Effect of Mn addition on Fe-rich intermetallics morphology and dry sliding wear investigation of hypereutectic Al-17.5%Si alloys
Source abstract
Abstract
The effect of Manganese addition on the iron-rich intermetallics and wear behavior of Al-17.5%Si hypereutectic alloys has been studied. Dry sliding wear tests have been conducted using a pin-on-disk machine under different normal loads of 18, 51, 74 and 100 N and at a constant sliding speed of 0.3 m/s. The addition of 1.2 wt.% Fe to the base alloy increased the wear rate due to the formation of needle beta intermetallics. Introducing 0.6 wt.% Mn to the iron-rich alloy changed the beta intermetallics into the modified alpha phases, and therefore reduced the detrimental effect of iron. Mn addition up to 0.9 wt.% to the 1.8Fe alloy did not impede formation of needle-like intermetallic compounds and had no positive effect on the modification of microstructure.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Henry · 1992 · vol. 18
2. Wear in Al-Si alloys under dry sliding conditions10.1016/0043-1648(87)90102-5 ↗
3. Warmuzek · 2004
4. Role of silicon in resisting subsurface plastic deformation in tribology of aluminium–silicon alloys10.1016/j.triboint.2009.06.020 ↗
5. Influence of iron on castability and properties of aluminium silicon alloys: literature review10.1080/13640461.2003.11819622 ↗
6. Gruzleski · 1990
7. Wang · 1993
8. Intermetallic compound formation in Fe–Al–Si ternary system: Part I10.1016/S1044-5803(03)00006-8 ↗
9. Effect of element additions on wear property of eutectic aluminium–silicon alloys10.1016/0043-1648(95)06707-8 ↗
10. Assessment of modification and formation of intermetallic compounds in aluminum alloy using thermal analysis10.1016/j.msea.2007.05.022 ↗
11. Mondolfo · 1978
12. An overview of the development of Al–Si-Alloy based material for engine applications10.1361/105994903770343132 ↗
13. The formation of β-Fe-SiAl5, and Be–Fe phases in Al-7Si-0.3Mg alloy containing Be10.1016/0921-5093(94)09602-S ↗
14. Electron microscope study of Al–Fe–Si intermetallics in 6201 aluminum alloy10.1007/BF02649760 ↗
15. Effect of Mn and Sr on intermetallics in Fe-rich eutectic Al–Si alloy10.1080/13640461.2002.11819459 ↗
16. Effect of iron-rich intermetallics on the sliding wear behavior of Al–Si alloys10.1016/j.msea.2008.01.001 ↗
17. Effect of Fe-rich intermetallics on the wear beheaviour of eutectic Al–Si piston alloy (LM13)10.1016/j.matdes.2010.02.015 ↗
18. Intermetallic compound formation in Fe–Al–Si turnery system: part II10.1016/S1044-5803(03)00005-6 ↗
19. Effect of metallurgical parameters on the hardness and microstructural characterization of as-cast and heat-treated 356 and 319 aluminum alloys10.1016/j.msea.2006.08.054 ↗
20. Chemical inhomogeneity of intermetallic phases precipitates formed during solidification of Al–Si alloys10.1016/j.matchar.2004.10.001 ↗
21. The effect of iron and manganese on the formation of intermetallic compounds in Al–Si alloys10.1016/S0921-5093(04)00832-9 ↗
22. Effect of microstructure on the oxidative wear behaviour of plain carbon Steel10.1016/j.wear.2006.11.009 ↗
23. An investigation of the wear behaviour of 0.2% C dual phase steels10.1016/j.jmatprotec.2007.09.044 ↗
24. The effect of solidification condition and chemistry on the formation and morpholgy of complex intermetallic compounds in aluminum–silicon alloys10.1080/09534962.1994.11819153 ↗
25. Belov · 2002
26. Modification of Fe-containing intermetallic compounds by K addition to Fe-rich AA319 aluminum alloys10.2320/matertrans.44.2611 ↗
27. Modification of microstructure and mechanical property of hypereutectic Al–Si alloy by laser surface remelting10.2464/jilm.50.609 ↗
28. Effect of precipitation and sedimentation of primary α-phase on liquid metal quality of cast Al-11.1Si-0.4Mg alloy10.1179/136404604225014792 ↗
29. Hutchings · 1992