Relationship between solidification and liquation cracks in the joining of GTD-111 nickel-based superalloy by Nd:YAG pulsed-laser welding
Source abstract
Abstract
Fusion welding of nickel-based superalloys with a total Al and Ti content of more than 6% has always been challenging. The reason for this is the occurrence of solidification and liquation cracks during welding. Investigating the mechanisms of formation of these two types of cracks can increase the theoretical and practical insight necessary to achieve a welded alloy without cracks. The objective of this research was to look at the link between solidification and liquidation fractures in Nd:YAG pulsed-laser welded GTD-111 nickel-base superalloy joints. The reason for choosing the pulsed-laser method is the mechanism of continuous welding of the pulses and the creation of separate microstructural zones due to the high liquation and solidification speed. Liquation cracks in the partially melted zone (PMZ) of base metal were shown to be significantly associated with solidification cracks in the weld metal, according to the findings. Liquation cracks in PMZ act as a strong place to create and extend solidification cracks. It was also observed that with increasing pulse frequency, the tendency to form both types of cracks decreases due to the increased tendency to back-filling.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Evolution of solidification and microstructure in laser-clad IN625 superalloy powder on GTD-111 superalloy10.1016/j.surfcoat.2021.127010 ↗
2. Effect of Nd: YAG pulsed-laser welding parameters on melting rate of GTD-111 superalloy joint10.1007/s11665-021-06099-z ↗
3. Hot cracking of GTD-111 nickel-based superalloy welded by pulsed Nd: YAG laser10.1007/s13632-019-00602-8 ↗
4. Effect of Nd: YAG pulsed laser welding process on the liquation and strain-age cracking in GTD-111 superalloy10.1016/j.jmapro.2020.01.049 ↗
5. Analysis of liquation and solidification cracks in the electron beam welding of GTD-111 nickel-base superalloy joint10.1088/2053-1591/ac1007 ↗
6. The liquation cracking behavior of IN738LC superalloy during low power Nd: YAG pulsed laser welding10.1016/j.matchar.2012.02.019 ↗
7. Chen · Metals · 2018 · 8 · 38710.3390/met8060387 ↗
8. Influence of heat treatment on creep behavior of IN625 coating on a Ni3Al-base superalloy10.1088/2053-1591/abfba4 ↗
9. Effect of pre-and post-weld heat treatment on microstructure and mechanical properties of GTD-111 superalloy welds10.1007/s12540-019-00465-2 ↗
10. Low heat input welding of nickel superalloy GTD-111 with Inconel 625 filler metal10.3139/120.111131 ↗
11. Direct metal deposition of IN625 on IN738LC superalloy: microstructure and crack analysis10.1007/s00339-021-04464-2 ↗
12. The effect of heat treatment on creep behavior of GTD-111 superalloy welded by pulsed Nd: YAG laser using small punch test10.1016/j.engfailanal.2021.105255 ↗
13. Determination of ideal conditions for GTD-111 superalloy welding through pre-heating, pre-cold and heat treatment
14. The effect of pre-heating and pre-cold treatment on the formation of liquation and solidification cracks of nickel-based superalloy welded by laser beam10.1016/j.jmrt.2020.07.053 ↗
15. Prediction of solidification cracking in pulsed laser welding of 2024 aluminum alloy10.1016/j.actamat.2014.09.002 ↗
16. Microstructural extremes and the transition from fatigue crack initiation to small crack growth in a polycrystalline nickel-base superalloy10.1016/j.actamat.2012.01.049 ↗
17. Effect of Nd: YAG pulsed-laser welding parameters on microstructure and mechanical properties of GTD-111 superalloy joint10.1088/2053-1591/ab1534 ↗
18. The initiation and propagation mechanism of the overlapping zone cracking during laser solid forming of IN-738LC superalloy10.1016/j.jallcom.2018.03.366 ↗
19. Influence of laser welding heat input on HAZ cracking in newly developed Haynes 282 superalloy10.1179/1743284711Y.0000000078 ↗
20. Investigation of melting rate in welding of IN738 Nickel-based superalloy by Nd: YAG pulsed-laser method
21. The relation between liquation and solidification cracks in pulsed laser welding of 2024 aluminium alloy10.1016/j.msea.2009.04.056 ↗
22. Laser cladding of Inconel 713 LC with Stellite 31 powder: statistical modeling and optimization10.1088/1555-6611/ac1920 ↗
23. Microstructural evolution of laser-clad 75Cr3C2+ 25 (80Ni20Cr) powder on Inconel 718 superalloy10.1016/j.jmatprotec.2020.116735 ↗
24. Contribution of constitutional liquation of gamma prime precipitate to weld HAZ cracking of cast Inconel 738 superalloy10.1016/j.scriptamat.2003.11.025 ↗
25. The effect of pre-cold treatment on microstructure, weldability and mechanical properties in laser welding of superalloys10.1016/j.jmapro.2018.06.018 ↗
26. The effect of service temperature on the impact strength and fracture toughness of GTD-111 superalloy10.1016/j.engfailanal.2021.105507 ↗