Influence of seawater absorption on vibrational and tensile characteristics of quasi-isotropic glass/epoxy composites
Source abstract
Abstract
Glass fibre reinforced composites are common structural materials in civil engineering and marine applications. Exposure to moisture is the key challenge for using fibre-reinforced composites in marine structures. This study focuses on preparation of quasi-isotropic E-glass/epoxy laminates with stacking sequence [0°/90°/+45°/−45°] s fabricated using vacuum bagging technique. Ageing studies in artificial seawater was conducted in sub-zero and ambient temperatures for a duration of 3600 h. Moisture absorption behaviour, variation of damping, stiffness properties , and microstructural failure analysis studies were carried out as per ASTM standards. Results indicate that the rate of moisture absorption depends on ageing temperature. In the current study, it is observed that composites aged in ambient temperature absorbed higher amount of moisture than sub-zero temperature aged specimen . Moisture absorption reduced stiffness and natural frequency of quasi-isotropic laminates.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Mechanical Behavior of Composites · Structural Analysis of Composite Materials · Composite Structure Analysis and Optimization
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Peter Davies · 2003 · vol. 19, no. 1/2
2. Effects of sea water environment on glass fiber reinforced plastic materials used for marine civil engineering constructions10.1016/j.matdes.2014.10.032 ↗
3. Influence of seawater absorption on the vibration damping characteristics and fracture behaviors of basalt/CNT/epoxy multiscale composites10.1016/j.compositesb.2014.03.010 ↗
4. Durability and prediction models of fiber-reinforced polymer composites under various environmental conditions: a critical review10.1177/0731684415610920 ↗
5. Modeling the transport of low-molecular-weight penetrants within polymer matrix composites10.1115/1.2202873 ↗
6. Moisture absorption and desorption of composite materials10.1177/002199837601000101 ↗
7. Seawater durability of glass- and carbon-polymer composites10.1016/j.compscitech.2003.10.019 ↗
8. Mallick · 2009 · vol. 76, no. 6
9. Standard for the preparation of substitute ocean water
10. Thermomechanical and hygroelastic properties of an epoxy system under humid and cold-warm cycling conditions10.1016/j.polymdegradstab.2013.11.011 ↗
11. Effect of laminate thickness on moisture diffusion of polymer matrix composites in artificial seawater ageing10.1007/s11706-012-0177-1 ↗
12. ASTM D 3039M – standard test method for tensile properties of polymer matrix composite materials
13. Standard test method for measuring vibration-damping properties of materials
14. Free vibration and damping characteristics of GFRP and BFRP laminated composites at various boundary conditions10.17485/ijst/2015/v8i12/54208 ↗
15. Failure of quasi-isotropic composite laminates with free edges10.1177/073168448800700602 ↗
16. Effect of harsh environmental conditions on the tensile properties of GFRP bars10.1016/j.compositesb.2012.05.004 ↗
17. Carbon nanofiber reinforced syntactic foams: degradation mechanism for long term moisture exposure and residual compressive properties10.1016/j.polymdegradstab.2013.07.007 ↗
18. Vibration characteristics of glass fabric/epoxy composites with different woven structures10.1177/0021998310377943 ↗
19. Damping studies in fiber-reinforced composites – a review10.1016/S0263-8223(99)00041-0 ↗