journal article·2020-07Open access

Surface characteristics and corrosion behavior of TC11 titanium alloy strengthened by ultrasonic roller burnishing at room and medium temperature

Hao Su, Xuehui Shen, Chonghai Xu, Jianqun He, Baolin Wang, Guosheng Su

Abstract

A roller tip was utilized in a set of self-fabricated ultrasonic burnishing equipment. Ultrasonic roller burnishing with/without heat treatment was proposed and investigated in the surface strengthening of TC11 titanium alloy material. Experimental research together with finite element analysis were carried out to perform the study. Three treatments, including conventional turning, ultrasonic roller burnishing at ambient temperature (URB) and ultrasonic roller burnishing at medium temperature (URB/HT), were comparatively evaluated in term of surface integrity and corrosion resistance of the treated sample. As a result, compared with URB, the surface of TC11 alloy treated by URB/HT had better surface finishing, which significantly improved corrosion resistance, and thus the surface of TC11 alloy was strengthened. The good performance of URB/HT was attributed to the combined effect of the high frequency dynamic impact from URB and the thermoplastic effect of the heat treatment. Owing to the excitation of the ultrasonic vibration during URB, an oscillating stress wave formed and propagated deep inside the being treated material, and the heat treatment in URB/HT case was supposed to accelerate this sort of stress propagation. Meanwhile, both the heat treatment and the dynamic oscillating stress wave facilitated the deformation of the surface layer.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Surface Treatment and Residual Stress · Erosion and Abrasive Machining · Ultrasound and Cavitation Phenomena

