Pressureless sintering behavior and mechanical properties of ZrB2–SiC composites: effect of SiC content and particle size
Source abstract
Abstract
In the present paper, ZrB2–SiC composites were prepared by pressureless sintering at temperatures of 2000–2200 °C for 1 h under argon atmosphere. In order to prepare composite samples, ZrB2 powder was milled for 2 h, then the reinforcing particles including of micron and nano-sized SiC powder were added. The mixtures were formed and, after the pyrolysis, they were sintered. Densification, microstructural and mechanical properties of ZrB2–SiC composites were investigated. The shrinkage of samples was measured both before and after the sintering, and the microstructure of samples was examined using scanning electron microscopy (SEM), equipped with EDS spectroscopy. Both mass fraction and size of SiC powder have a great effect on relative density, porosity, shrinkage, hardness and microstructure of these composites. The highest relative density and hardness were 98.12% and 15.02 GPa, respectively, in ZrB2–10 wt% SiCnano composite sintered at 2200 °C.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. Processing and properties of ultra-high temperature ceramics for space applications10.1016/j.msea.2007.08.054 ↗
2. Evaluation of ultra-high temperature ceramics for aeropropulsion use10.1016/S0955-2219(02)00140-1 ↗
3. Metallic borides: preparation of solid bodies, sintering methods and properties of solid bodies
4. Activated sintering of zirconium boride
5. Hot-pressing of zirconium diboride–molybdenum disilicide mixtures10.2109/jcersj1950.78.894_64 ↗
6. Effect of thermal exposure on strength of ZrB2-based composites with nano-sized SiC particles10.1016/j.compscitech.2008.06.021 ↗
7. 1990 · 637
8. Effect of SiC content, additives and process parameters on densification and structure–property relations of pressureless sintered ZrB2–SiC composites10.1016/j.ceramint.2012.09.066 ↗
9. Mechanical properties of sintered ZrB2–SiC ceramics10.1016/j.jeurceramsoc.2010.11.013 ↗
10. Microstructure and mechanical properties of ZrB2–SiC composites10.1016/j.matlet.2009.02.054 ↗
11. Densification behavior and microstructure of spark plasma sintered ZrB2-based composites with SiC particles10.1016/j.ceramint.2011.08.003 ↗
12. Influence of nanosized SiC particle on the fracture toughness of ZrB2-based nanocomposite ceramic10.1016/j.msea.2010.01.059 ↗
13. Densification mechanisms during hot pressing of ZrB2–20vol% SiC composite10.1016/j.scriptamat.2013.05.021 ↗
14. Densification of ZrB2-based composites and their mechanical and physical properties: a review10.1016/j.jeurceramsoc.2008.11.008 ↗
15. Pressureless sintering ZrB2–SiC ceramics at low temperatures10.1016/j.matlet.2009.06.041 ↗
16. Microstructure and mechanical properties of ZrB2–SiC nanocomposite ceramic10.1016/j.scriptamat.2009.05.041 ↗
17. Microstructure and densification of ZrB2–SiC composites prepared by spark plasma sintering10.1016/j.jeurceramsoc.2009.01.011 ↗
18. Oxidation behavior of zirconium diboride-silicon carbide at 1800°C10.1016/j.scriptamat.2007.07.009 ↗
19. Oxidation-resistant ZrB2–SiC composites at 2200°C10.1016/j.compscitech.2007.08.017 ↗
20. Improved processing and oxidation-resistance of ZrB2 ultra-high temperature ceramics containing SiC nanodispersoids10.1016/j.msea.2007.03.002 ↗
21. Boride-based hard materials
22. Phase equilibria in the system Zr–W–C10.1007/BF00777011 ↗