Formation of equiaxed grains in selective laser melted pure titanium during annealing
Source abstract
Abstract
Commercially pure titanium (CP-Ti) has seen major applications in biomedical equipment. The use of selective laser melting (SLM) has become more common concerning the fabrication of CP-Ti components with a complicated shape in biomedical implants, where high strength and ductility are required. However, SLM manufactured CP-Ti often exhibits high strength and low ductility, as well as mechanical anisotropy because SLM process typically results in the formation of long columnar grains comprising of fine acicular α′ martensite. Heat treatment must be preceded to transform the acicular α′ to equiaxed α grain. This study demonstrated that annealing at 650 °C of SLM CP-Ti can create an equiaxed structure, resulting in a weakened texture. The formation of equiaxed grains occurred at two types of microstructural features, acicular α′ and irregular massive (α′m) martensite, which exhibited different sizes, morphologies, and contained different types of substructures under SLM as-fabricated condition. The formation mechanism of equiaxed grains in the α′ region is dominated by the coalescence of acicular α′ of the same variant and the dissolution of α′ into the matrix, whereas the formation mechanism in the α′m region is primarily dominated by the growth of the preexisting subgrains. A small number of equiaxed grains with new orientations were formed in the α′m region. The majority of equiaxed grains were formed in the acicular α′ region and inherited the grain orientations of the preexisting α′ or matrix. Therefore, a similar but weakened texture was inherited from the microstructure of the SLM CP-Ti after annealing.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (53)
Show source-provided references
1. Perspectives on titanium science and technology10.1016/j.actamat.2012.10.043 ↗
2. A review on biomedical titanium alloys: recent progress and prospect10.1002/adem.201801215 ↗
3. Corrosion resistance and antibacterial activity of different zones in TA2 weldment by TIG welding10.1007/s12598-014-0395-z ↗
4. Martensitic transformation, shape memory effect and superelasticity of Ti–xZr–(30–x)Nb–4Ta alloys10.1007/s12598-019-01305-3 ↗
5. Preparation of Ti–Nb–Ta–Zr alloys for load-bearing biomedical applications10.1007/s12598-019-01239-w ↗
6. Manufacture by selective laser melting and mechanical behavior of a biomedical Ti–24Nb–4Zr–8Sn alloy10.1016/j.scriptamat.2011.03.024 ↗
7. Microstructural homogeneity and mechanical behavior of a selective laser melted Ti-35Nb alloy produced from an elemental powder mixture10.1016/j.jmst.2020.05.052 ↗
8. Mechanical behavior and phase transformation of β-type Ti-35Nb-2Ta-3Zr alloy fabricated by 3D-Printing10.1016/j.jallcom.2019.03.138 ↗
9. Superelastic response of low-modulus porous beta-type Ti-35Nb-2Ta-3Zr alloy fabricated by laser powder bed fusion
10. Transformation-induced plasticity and high strength in beta titanium alloy manufactured by selective laser melting10.1016/j.mtla.2019.100299 ↗
11. Densification behavior, microstructure evolution, and wear performance of selective laser melting processed commercially pure titanium10.1016/j.actamat.2012.04.006 ↗
12. Thermal behavior during selective laser melting of commercially pure titanium powder: numerical simulation and experimental study
13. Manufacture by selective laser melting and mechanical behavior of commercially pure titanium10.1016/j.msea.2013.11.038 ↗
14. Microstructure and mechanical properties investigation of CP titanium processed by selective laser melting (SLM)10.1016/j.jmatprotec.2016.10.022 ↗
15. Selective laser melting of weak-textured commercially pure titanium with high strength and ductility: a study from laser power perspective10.1016/j.matdes.2016.12.019 ↗
16. On the texture, phase and tensile properties of commercially pure Ti produced via selective laser melting assisted by static magnetic field10.1016/j.msec.2016.09.011 ↗
17. Comparative study of commercially pure titanium produced by laser engineered net shaping, selective laser melting and casting processes10.1016/j.msea.2017.08.103 ↗
18. Preparation of weak-textured commercially pure titanium by electron beam melting
19. Effect of cyclic heat treatment on commercially pure titanium part fabricated by electron beam additive manufacturing10.1016/j.jallcom.2019.04.335 ↗
20. Abnormal grain growth in commercially pure titanium during additive manufacturing with electron beam melting10.1016/j.mtla.2019.100281 ↗
