journal article·2021-05Open access

Improving surface properties of Fe-based laser cladding coating deposited on a carbon steel by heat assisted ultrasonic burnishing

Changsheng Zhang, Xuehui Shen, Jiatian Wang, Chonghai Xu, Jianqun He, Xiaolan Bai

Abstract

In the present study, the combination of ultrasonic burnishing and heat treatment were applied on a laser cladded Fe-based coating. Besides ultrasonic burnishing at room temperature (UB), two combination strategies of ultrasonic burnishing and heat treatment were explored, i.e. ultrasonic burnishing at a medium temperature (ultrasonic warm burnishing, UWB), and UWB coupled with continuous heat treatment for a period of time (ultrasonic warm burnishing coupled with heat treatment, UWB/HT). Total four samples were prepared and experimentally investigated. Comparing with untreated (control) sample, the surface properties of the three differently treated samples were improved to varying degrees, where the sample subjected to UWB/HT process acquired the best one. UWB/HT Process declined the roughness and porosity of Fe-based coating by 87.86%, 65.41%, and the hardness increased by 34.88% compared to that of control sample, respectively. The residual stress and microstructure of UWB/HT sample also acquired a largest improvement. In addition, the UWB/HT Fe-based coating exhibited the best wear resistance. Summarily, UWB/HT is considered to have the greatest potential to achieve the effective treatment of laser cladding with excellent surface properties over the other two strategies, which is expected to further advance the application of laser cladding technique particularly in the fabrication of some high-demand products serving in harsh conditions.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Surface Treatment and Residual Stress · High Entropy Alloys Studies · Additive Manufacturing Materials and Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (62)

