High-strength vacuum diffusion bonding of Cu-plated, sandblasted W and CuCrZr alloy
Source abstract
Abstract
W/CuCrZr alloy composite panels are promising plasma-facing components for use in future nuclear-fusion reactors. However, the intrinsic immiscibility of W and Cu makes joining them difficult. In this study, we developed a vacuum diffusion bonding method that involves sandblasting of the W substrate surface , Cu electroplating and annealing, and subsequent vacuum diffusion bonding to realize W/CuCrZr joints with high bond strength . The morphologies and structures of the W and W/CuCrZr joints were investigated by scanning electron microscopy, X-ray diffraction, and high-resolution transmission electron microscopy. Sandblasting was found to induce the plastic deformation , roughening, and grain refinement of the W substrate surface. During Cu plating on the surface of the sandblasted W (and subsequent annealing), the Cu layer was embedded in micron-scale irregular pits on the sandblasted W surface, creating a tight bond. The shear bond strength (184 MPa) and bonding quality of a W/CuCrZr joint obtained with the sandblasting/Cu interlayer method was superior to those of a W/CuCrZr joint prepared by conventional vacuum diffusion bonding. The structural origins of this superior W/CuCrZr joint were related to a region of W and Cu interdiffusion with a thickness of approximately 30 nm. This improved vacuum diffusion bonding method for W and CuCrZr can facilitate the development of plasma-facing components for future nuclear-fusion devices.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Fusion materials and technologies · Advanced materials and composites · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Joining of oxygen-free high-conductivity Cu to CuCrZr by direct diffusion bonding without using an interlayer at Low temperature10.1016/j.fusengdes.2019.111400 ↗
2. Influence of helium ion irradiation damage behavior after laser thermal shock of W-2%vol Y2O3 composites10.1016/j.pnucene.2020.103241 ↗
3. High heat load properties of actively cooled W/CuCrZr mock-ups by diffusion bonding with Ni or Ti interlayer10.1016/j.fusengdes.2011.06.002 ↗
4. Tensile strength improvement of martensitic ODS steels with Zr and Hf additions10.1016/j.msea.2021.142071 ↗
5. Repair behavior of He+-irradiated W–Y2O3 composites after different temperature-isochronal annealing experiments10.1016/j.nimb.2017.11.013 ↗
6. Thermomechanical analysis of diffusion-bonded tungsten/EUROFER97 with a vanadium interlayer10.1016/j.jnucmat.2014.09.007 ↗
7. Process optimization for diffusion bonding of tungsten with EUROFER97 using a vanadium interlayer10.1016/j.jnucmat.2015.01.033 ↗
8. High-strength diffusion bonding of oxide-dispersion-strengthened tungsten and CuCrZr alloy through surface nano-activation and Cu plating10.1016/j.jmst.2021.03.040 ↗
9. The simultaneous improvements of strength and ductility in W–Y2O3 alloy obtained via an alkaline hydrothermal method and subsequent low temperature sintering10.1016/j.msea.2020.139329 ↗
10. Controlled synthesis of high-quality W-Y2O3 composite powder precursor by ascertaining the synthesis mechanism behind the wet chemical method10.1016/j.jmst.2019.05.067 ↗
11. Microstructure and mechanical properties of W/Cu vacuum diffusion bonding joints using amorphous Fe-W alloy as interlayer10.1016/j.vacuum.2015.01.008 ↗
12. Microstructural and mechanical characterizations of W/CuCrZr and W/steel joints brazed with Cu-22TiH2 filler10.1016/j.jmatprotec.2017.11.056 ↗
13. Bonding interface of W–CuCrZr explosively welded composite plates for plasma facing components10.1016/j.jmst.2014.11.014 ↗
14. Baseline high heat flux and plasma facing materials for fusion10.1088/1741-4326/aa6b60 ↗
