Effect of ionic plasma nitriding process on the corrosion and micro-abrasive wear behavior of AISI 316L austenitic and AISI 470 super-ferritic stainless steels
Source abstract
Abstract
The aim of this work was to study the influence of thermochemical treatment of ionic plasma nitriding on the resistance to micro-abrasive wear and to the corrosion process of AISI 316L and AISI 470 stainless steels. The thermochemical treatment was performed at different times and temperatures with a gas mixture of 25% H2 and 75% N2. The treated materials were characterized by using optical microscopy (OM), scanning electron microscopy (SEM), X-ray diffraction (XRD), microhardness tests, micro-abrasive wear tests (MAWTs) and corrosion tests. The results show an increase in the thickness of the layer formed by increasing treatment time and in the wear resistance of the materials studied. Temperatures exceeding 450 °C favor the formation chromium nitrides, which, for being very hard broke making the formed layer brittle decreasing the wear resistance of the material. In addition, the formation of these phases substantially decrease the corrosion resistance of stainless steels.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. 2005 · vol. 1
2. 1994
3. Glow-discharge nitriding of AISI 316L austenitic stainless steel: influence of treatment temperature10.1016/j.surfcoat.2004.07.110 ↗
4. On the formation of expanded austenite during plasma nitriding of an AISI 316L austenitic stainless steel10.1016/j.surfcoat.2006.08.060 ↗
5. Manfrintao · 2006
6. Wear and corrosion study of plasma nitriding F53 super duplex stainless steel10.1590/1980-5373-mr-2015-0656 ↗
7. Surface modification of ferritic stainless steel by active screen plasma nitriding
8. 2014
9. Friction characteristics of nitride layers on AISI 430 ferritic stainless steel obtained by various nitriding processes
10. Cathodic cage nitriding of AISI 409 ferritic stainless steel with the addition of CH410.1590/S1516-14392012005000016 ↗
11. Desenvolvimento de dispositivo e estudo do comportamento ao microdesgaste abrasivo do aço AISI 420 temperado e revenido
12. A micro-abrasive wear test with particular application to coated systems10.1016/0257-8972(95)02461-1 ↗
13. Plasma nitriding of Al alloys by DC glow discharge10.1016/j.surfcoat.2005.12.002 ↗
14. Projeto, construção e comissionamento de um reator para tratamento de nitretação iônica a plasma em aço P20
15. Oliveira · 2005
16. Askeland · 2015
17. Diffusion behavior of carbon and its hardening effect on plasma carburized M50NiL steel: influence of treatment temperature and duration10.1016/j.surfcoat.2017.10.068 ↗
18. Micro abrasive wear behaviour study of carburization and ion plasma nitriding of P20 steel10.1590/1980-5373-MR-2015-0721 ↗
19. Marinho · 2003
20. Decreasing chromium precipitation in AISI 304 stainless steel during the plasma-nitriding process10.1016/S0257-8972(99)00506-X ↗
21. Influência da temperatura de nitretação a plasma na espessura e resistência ao desgaste de camadas de austenita expandida formadas em aço inoxidável AISI 316L
22. On the crystallography structure of S phase10.1016/j.scriptamat.2003.09.042 ↗
23. On the significance of H/E ratio in wear control: a nanocomposite coating approach to optimized tribological behaviour10.1016/S0043-1648(00)00488-9 ↗
24. Estrutura e propriedades do aço inoxidável austenítico AISI 316L Grau ASTM F138 nitretado sob plasma à baixa temperatura10.1590/S0370-44672010000100023 ↗
25. Tratamento térmico e superficial do aço inoxidável martensítico AISI 420 destinado a moldes para injeção de polímeros parte I: tratamento térmico
26. Tribological properties of SiNx films on PH stainless steel with and without nitriding a pre-treatment10.1016/j.mspro.2012.06.042 ↗
27. Study of the steady state of wear in micro-abrasive wear testes by rotative ball conducted on specimen of WC–Co P20 and M2 tool-steel