jmapro.2020.01.052 ↗
15. Optimization of selective laser melting process parameters for surface quality performance of the fabricated Ti6Al4V10.1007/s00170-021-06953-3 ↗
16. High-quality surface finishing of industrial three-dimensional metal additive manufacturing using electrochemical polishing
17. Surface quality and material removal in magnetic abrasive finishing of selective laser melted 316L stainless steel10.1016/j.jmapro.2019.07.044 ↗
18. Post-processing of complex SLM parts by barrel finishing10.3390/app10041382 ↗
19. The effect of post-processing operations on surface characteristics of 316L stainless steel produced by selective laser melting
20. Enhancing surface quality of SLM produced AlSi10Mg components through chemical polishing10.1007/s13198-023-02038-4 ↗
21. Effect of processing parameters on overhanging channel forming quality during laser powder bed fusion of AlSi10Mg10.1016/j.jmapro.2023.12.052 ↗
22. Surface roughness improvement of Ti-6Al-4V alloy overhang structures via process optimization for laser-powder bed fusion10.1016/j.jmapro.2024.01.008 ↗
23. Investigation of distortion, porosity and residual stresses in internal channels fabricated in maraging 300 steel by laser powder bed fusion
24. Effects of channel contour laser strategies on fatigue properties and residual stresses of laser powder bed printed maraging stee10.1007/s00170-022-10246-8 ↗
25. Surface quality of the curved overhanging structure manufactured from 316-L stainless steel by SLM
26. Understanding the deformation mechanisms of horizontal internal channels during the LPBF of 18Ni300 maraging steel10.1016/j.jmapro.2021.07.063 ↗
27. On the effect of internal channels and surface roughness on the high-cycle fatigue performance of Ti-6Al-4V processed by SLM10.1016/j.matdes.2018.01.042 ↗
28. Investigation of microstructural and mechanical properties on a pure niobium fabricated by selective laser melting for defect-free process based on the energy density10.1016/j.matlet.2025.138487 ↗
29. Hyung Giun Kim effect of energy density on down surface characteristics of AlSi10Mg alloy fabricated via selective laser melting10.1016/j.heliyon.2024.e39522 ↗
30. Thermal conductivity of Ti-6Al-4V in laser powder bed fusion10.3389/fmech.2022.830104 ↗
31. Thermophysical phenomena in metal additive manufacturing by selective laser melting: fundamentals, modeling, simulation and experimentation
32. Surface roughness of interior fine flow channels in selective laser melted Ti-6Al-4V alloy components10.3390/mi15030348 ↗
33. Microstructural study on a Fe-10Cu alloy fabricated by selective laser melting for defect-free process optimization based on the energy density10.1016/j.jmrt.2020.09.051 ↗
34. Effect of laser power on oxygen and nitrogen concentration of commercially pure titanium manufactured by selective laser melting10.1016/j.matchar.2018.03.003 ↗
35. Recent advance in laser powder bed fusion of Ti–6Al–4V alloys: microstructure, mechanical properties and machinability
36. Analytical modelling of temperature distribution in SLM process with consideration of scan strategy difference between layers10.3390/ma14081869 ↗
37. Elucidation of dross formation in laser powder bed fusion at down-facing surfaces: Phenomenon-oriented multiphysics simulation and experimental validation
38. Effect of scanning strategies on the microstructure and mechanical properties of Ti-22Al-25Nb alloy fabricated through selective laser melting
39. Effect of laser scanning speed on the microstructure and mechanical properties of laser-powder-bed-fused K418 nickel-based alloy10.3390/ma15093045 ↗
40. Influence of the thermal-fluid behavior on the microstructure evolution during the process of selective laser melting of Ti6Al4V10.1016/j.heliyon.2022.e11725 ↗
41. Effects of heat treatment on the microstructure, residual stress, and mechanical properties of Co–Cr alloy fabricated by selective laser melting
42. Manufacture by selective laser melting and mechanical behavior of commercially pure titanium10.1016/j.msea.2013.11.038 ↗
43. Effect of energy density on the microstructure and texture evolution of Ti-6Al-4V manufactured by laser powder bed fusion10.1016/j.matchar.2020.110238 ↗