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Tensile creep behavior of heat-treated TC11 titanium alloy at 450–550 ℃10.1016/j.msea.2013.03.038 ↗
2. Deformation behavior in isothermal compression of the TC11 titanium alloy10.1016/j.matdes.2009.12.051 ↗
3. Microstructure characterization and thermal stability of TC11/Ti2AlNb joints during thermal exposure10.1016/j.matchar.2018.09.015 ↗
4. Hot corrosion behavior of TC11 titanium alloy treated by laser shock processing10.1016/j.apsusc.2013.07.017 ↗
5. Effect study and application to improve high cycle fatigue resistance of TC11 titanium alloy by laser shock peening with multiple impacts10.1016/j.surfcoat.2014.05.015 ↗
6. Effect of laser shock peening on microstructure and hot corrosion of TC11 alloy10.1016/j.surfcoat.2017.12.003 ↗
7. Surface modification of TC4 titanium alloy by high current pulsed electron beam (HCPEB) with different pulsed energy densities10.1016/j.jallcom.2013.04.002 ↗
8. Compressive residual stress into titanium alloy using cavitation shotless peening method10.1023/B:TRIL.0000044497.45014.f2 ↗
9. Evaluation of microstructure variation of TC11 alloy after electroshocking treatment10.1016/j.jmrt.2019.12.076 ↗
10. Gradient crystalline structure induced by ultrasonic impacting and rolling and its effect on fatigue behavior of TC11 titanium alloy10.1016/j.rinp.2017.05.026 ↗
11. The compound process of laser shock peening and vibratory finishing and its effect on fatigue strength of Ti-3.5Mo-6.5Al-1.5Zr-0.25Si titanium alloy10.1016/j.jallcom.2018.12.294 ↗
12. Hot tensile characterization of Ti-6.5 Al-3.5 Mo-1.5 Zr-0.3 Si alloy with an equiaxed microstructure10.1016/j.matdes.2008.05.077 ↗
13. Influence of gradient heat treatment on microstructure and microhardness in weld seam of Ti3Al/TC11 dual alloys10.1016/S1875-5372(10)60075-6 ↗
14. Mechanical and electrochemical properties of Zr and Zr–Er alloyed layers deposited on titanium alloy (TC11)10.1016/j.surfcoat.2015.09.031 ↗
15. Effects of the different frequencies and loads of ultrasonic surface rolling on surface mechanical properties and fretting wear resistance of HIP Ti–6Al–4V alloy10.1016/j.apsusc.2016.07.120 ↗
16. Wear resistance enhancement of titanium alloy (Ti–6Al–4V) by ball burnishing process10.1016/j.jmrt.2016.03.007 ↗
17. Characterization of hot deformation microstructures of alpha-beta titanium alloy with equiaxed structure10.1016/S1003-6326(11)61205-3 ↗
18. Johnson–Cook constitutive equation for titanium alloy TC1110.4028/www.scientific.net/KEM.589-590.140 ↗
19. Simulation of shot dynamics for ultrasonic shot peening: effects of process parameters10.1016/j.ijmecsci.2014.03.006 ↗
20. A new formula for the breadth of debye scherrer lines10.1016/S0031-8914(42)80059-2 ↗
21. Manufacturing of nanostructured titanium Grade2 using caliber rolling
22. Gradient nanostructure evolution and phase transformation of α phase in Ti-6Al-4V alloy induced by ultrasonic surface rolling process
23. Face-centered titanium induced by ultrasonic surface rolling process in Ti-6Al-4V alloy and its tensile behavior10.1016/j.matchar.2018.09.004 ↗
24. Precipitation behavior and grain refinement of burnishing Al–Zn–Mg alloy10.1016/j.pnsc.2017.11.006 ↗
25. Minimum necessary strain to induce tangled dislocation to form cell and grain boundaries in a 6N–Al
26. New insight on acoustoplasticity- ultrasonic irradiation enhances subgrain formation during deformation10.1016/j.ijplas.2010.09.007 ↗
27. Spectral response of polarization properties of fiber Bragg grating under local pressure10.1016/j.yofte.2015.07.003 ↗
28. Tribological behavior of UHMWPE against TiAl6V4 and CoCr28Mo alloys under dry and lubricated conditions10.1016/j.jmbbm.2016.07.002 ↗
29. The influence of initial roughness and circular axial run-out on friction and wear behavior of Si3N4–Al2O3 sliding in water10.1016/j.triboint.2016.04.005 ↗
30. Fatigue properties of a S45C steel subjected to ultrasonic nanocrystal surface modification10.1016/j.apsusc.2010.04.007 ↗
31. Plastic flow behavior for machined surface material Ti-6Al-4V with rotary ultrasonic burnishing10.1016/j.jmrt.2019.12.071 ↗
32. Effects of ball burnishing parameters on surface finish—a literature survey and discussion10.1016/0141-6359(88)90056-6 ↗
33. The evaluation of the micro-tracks and micro-dimples on the tribological characteristics of thrust ball bearings10.1166/jnn.2011.3289 ↗
34. Topological surface integrity modification of AISI 1038 alloy after vibration-assisted ball burnishing10.1016/j.surfcoat.2018.05.061 ↗
35. Effects of the different frequencies and loads of ultrasonic surface rolling on surface mechanical properties and fretting wear resistance of HIP Ti–6Al–4V alloy10.1016/j.apsusc.2016.07.120 ↗
36. Evaluation of optimized surface properties and residual stress in ultrasonic assisted ball burnishing of AA6061-T610.1016/j.measurement.2017.11.001 ↗
37. An investigation of stress condition in vibration-assisted burnishing10.1007/s00170-019-04128-9 ↗
38. Fretting wear and friction reduction of CP titanium and Ti-6Al-4V alloy by ultrasonic nanocrystalline surface modification10.1016/j.surfcoat.2012.06.046 ↗
39. Fatigue properties of nanocrystallized surfaces obtained by high energy shot peening10.1016/j.proeng.2010.03.181 ↗
40. Microstructural evolution and surface properties of nanostructured Cu-based alloy by ultrasonic nanocrystalline surface modification technique10.1016/j.apsusc.2016.01.237 ↗
41. Topological surface integrity modification of AISI 1038 alloy after vibration-assisted ball burnishing10.1016/j.surfcoat.2018.05.061 ↗
42. Local heat treatment with and without ultrasonic nanocrystal surface modification of Ti-6Al-4V alloy: mechanical and tribological properties10.1016/j.surfcoat.2017.07.064 ↗
43. Influence of surface morphology on corrosion and electronic behavior10.1016/j.actamat.2005.09.017 ↗
44. Ultrafine-grained surface layer on Mg–Al–Zn alloy produced by cryogenic burnishing for enhanced corrosion resistance10.1016/j.scriptamat.2011.06.013 ↗
45. Enhanced pitting corrosion resistance of 304 SS in 3.5 wt% NaCl by ultrasonic nanocrystal surface modification10.1149/2.1781712jes ↗
46. Roles of compressive residual stress in enhancing the corrosion resistance of nano nitride composite coatings on steel10.1016/j.jascer.2013.03.002 ↗
47. Effects of surface mechanical attrition treatment and spot peening on corrosion behavior of commercial pure titanium
48. Effect of surface mechanical attrition treatment on corrosion resistance of commercial pure titanium10.1016/j.surfcoat.2015.08.041 ↗
49. In situ hydrothermal synthesis of oxide film on NiTi for improving corrosion resistance in Hanks’ solution10.1016/j.scriptamat.2006.10.014 ↗
50. Graphical analysis of electrochemical impedance spectroscopy data in Bode and Nyquist representations10.1016/j.jpowsour.2016.01.073 ↗