21. Selective laser melting of TiC/Ti bulk nanocomposites: influence of nanoscale reinforcement10.1016/j.scriptamat.2012.04.013 ↗
22. Mechanical behavior of porous commercially pure Ti and Ti–TiB composite materials manufactured by selective laser melting10.1016/j.msea.2014.12.036 ↗
23. Carbon nanotubes enabled laser 3D printing of high-performance titanium with highly concentrated reinforcement10.1016/j.isci.2020.101498 ↗
24. Effect of powder particle shape on the properties of in situ Ti–TiB composite materials produced by selective laser melting10.1016/j.jmst.2015.08.007 ↗
25. Development and mechanical characterization of porous titanium bone substitutes10.1016/j.jmbbm.2012.01.008 ↗
26. Fabrication of commercial pure Ti by selective laser melting using hydride-dehydride titanium powders treated by ball milling10.1016/j.jmst.2018.09.058 ↗
27. Achieving high ductility in a selectively laser melted commercial pure-titanium via in-situ grain refinement10.1016/j.scriptamat.2020.09.023 ↗
28. Realizing superior ductility of selective laser melted Ti-6Al-4V through a multi-step heat treatment10.1016/j.msea.2020.140367 ↗
29. Globularization using heat treatment in additively manufactured Ti-6Al-4V for high strength and toughness10.1016/j.actamat.2018.09.064 ↗
30. Fatigue behavior of thin-walled grade 2 titanium samples processed by selective laser melting. Application to life prediction of porous titanium implants10.1016/j.jmbbm.2013.08.011 ↗
31. Simultaneous achievement of equiaxed grain structure and weak texture in pure titanium via selective laser melting and subsequent heat treatment10.1016/j.jallcom.2019.06.305 ↗
32. Deformation heterogeneity and its effect on recrystallization behavior in commercially pure titanium: comparative study on initial microstructures10.1016/j.msea.2019.138211 ↗
33. Ultrahigh-strength titanium gyroid scaffolds manufactured by selective laser melting (SLM) for bone implant applications10.1016/j.actamat.2018.08.005 ↗
34. In-situ measurement of continuous cooling β → α transformation behavior of CP-Ti10.1007/s11661-002-0206-2 ↗
35. Continuous cooling β-to-α transformation behaviors of extra-pure and commercially pure Ti10.1007/s11661-004-0052-5 ↗
36. Massive transformation in Ti-6Al-4V additively manufactured by selective electron beam melting10.1016/j.actamat.2015.11.011 ↗
37. Orientation gradients and geometrically necessary dislocations in ultrafine grained dual-phase steels studied by 2D and 3D EBSD10.1016/j.msea.2010.01.004 ↗
38. Effect of heat treatment on microstructure and mechanical properties of the selective laser melting processed Ti-5Al-2.5Sn α titanium alloy10.1016/j.msea.2017.10.061 ↗
39. On the ductility of alpha titanium: the effect of temperature and deformation mode10.1016/j.actamat.2018.02.022 ↗
40. Deformation anisotropy and associated mechanisms in rolling textured high purity titanium10.1016/j.jallcom.2015.08.075 ↗
41. Anisotropic deformation behavior under various strain paths in commercially pure titanium Grade 1 and Grade 2 sheets10.1016/j.msea.2015.12.081 ↗
42. Formation of nanostructures in commercial-purity titanium via cryorolling10.1016/j.actamat.2012.10.026 ↗
43. Five-parameter intervariant boundary characterization of martensite in commercially pure titanium10.1016/j.actamat.2018.05.023 ↗
44. Variant selection and intervariant crystallographic planes distribution in martensite in a Ti–6Al–4V alloy10.1016/j.actamat.2014.06.064 ↗
45. Additive manufacturing of strong and ductile Ti-6Al-4V by selective laser melting via in situ martensite decomposition10.1016/j.actamat.2014.11.028 ↗
46. Effect of temperature on microstructure and texture evolution during uniaxial tension of commercially pure titanium10.1016/j.msea.2017.07.081 ↗
47. Grain-structure development in heavily cold-rolled alpha-titanium10.1016/j.msea.2014.03.141 ↗
48. The influence of grain size on twinning and microstructure refinement during cold rolling of commercial-purity titanium10.1007/s11661-016-3679-0 ↗
49. The nucleation of recrystallization at second phase particles in deformed aluminium10.1016/0001-6160(77)90109-2 ↗
50. Heterogeneous lamella structure unites ultrafine-grain strength with coarse-grain ductility10.1073/pnas.1517193112 ↗
51. High strength and high ductility in the Co–20Cr–15W–10Ni alloy having a bimodal grain structure achieved by static recrystallization10.1016/j.msea.2018.06.104 ↗
52. Bimodal grain structures and tensile properties of a biomedical Co–20Cr–15W–10Ni alloy with different pre-strains
53. Grain size effect on deformation mechanisms and mechanical properties of titanium10.1016/j.msea.2019.138721 ↗