The effect of strain rate on stress corrosion performance of Ti6Al4V alloy produced by additive manufacturing process
Source abstract
Abstract
Ti6Al4V alloy is considered as a favourable material for additive manufacturing (AM) and in particular for selective laser melting (SLM), due to the inherent difficulties relating to casting and plastic forming of this alloy. However, the significantly increased solidification rate associated with the SLM process results in a modified micro-structure and inherent casting imperfections that can have a detrimental effect on the alloy stress corrosion performance. The main objective of this study was to evaluate the effect of strain rate on stress corrosion behavior of Ti6Al4V alloy produced by SLM, as compared to its wrought alloy (Grade 5) counterpart of the same chemical composition. Micro-structure and phase identification were examined by scanning electron microscopy and X-ray diffraction analysis. General corrosion resistance was evaluated in terms of open circuit potential, potentiodynamic polarization analysis and by impedance spectroscopy, while stress corrosion behavior was examined at various strain rates in a 3.5% NaCl solution at ambient temperature. The results obtained revealed that general corrosion resistance and stress corrosion endurance at slow strain rate, in terms of time to failure and ductility of the SLM alloy, were relatively reduced, as compared to the wrought alloy counterpart. This was mainly due to the formation of a strained martensitic matrix in the form of α' phase and the significant reduction of the β phase in the alloy produced by SLM process.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Time-dependent enhanced corrosion of Ti6Al4V in the presence of H 2 O 2 and albumin
2. Sliding wear behavior of Ti6Al4V implant alloy in the simulated body environment
3. Characterization of titanium alloy Ti-6Al-4V for chemical, marine and industrial applications10.1016/j.matchar.2003.10.006 ↗
4. Tracking microstructure, texture and boundary misorientation evolution of hot deformed and post-deformation annealed Ti-6Al-4V alloy10.1016/j.msea.2015.09.060 ↗
5. A study of the microstructural evolution during selective laser melting of Ti-6Al-4V10.1016/j.actamat.2010.02.004 ↗
6. Selective laser melting of titanium alloys and titanium matrix composites for biomedical applications: a review10.1002/adem.201500419 ↗
7. Corrosion behavior of AlSi10Mg alloy produced by additive manufacturing (AM) vs. Its counterpart gravity cast alloy10.3390/met6070148 ↗
8. Effect of surface roughness on corrosion fatigue performance of AlSi10Mg alloy produced by selective laser melting (SLM)10.1016/j.matchar.2017.06.029 ↗
9. Review of selective laser melting: materials and applications10.1063/1.4935926 ↗
10. Formation and control of martensite in Ti-6Al-4V alloy produced by selective laser melting10.1016/j.matdes.2016.06.117 ↗
11. Inducing stable α + β microstructures during selective laser melting of Ti-6Al-4V using intensified intrinsic heat treatments10.3390/ma10030268 ↗
12. Corrosion behavior of nano/sub-micron F401 titanium alloy10.1002/adem.201400147 ↗
13. NaCl induced corrosion of Ti-6Al-4V alloy at high temperature10.1016/j.corsci.2016.04.016 ↗
14. Corrosion behavior of Ti-8Al-1Mo-1V alloy compared to Ti-6Al-4V10.1016/j.matdes.2010.09.009 ↗
15. Corrosion resistance characteristics of a Ti-6Al-4V alloy scaffold that is fabricated by electron beam melting and selective laser melting for implantation in vivo10.1016/j.msec.2016.07.045 ↗
16. Corrosion behavior of selective laser melted Ti-6Al-4V alloy in NaCl solution10.1016/j.corsci.2015.10.041 ↗
17. Anisotropic response of Ti-6Al-4V alloy fabricated by 3D printing selective laser melting10.1016/j.msea.2016.11.061 ↗
18. The relationship between crystallographic texture and salt water cracking susceptibility in Ti-6A1-4V10.1016/0921-5093(95)09820-8 ↗
19. The mechanism of aqueous stress-corrosion cracking of α + β titanium alloys10.1016/j.corsci.2017.05.025 ↗
20. Selective laser melting of Ti6Al4V alloy for biomedical applications: temperature monitoring and microstructural evolution10.1016/j.jallcom.2013.08.183 ↗
21. Effects of annealing temperature and quenching medium on microstructure, mechanical properties as well as fatigue behavior of Ti-6Al-4V alloy10.1016/j.msea.2016.11.095 ↗
22. In situ observation of texture and microstructure evolution during rolling and globularization of Ti-6Al-4V10.1016/j.actamat.2012.11.037 ↗
23. A study of the microstructures and mechanical properties of Ti6Al4V fabricated by SLM under vacuum10.1016/j.msea.2018.03.021 ↗
24. Additive manufacturing of strong and ductile Ti-6Al-4V by selective laser melting via in situ martensite decomposition10.1016/j.actamat.2014.11.028 ↗
25. On the texture formation of selective laser melted Ti-6Al-4V10.1007/s11661-014-2218-0 ↗
26. Corrosion behaviour of hot-pressed austenitic stainless steel in H2SO4 solutions at room temperature10.1016/0010-938X(83)90090-2 ↗
27. An anodic behaviour study of an analogical sintered system of austenitic stainless steel in H2SO4 solution10.1016/0010-938X(84)90043-X ↗
28. Corrosion behavior of additive manufactured Ti-6Al-4V alloy in NaCl solution10.1007/s11661-017-4087-9 ↗
29. Passivity breakdown of 316L stainless steel during potentiodynamic polarization in NaCl solution10.1016/j.corsci.2016.06.011 ↗
30. Susceptibility of Ti-6Al-4V alloy to stress corrosion cracking in a Lewis-neutral aluminium chloride-1-ethyl-3-methylimidazolium chloride ionic liquid10.1016/j.corsci.2013.07.009 ↗
31. Distinction in corrosion resistance of selective laser melted Ti-6Al-4V alloy on different planes10.1016/j.corsci.2016.06.009 ↗
32. Corrosion characterization of titanium alloys by electrochemical techniques10.1016/j.electacta.2005.02.121 ↗
33. Investigation about the stress corrosion cracking of TI-6AL-4V
34. Basic mechanisms of stress-corrosion cracking of titanium
35. Improved stress corrosion cracking resistance of a novel biodegradable EW62 magnesium alloy by rapid solidification, in simulated electrolytes10.1016/j.msec.2015.03.001 ↗
36. Stress corrosion cracking of nano/sub-micron E906 magnesium alloy10.1002/adem.200800031 ↗
37. Effect of long term exposure and hydrogen effects on HSSCC behaviour of titanium alloy IMI 83410.1016/j.matdes.2015.08.002 ↗
38. Deformation behavior and microstructure of Ti6Al4V manufactured by SLM10.1016/j.phpro.2016.08.080 ↗
39. Mechanistic and fractographic aspects of stress corrosion cracking10.1515/corrrev-2012-0501 ↗
40. Revie · 2000
41. Evaluation of residual stress in stainless steel 316L and Ti6Al4V samples produced by selective laser melting10.1080/17452759.2015.1026045 ↗
42. Stress corrosion cracking (SCC) in aerospace vehicles10.1533/9780857093769.4.608 ↗
43. Effect of heat treatment on stress corrosion cracking behavior and electrochemical characteristic of welded Ti-6Al- 4V alloy during slow strain rate test10.20964/2016.12.75 ↗