journal article·2021-03Open access

IMC microstructure modification and mechanical reinforcement of Sn–Ag–Cu/Cu microelectronic joints through an advanced surface finish technique

C.E. Ho, S.P. Yang, P.T. Lee, C.Y. Lee, C.C. Chen, T.T. Kuo

Abstract

Intermetallic compound(s) (IMC) that nucleates at the interface between solder and Cu trace during a soldering reaction, is one of the most crucial factors for microelectronic packaging reliability. This study was conducted to modify the IMC microstructure and to reinforce the mechanical strength of Sn–Ag–Cu/Cu microelectronic joints through various surface finish coatings, including organic solderability preservative (OSP), immersion Ag (ImAg), immersion Sn (ImSn), Au/Pd (electroless palladium/immersion gold, EPIG), and Au/Pd/Au (IGEPIG) layer(s). We confirmed that the type of surface finish dominated the IMC growth morphology and mechanical characteristics of the Sn–Ag–Cu/Cu solder joints, even though these surface finishes were eliminated in a few seconds of the soldering process. A dense Cu6Sn5 layer with a scallop-like appearance was obtained for the traditional OSP case, while a prismatic, loose Cu6Sn5 microstructure was produced for the alternative cases (metal films). This loose Cu6Sn5 microstructure offered numerous molten solder channels for the in-diffusion of Sn to Cu, retarding undesired Cu3Sn growth at the Cu6Sn5/Cu interface; consequently, a brittle-to-ductile transition in the joint fracture mode with a high shear strength and fracture energy was obtained in the high-speed ball shear (HSBS) test. A significant mechanical reinforcement of the Sn–Ag–Cu/Cu microelectronic joints can be achieved with the replacement of the traditional OSP coating by the newly developed IGEPIG trilayer surface finish.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. Interface reaction and intermetallic compound growth behavior of Sn-Ag-Cu lead-free solder joints on different substrates in electronic packaging10.1007/s10853-018-2907-y ↗
2. Effect of La on the Cu-Sn intermetallic compound (IMC) growth and solder joint reliability10.1016/S0925-8388(01)01747-9 ↗
3. Interfacial reaction issues for lead-free electronic solders10.1007/s10854-006-9031-5 ↗
4. TEM investigation of interfacial microstructure and fracture mode of the Sn-Ag-Cu/Ni joint system10.1016/j.msea.2017.08.116 ↗
5. The Zn accumulation behavior, phase evolution and void formation in Sn-xZn/Cu systems by considering trace Zn: a combined experimental and theoretical study10.1016/j.jmrt.2019.07.023 ↗
6. Kinetic theory of flux-driven ripening10.1103/PhysRevB.66.115403 ↗
7. Kinetic analysis of the soldering reaction between eutectic SnPb alloy and Cu accompanied by ripening10.1103/PhysRevB.53.16027 ↗
8. Coarsening mechanisms, texture evolution and size distribution of Cu6Sn5 between Cu and Sn-based solders10.1016/j.matchemphys.2011.08.061 ↗
9. Interfacial reactions of eutectic Sn3.5Ag and pure tin solders with Cu substrates during liquid-state soldering10.1016/j.intermet.2012.02.023 ↗
10. Cu6Sn5 morphology transition and its effect on mechanical properties of eutectic Sn-Ag solder joints10.1007/s11664-010-1430-y ↗
11. Effect of Ag3Sn nanoparticles and temperature on Cu6Sn5 IMC growth in Sn-xAg/Cu solder joints10.1016/j.materresbull.2017.11.022 ↗
12. Influence of Au addition on the phase equilibria of near-eutectic Sn-3.8Ag-0.7Cu Pb-free solder alloy10.1007/s11664-003-0117-z ↗
