Characterizations the deposition behavior and mechanical properties of detonation sprayed Fe-based amorphous coatings
Source abstract
Abstract
In this study, the spreading morphologies and deposition behaviors of molten droplet in a single detonation sprayed shot under different oxygen-fuel ratio conditions are characterized in detail to reveal the formation mechanism of Fe-based amorphous coatings. Additionally, the porosities, micro-hardness, amorphous phase content and wear behavior of the coatings were also carefully evaluated to correlate the relationship between preparation process parameters, particle deposition behavior, spreading morphology, and mechanical properties. The results indicate that the spraying oxygen-fuel ratio (OF) parameter can determine the microstructure change of the coating, which is considered to be a reflection of the molten state of the sprayed particles. The low OF reduces the combustion efficiency, making the coating particles deposited in a form similar to cold spraying, resulting in uneven coating structure. In the case of medium OF (2.00), amorphous particles can form completely melted droplets and spread well on the substrate, and produce a good metallurgical bond with the substrate. Thanks to the good spread of the amorphous droplets, the OF-2.00 coating displays a very uniform and dense structure and uniformly distributed microhardness, which also makes its wear resistance (0.63 × 10−6 mm3 N−1 m−1) increased by about 8 times compared with OF-1.43 coating.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Diamond and Carbon-based Materials Research · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Significantly enhanced resistance to SRB corrosion via Fe-based amorphous coating designed with high dose corrosion-resistant and antibacterial elements10.1016/j.corsci.2019.108305 ↗
2. Corrosion resistance mechanisms of detonation sprayed Fe-based amorphous coating on AZ31B magnesium alloy10.1016/j.jnoncrysol.2021.121276 ↗
3. A study on corrosion and corrosion-wear behavior of Fe-based amorphous alloy coating prepared by high velocity oxygen fuel method10.1016/j.jmrt.2021.10.103 ↗
4. Characterization and elevated-temperature tribological performance of AC-HVAF-sprayed Fe-based amorphous coating10.1016/j.surfcoat.2020.125535 ↗
5. The wear properties and mechanism of detonation sprayed iron-based amorphous coating10.1016/j.surfcoat.2019.03.028 ↗
6. Corrosion and erosion–corrosion behaviour of activated combustion high-velocity air fuel sprayed Fe-based amorphous coatings in chloride-containing solutions10.1016/j.corsci.2015.05.044 ↗
7. Microstructure and wear behavior of Fe-based amorphous HVOF coatings produced from commercial precursors10.1016/j.surfcoat.2016.10.057 ↗
8. Corrosion and erosion-corrosion behavior of activated combustion high-velocity air fuel sprayed Fe-based amorphous coatings in chloride-containing solutions10.1016/j.corsci.2015.05.044 ↗
9. Hot corrosion behavior of an arc sprayed Fe-based amorphous coating in a simulated biomass-firing environment10.1016/j.corsci.2021.109938 ↗
10. Method and apparatus utilizing detonation waves for spraying and other purposes
11. Flame plating using detonation reactants
12. Analysis of particle dynamics and heat transfer in detonation thermal spraying systems10.1361/10599630419373 ↗
13. Enhancing the properties of WC/Co detonation coatings using two-component fuels10.1016/j.surfcoat.2016.08.008 ↗
14. Room temperature nanoindentation creep behavior of detonation sprayed Fe-based amorphous coating10.1016/j.intermet.2021.107426 ↗
15. Computer-controlled detonation spraying: from process fundamentals toward advanced applications10.1007/s11666-011-9649-6 ↗
16. Laminar Fe-based amorphous composite coatings with enhanced bonding strength and impact resistance10.1016/j.actamat.2014.03.047 ↗
17. Toughening Fe-based amorphous coatings by reinforcement of amorphous carbon10.1038/s41598-017-04504-z ↗
18. Interfacial characteristic and microstructure of Fe-based amorphous coating on magnesium alloy10.1016/j.surfcoat.2021.127659 ↗
19. Strategy for improving the wear-resistance properties of detonation sprayed Fe-based amorphous coatings by cryogenic cycling treatment10.1016/j.surfcoat.2021.126962 ↗
20. Interfacial bonding mechanism and properties of HVOF-sprayed Fe-based amorphous coatings on LA141 magnesium alloy substrate10.1016/j.surfcoat.2021.127801 ↗
21. Microstructures and corrosion properties of novel Fe46.8Mo30.6Cr16.6C4.3B1.7 metallic glass coatings manufactured by vacuum plasma spray process10.1016/j.intermet.2020.107061 ↗
22. Contact and rubbing of flat surfaces10.1063/1.1721448 ↗
23. Differences in dry sliding wear behavior between HVAF-sprayed amorphous steel and crystalline stainless steel coatings10.1016/j.jmst.2018.11.006 ↗
24. Dry sliding wear behaviors of Fe-based amorphous metallic coating synthesized by D-gun spray10.1016/j.jnoncrysol.2020.120018 ↗
25. Conditions and mechanisms for the bonding of a molten ceramic droplet to a substrate after high-speed impact10.1016/j.actamat.2016.07.057 ↗
26. Epitaxial growth during the rapid solidification of plasma-sprayed molten TiO2 splat10.1016/j.actamat.2017.05.052 ↗
27. Interfacial metal/ceramic bonding mechanism for metallization of ceramics via cold spraying10.1016/j.jmatprotec.2020.116845 ↗
28. Detonation spraying behaviour of refractory metals: case studies for Mo and Ta-based powders10.1016/j.apt.2018.04.023 ↗
29. Improvement of interfacial bonding between plasma-sprayed cast iron splat and aluminum substrate through preheating substrate10.1016/j.surfcoat.2017.03.032 ↗
30. Particle in-flight status and its influence on the properties of supersonic plasma-sprayed Fe-based amorphous metallic coatings10.1016/j.surfcoat.2018.11.049 ↗
31. Microstructure, corrosion-resistance, and wear-resistance properties of subsonic flame sprayed amorphous Fe-Mo-Cr-Co coating with extremely high amorphous rate10.1016/j.jmrt.2020.01.024 ↗
32. Substrate temperature dependence of splat morphology for plasma-sprayed cast iron on aluminum surface10.1016/j.surfcoat.2015.10.073 ↗
33. Detonation spraying of copper: theoretical analysis and experimental studies10.1016/j.matpr.2017.09.006 ↗
34. Solid-state additive manufacturing high performance aluminum alloy 6061 enabled by an in-situ micro-forging assisted cold spray10.1016/j.msea.2020.139024 ↗
35. Solid-state additive manufacturing high performance aluminum alloy 6061 enabled by an in-situ micro-forging assisted cold spray10.1016/j.msea.2020.139024 ↗
36. Predicting splat morphology in a thermal spray process10.1016/j.surfcoat.2007.03.010 ↗
37. Automated image inspection system to quantify thermal spray splat morphology10.1016/j.surfcoat.2015.07.065 ↗