journal article·2019-09Open access

Optimized mix design for 180 MPa ultra-high-strength concrete

Hyun-Oh Shin, Doo-Yeol Yoo, Joo-Ha Lee, Seung-Hoon Lee, Young-Soo Yoon

Abstract

This study aims to optimize the proportion and constituents of the mixture used for fabricating 180 MPa ultra-high-strength concrete (UHSC) including coarse aggregate. Various parameters, such as the supplementary cementitious material (SCM) type and amount, water–binder (W/B) ratio, fine and coarse aggregate type and amount, chemical admixture, and mixing process, were considered and their effect on the compressive strength was examined. Based on several experimental tests, the optimized SCM proportions for cement, silica fume (SF), ground-granulated blast furnace slag (BFS), and gypsum are 55%, 20%, 20%, and 5%, respectively. The most appropriate W/B ratio, unit water content, and sand–total aggregate (S/a) ratio are 12.5%, 150 kg/m3, and 0.35, respectively. The use of very fine SF with a specific surface area of 13.7 m2/g and diorite, which is a type of coarse aggregate, improves the compressive strength of UHSC. The optimum amount of superplasticizer ranges between 1.3% and 1.6% and the most suitable slump flow is 750 mm. Finally, for this type of flowable UHSC, a mixing time and speed of 5 min and 40 rpm, respectively, and natural self-compacting without using a tamping bar are recommended. Based on the optimized mix design, UHSC with a compressive strength of 180 MPa can be certainly fabricated. Keywords: Ultra-high-strength concrete, Compressive strength, Supplementary cementitious materials, Self-compaction, Optimum mix design
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Innovative concrete reinforcement materials · Concrete and Cement Materials Research · Structural Behavior of Reinforced Concrete

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Workability, testing, and performance of self-consolidating concrete
2. Seismic behavior of 200MPa ultrahigh-strength steel-fiber reinforced concrete columns under varying axial load10.3151/jact.5.193 ↗
3. Stress distribution and crack formation in full-scaled ultra-high strength concrete columns10.1617/s11527-012-9873-7 ↗
4. Impact response of ultra-high-strength fiber-reinforced cement composite
5. The effect of heat treatment on the salt freeze-thaw durability of UHSC
6. Fire resistance of hybrid fibre-reinforced, ultrahigh-strength concrete columns with compressive strength from 120 to 200MPa10.1680/macr.11.00034 ↗
7. Axial load response of ultra-high-strength concrete columns and high-strength reinforcement
8. Autogenous shrinkage of concrete with design strength 60–120N/mm210.1680/macr.2011.63.10.751 ↗
9. Shrinkage of fiber-reinforced ultrahigh strength concrete10.1061/(ASCE)MT.1943-5533.0000420 ↗
10. KS · 2014
11. KS · 2014
12. Lee · 2013 · 198
13. ASTM C1611/C1611M · 2014
14. ASTM C 39/C39M · 2014
15. Neville · 2002
16. Use of waste gypsum to replace natural gypsum as set retarders in Portland cement10.1016/j.wasman.2008.11.014 ↗
17. A comparison of the performance of various synthetic gypsums in plant trials during the manufacturing of OPC clinker10.1016/j.cemconres.2004.04.002 ↗
18. Effect of protogenetic anhydrite on the hydration of cement under different curing temperature10.1016/j.conbuildmat.2017.03.064 ↗
19. Reactivity and self-hardening of fly ash from the fluidized bed combustion of wood and peat10.1016/j.fuel.2014.06.029 ↗
20. Pore structure of concrete with mineral admixtures and its effect on self-desiccation shrinkage
21. Properties of tungsten mine waste geopolymeric binder10.1016/j.conbuildmat.2007.01.022 ↗
22. Electrical and self-sensing properties of ultra-high-performance fiber-reinforced concrete with carbon nanotubes10.3390/s17112481 ↗
23. Shrinkage cracking of high-strength concrete
24. ASTM C1437-07 · 2007
25. ASTM C1749-17a · 2017
26. Bache · 1987 · 87
27. Hydration kinetics, change of relative humidity, and autogenous shrinkage of ultra-high-strength concrete10.1016/S0008-8846(99)00022-8 ↗
28. The hydration and microstructure of ultra high-strength concrete with cement–silica fume–slag binder10.1016/j.cemconcomp.2015.04.013 ↗
29. Effect of material constituents and mix design on performance of SCC for precast, prestressed girders
30. Effect of mixture design parameters on segregation of self-consolidating concrete
31. Influence of nano-and micro-silica additions on the durability of a high-performance self-compacting concrete10.1016/j.conbuildmat.2017.12.100 ↗
32. Production of high-strength concrete using high volume of industrial by-products10.1016/j.conbuildmat.2010.01.016 ↗
33. Electric arc furnace slag in concrete10.1061/(ASCE)0899-1561(2004)16:6(639) ↗