13. Development and evaluation of direct deposition of Au/Pd(P) bilayers over Cu pads in soldering applications10.1007/s11664-012-2200-9 ↗
14. Influence of interfacial reaction on reliability of QFP joints with Sn-Ag based Pb free solders10.2320/matertrans.42.794 ↗
15. Morphologies, orientation relationships and evolution of Cu6Sn5 grains formed between molten Sn and Cu single crystals10.1016/j.actamat.2008.01.055 ↗
16. Size distribution and morphology of Cu6Sn5 scallops in wetting reaction between molten solder and copper10.1016/j.actamat.2007.11.009 ↗
17. Abnormal Cu3Sn growth and Kirkendall formation between Sn and (111) and (220) preferred-orientation Cu substrates10.1149/1.3608248 ↗
18. Relationship between morphologies and orientations of Cu6Sn5 grains in Sn3.0Ag0.5Cu solder joints on different Cu pads10.1016/j.matchar.2013.12.006 ↗
19. Three-dimensional placement rules of Cu6Sn5 textures formed on the (111)Cu and (001)Cu surfaces using electron backscattered diffraction10.1016/j.matdes.2016.01.037 ↗
20. High-speed Cu electrodeposition and reliability of Cu pillar bumps in high-temperature storage10.1149/2.1001813jes ↗
21. High-speed Cu electrodeposition and its solderability10.1016/j.surfcoat.2016.11.016 ↗
22. Study of grain size effect of Cu metallization on interfacial microstructures of solder joints10.1016/j.microrel.2019.05.018 ↗
23. Impurity-induced unusual microstructural evolution and mechanical property in Sn/Cu solder joints10.1007/s10854-018-9403-7 ↗
24. Suppression of void formation at Sn/Cu joint due to twin formation in Cu electrodeposit10.1007/s11837-019-03576-8 ↗
25. High-temperature stability of Au/Pd/Cu and Au/Pd(P)/Cu surface finishes10.1016/j.apsusc.2017.11.247 ↗
26. Reaction of Au/Pd/Cu and Au/Pd/Au/Cu multilayers with Sn-Ag-Cu alloy10.1016/j.surfcoat.2018.11.085 ↗
27. Joint IPC/JEDEC J-STD-020C · 2004
28. JESD22-B117A · 2006
29. Morphological stability of solder reaction products in flip chip technology10.1007/s11664-001-0139-3 ↗
30. Comparative study between Au/Pd/Cu and Au/Pd(P)/Cu films in soldering applications10.1016/j.surfcoat.2016.03.070 ↗
31. Baker · 1992
32. Villars · 1997
33. Critical current density for inhibiting the (Cu,Ni)6Sn5 formation on the Ni side of Cu/Solder/Ni joints10.1007/s11664-010-1299-9 ↗
34. Effect of thermal aging on high speed ball shear and pull tests of SnAgCu lead-free solder balls
35. An X-ray diffraction and calorimetric investigation of the compound Cu6Sn510.1007/BF02643268 ↗
36. The superstructure of domain-twinned η’-Cu6Sn510.1107/S0108768194004052 ↗
37. EBSD investigation of Cu-Sn IMC microstructural evolution in Cu/Sn-Ag/Cu microbumps during isothermal annealing10.1007/s11664-013-2675-z ↗
38. Inhibiting the growth of Cu3Sn and Kirkendall voids in the Cu/Sn-Ag-Cu system by minor Pd alloying10.1007/s13391-012-2049-3 ↗
39. Effect of Cu grain size on the voiding propensity at the interface of SnAgCu/Cu solder joints10.1016/j.matlet.2015.01.013 ↗
40. Kirkendall void formation in eutectic SnPb solder joints on bare Cu and its effect on joint reliability10.1063/1.1839637 ↗
41. Tu · Solder joint technology, New York: Springer; · 200710.1007/978-0-387-38892-2 ↗
42. Impurity and alloying effects on interfacial reaction layers in Pb-free soldering10.1016/j.mser.2009.12.001 ↗
43. Review of data for the surface tension of pure metals10.1179/imr.1993.38.4.157 ↗
44. Diffusion parameters and growth mechanism of phases in the Cu-Sn system10.1007/s11661-010-0592-9 ↗