journal article·2025-03Open access

Study on initial solidification characteristics of high-Mn steel for ultra-low temperature applications

Yin Cui, Changgui Cheng, Yang Li, Liang Liu, Hao Chen

Abstract

The formation of cracks and the breakout of high-Mn steel for ultra-low temperature applications during continuous casting processes negatively affect slab quality. This issue is closely related to the initial solidification behavior of molten steel in the mold. This study investigated the effects of molten steel temperature and the cooling intensity of copper plate on the free deformation of solidified shell using the levitation melting technique. It aims to elucidate the initial solidification characteristics of high-Mn steel for ultra-low temperature applications. The results indicate that the solidified shell exhibits a thin, flaky shape with a slight degree of deformation at lower molten steel temperature and smaller cooling intensity. Conversely, at higher molten steel temperature and greater cooling intensity, the solidified shell exhibits a hemispherical morphology with considerable deformation. Additionally, the heat flux density of the copper plate diminishes as the molten steel temperature increases, while it rises with higher cooling intensity within a specific range. The initial solidification structure of high-Mn steel for ultra-low temperature applications is austenitic, characterized by a high thermal expansion coefficient and low thermal conductivity, resulting in relatively large shrinkage stress and thermal stress on the solidified shell. Furthermore, the wettability of molten steel is generally favorable, and it decreases as the molten steel temperature and cooling intensity increases.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metallurgical Processes and Thermodynamics · Metallurgical and Alloy Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. Study on comprehensive evaluation and countermeasures of natural gas safety in EU10.1016/j.esr.2023.101167 ↗
2. Natural gas industry in China: development situation and prospect10.1016/j.ngib.2020.04.003 ↗
3. Analysis of industrial LNG production technologies10.1007/s10556-022-01036-w ↗
4. Evaluations of energy, exergy, and economic (3E) on a liquefied natural gas (LNG) cold energy utilization system10.1016/j.ijhydene.2024.04.053 ↗
5. A systematic review for sustainability of global liquified natural gas industry: a 10-year update
6. Hydrogen energy, economy and storage: review and recommendation10.1016/j.ijhydene.2019.04.068 ↗
7. On the austenite stability of cryogenic Ni steels: microstructural effects: a review10.1007/s10853-021-06068-w ↗
8. Exploring the improvement of strength and cryogenic impact toughness in hot-rolled high Mn austenitic steel for cryogenic application10.1016/j.jmrt.2022.11.003 ↗
9. Deformation microstructures as well as strengthening and toughening mechanisms of low-density high Mn steels for cryogenic applications10.1016/j.jmrt.2021.05.018 ↗
10. Effects of cooling process on the microstructure and mechanical properties of a novel high-V high-Mn TWIP steel for cryogenic storage tank applications10.1016/j.jmrt.2024.05.003 ↗
11. Temperature dependency of embrittlement resistance of austenitic Fe-24Mn-3Cr-0.5Cu-0.47C steel10.1016/j.msea.2023.145838 ↗
12. Low-temperature tensile and impact properties of hydrogen-charged high-manganese steel10.1016/j.ijhydene.2019.01.065 ↗
13. Effects of Mn and Al contents on cryogenic-temperature tensile and Charpy impact properties in four austenitic high-Mn steels10.1016/j.actamat.2015.08.027 ↗
14. Effects of Ni and Cu addition on cryogenic-temperature tensile and Charpy impact properties in austenitic 22Mn-0.45C-1Al steels10.1016/j.jallcom.2019.152407 ↗
15. Hot tearing of Fe-18Mn-0.6C-2.6Al high manganese steel10.1007/s11663-024-03153-8 ↗
16. Mechanical properties and crack susceptibility of steel during solidification10.1002/srin.199905652 ↗
17. Development of a mold cracking simulator: the study of breakout and crack formation in continuous casting mold10.1007/s11663-016-0705-y ↗
18. Origin of heat transfer anomaly and solidifying shell deformation of peritectic steels in continuous casting10.2355/isijinternational.36.Suppl_S171 ↗
19. Effect of grade on thermal-mechanical behavior of steel during initial solidification10.1007/s11661-017-4112-z ↗
20. Experimental investigation on solidification structure and carbides in continuously cast slab of high manganese steel Mn1310.1007/s11663-022-02596-1 ↗
21. Effect of superheat on the initial solidification behaviors of 3.5 wt pct Si non-oriented electrical steel during strip casting10.1007/s11663-024-03015-3 ↗
22. Effects of manganese content on solidification structures, thermal properties, and phase transformation characteristics in Fe-Mn-Al-C steels10.1007/s11663-015-0330-1 ↗
23. Grain size dependence of twinning behaviors and resultant cryogenic impact toughness in high manganese austenitic steel10.1016/j.jmrt.2020.12.030 ↗
24. Investigation of strand surface defects using mould instrumentation and modelling10.1179/030192304225019261 ↗
25. Numerical simulation of stress field in a wide slab mould of peritectic steel continuous casting
26. Characteristics of slag infiltration in high-Mn steel castings10.1007/s11663-019-01511-5 ↗
27. Evolution of compositions and properties of CaO-SiO2 based mold flux for continuous casting high Mn steel10.2355/isijinternational.ISIJINT-2016-315 ↗
28. Improvement of the initial stage of solidification by using mild cooling mold powder10.2355/isijinternational.37.134 ↗
29. Research on solidification behavior of a high Mn steel during continuous casting based on solidification characteristic unit analysis10.1016/j.matlet.2022.133028 ↗
30. Effect of mold cooling intensity on the depression type crack formation and mold flux infiltration during continuous casting process10.1007/s11663-023-02911-4 ↗
31. High temperature behavior during solidification of peritectic steels under continuous casting conditions
32. Free deformation of initial solidified layer of steel
33. Free deformation and solidification structure of initial solidified shell
34. Deformation and structure difference of steel droplets during initial solidification10.1515/htmp-2016-0113 ↗
35. Free deformation of the initial solid layer of some non-ferrous alloys
36. Direct observation of deformation of shell solidified at melt-chill contact10.2320/matertrans1989.35.196 ↗
37. High-resolution inductive measurement of electrical resistivity and density of electromagnetically levitated liquid metal droplets
38. Transport property measurement of liquid metals and alloys using electromagnetic and electrostatic Levitation
39. Modeling and characterization of surface deformation and current distribution of molten droplets under electromagnetic levitation10.1007/s11663-023-02794-5 ↗
40. Electromagnetic forces and power absorption in levitation melting10.1088/0508-3443/16/5/308 ↗
41. Electromagnetic force calculations for a conical coil10.1007/BF02663134 ↗
42. Crack sensitivity of high-manganese cryogenic steels in initial solidification during continuous casting
43. Effect of surface roughness on contact angle measurement of nanofluid on surface of stainless steel 304 by sessile drop Method
44. Degree of undercooling and wettability behavior of liquid steel on single-crystal Al2O3 and MgO substrate under controlled oxygen partial pressure10.2355/isijinternational.ISIJINT-2015-729 ↗