15. Comprehensive enhancement of the mechanical and thermo-mechanical properties of W/Cu joints via femtosecond laser fabricated micro/nano interface structures10.1016/j.msea.2017.04.063 ↗
16. Direct diffusion bonding of immiscible tungsten and copper at temperature close to Copper's melting point10.1016/j.matdes.2017.10.052 ↗
17. Low-temperature densification and microstructure of W–Cu composites with Sn additives10.1016/j.jmrt.2020.12.013 ↗
18. Thermodynamic mechanism for direct alloying of immiscible tungsten and copper at a critical temperature range10.1016/j.jallcom.2018.09.385 ↗
19. Diffusion bonding between W and EUROFER97 using V interlayer10.1016/j.jnucmat.2012.05.049 ↗
20. Vacuum diffusion bonding W to W-Cu composite: interfacial microstructure and mechanical properties10.1016/j.vacuum.2019.03.060 ↗
21. Mechanical properties of HIP bonded W and Cu-alloys joint for plasma facing components10.1016/S0022-3115(02)01169-8 ↗
22. Interface diffusion and mechanical properties of ODS-W/Cu prepared by spark plasma sintering10.1016/j.vacuum.2021.110278 ↗
23. Diffusion bonding of 304 austenitic stainless-steel using pressure pulses
24. Microstructure and mechanical properties of diffusion bonded joints of high-entropy alloy Al5(HfNbTiZr)95 and TC4 titanium alloy10.1016/j.jmrt.2021.02.003 ↗
25. High-temperature mechanical behaviors of diffusion-welded Alloy 61710.1016/j.nucengdes.2020.110617 ↗
26. Improvement of aluminum lithium alloy adhesion performance based on sandblasting techniques10.1016/j.ijadhadh.2018.04.007 ↗
27. Sandblasting parameter variation effect on galvanized steel surface chemical composition, roughness and free energy10.1016/j.ijadhadh.2020.102653 ↗
28. Preparation of a nanoporous active tungsten foil by two-step anodizing and deoxidized annealing for hydrogen evolution reaction10.1088/1361-6528/aae7a7 ↗
29. Effects of surface roughness and energy on ice adhesion strength10.1016/j.apsusc.2010.11.149 ↗
30. Effect of grit-blasting air pressure on adhesion strength of resin to titanium10.1016/j.ijadhadh.2015.11.003 ↗
31. Effects of sandblasting distance and angles on resin cement bonding to zirconia and titanium10.1016/j.ijadhadh.2015.06.009 ↗
32. The effect of sandblasting on surface properties for adhesion10.1016/j.ijadhadh.2016.06.010 ↗
33. Investigation on the diffusion bonding of tungsten and EUROFER9710.1016/j.jnucmat.2010.12.121 ↗
34. Microstructure and tensile strength of the bonded interfaces and parent materials in W/ODS steel joints fabricated by direct SSDB
35. Investigation of tungsten/steel brazing using Ta and Cu interlayer10.1016/j.fusengdes.2016.11.004 ↗
36. Supermodulus effect by grain-boundary wetting in nanostructured multilayers10.1016/j.jmst.2020.03.084 ↗
37. Microstructure evolution and interface structure of Al-40 wt% Si composites produced by high-energy ball milling10.1016/j.jmst.2018.10.005 ↗
38. Empirical and theoretical insights into the structural effects of selenite doping in hydroxyapatite and the ensuing inhibition of osteoclasts10.1016/j.msec.2020.111257 ↗
39. Direct alloying of immiscible molybdenum-silver system and its thermodynamic mechanism10.1016/j.jmst.2020.04.083 ↗
40. Investigation of tungsten/steel diffusion bonding with Ni–Fe cladding on tungsten substrate10.1016/j.fusengdes.2017.11.014 ↗
41. Evaluation of the bonded ratio of TC4 diffusion bonded joints based on ultrasonic C-scan10.1016/j.jmapro.2019.09.025 ↗
42. Femtosecond laser fabricated micro/nano interface structures toward enhanced bonding strength and heat transfer capability of W/Cu joining10.1016/j.matdes.2016.11.094 ↗
43. Mechanically driven alloying of immiscible elements10.1103/PhysRevLett.68.2235 ↗