Show source-provided references
1. A review report on the plating process of fused deposition modelling (FDM) built parts10.1016/j.matpr.2020.02.461 ↗
2. Fabrication, microstructure and wear properties of novel Fe-Mo-Cr-C-B metallic glass coating layers manufactured by various thermal spray processes10.1016/j.matdes.2020.109043 ↗
3. Weld deposition of nickel on titanium for surface hardening with Ti-Ni-based intermetallic compounds10.1016/j.matpr.2019.09.075 ↗
4. Corrosion and wear protection of mild steel substrates by innovative PVD coatings10.1016/j.surfcoat.2020.125659 ↗
5. Electroless-plating of Ag nanoparticles on Al2O3 for enhanced mechanical and wear properties of Cu-Al2O3 nanocomposites10.1016/j.jmrt.2020.09.077 ↗
6. Modified epoxy coatings on mild steel: tribology and surface energy10.1016/j.eurpolymj.2010.08.006 ↗
7. The fabrication of NiTi shape memory alloy by selective laser melting: a review10.1108/RPJ-11-2018-0292 ↗
8. Research status and application of the high-entropy and traditional alloys fabricated via the laser cladding
9. Phase constitution, microstructure and properties of pulsed laser-clad ternary CrNiTi medium-entropy alloy coating on pure titanium10.1016/j.surfcoat.2020.126503 ↗
10. A validated analytical-numerical modelling strategy to predict residual stresses in single-track laser deposited IN71810.1016/j.ijmecsci.2018.12.004 ↗
11. Characterization of FeP-based metallic glass coatings prepared with laser cladding10.1016/j.surfcoat.2020.126733 ↗
12. Plastic deformation and critical condition for orthogonal machining two-layered materials with laser cladded Cr-Ni-based stainless steel onto AISI 104510.1016/j.jclepro.2017.02.167 ↗
13. Production of corrosion-resistant 316L stainless steel clads on carbon steel using powder bed fusion-selective laser melting10.1016/j.jmatprotec.2019.05.024 ↗
14. The effect of particle size on the heat affected zone during laser cladding of Ni–Cr–Si–B alloy on C45 carbon steel10.1016/j.optlaseng.2017.09.021 ↗
15. Microhardness and wear resistance of Al2O3-TiB2-TiC ceramic coatings on carbon steel fabricated by laser cladding10.1016/j.ceramint.2018.09.140 ↗
16. Study on chip morphology and milling characteristics of laser cladding layer10.1007/s00170-014-6483-2 ↗
17. Identifying defects and problems in laser cladding and suggestions of some remedies for the same10.1016/j.matpr.2018.02.297 ↗
18. Laser polishing parameter optimisation on selective laser sintered parts
19. Repairing parts from nickel base material alloy by laser cladding and ball end milling10.1007/s11740-016-0690-7 ↗
20. Machinability for dry turning of laser cladded parts with conventional vs. wiper insert10.1016/j.jmapro.2017.04.017 ↗
21. Effects of laser cladding on fatigue performance of AISI 4340 steel in the as-clad and machine treated conditions10.1016/j.jmatprotec.2016.12.020 ↗
22. Cutting force models for Fe–Al-based coating processed by a compound NC machine tool10.1007/s00170-015-6817-8 ↗
23. Effect of grinding on the residual stress and adhesion strength of HVOF thermally sprayed WC–10Co–4Cr coating10.1080/10426914.2014.930893 ↗
24. Enhancing surface integrity and corrosion resistance of laser cladded Cr–Ni alloys by hard turning and low plasticity burnishing10.1016/j.apsusc.2017.03.028 ↗
25. Slide diamond burnishing of tool steels with adhesive coatings and diffusion layers10.1179/1433075X12Y.0000000060 ↗
26. Microstructure and mechanical properties of laser cladded Cr-Ni alloy by hard turning (HT) and ultrasonic surface rolling (USR)10.1016/j.surfcoat.2020.125806 ↗
27. Experimental validation of contact models for cold-rolling processes10.1016/j.jmatprotec.2019.116371 ↗
28. Improved plasticity and cold-rolling workability of Fe–6.5 wt% Si alloy by warm-rolling with gradually decreasing temperature10.1016/j.jmst.2016.01.017 ↗
29. Friction and wear behaviour of tool steels sliding against 22MnB5 steel10.1016/j.jmrt.2017.04.002 ↗
30. Strengthening of Ti-6Al-4V alloy by high temperature ultrasonic nanocrystal surface modification technique10.1016/j.matlet.2017.03.059 ↗
31. Effect of ultrasonic nanocrystal surface modification on elevated temperature residual stress, microstructure, and fatigue behavior of ATI 718Plus alloy10.1016/j.ijfatigue.2018.01.017 ↗
32. An investigation of stress condition in vibration-assisted burnishing10.1007/s00170-019-04128-9 ↗
33. Surface characteristics and corrosion behavior of TC11 titanium alloy strengthened by ultrasonic roller burnishing at room and medium temperature10.1016/j.jmrt.2020.05.059 ↗
34. Porosity elimination and heat treatment of diode laser-clad homogeneous coating on cast aluminum-copper alloy10.1016/j.surfcoat.2017.04.027 ↗
35. Physical-mechanical and electrochemical corrosion behaviors of additively manufactured Cr-Ni-based stainless steel formed by laser cladding10.1016/j.matdes.2016.03.151 ↗
36. The role of plastic deformation of rough surfaces in the size-dependent hardness10.1016/j.actamat.2003.08.026 ↗
37. Improvement of the tribological properties of Al6061-T6 alloy under dry sliding conditions10.1016/j.triboint.2013.02.034 ↗
38. Toward a quantitative understanding of mechanical behavior of nanocrystalline metals10.1016/j.actamat.2007.01.038 ↗
39. Effect of ultrasonic surface rolling at low temperatures on surface layer microstructure and properties of HIP Ti-6Al-4V alloy10.1016/j.surfcoat.2017.01.099 ↗
40. Influence of dynamic strain aging on the apparent activation volume for deformation10.1016/0025-5416(85)90082-5 ↗
41. Dynamic strain aging and hydrogen-induced softening in alpha titanium10.1007/BF02651937 ↗
42. Effect of ferrite grain boundary on strain aging behavior in Nb-bearing ultra-low-carbon steel sheets10.4028/www.scientific.net/MSF.706-709.2222 ↗
43. Stress gradient induced strain localization in metals: high resolution strain cross sectioning via synchrotron X-Ray diffraction10.1115/1.2840962 ↗
44. Wear resistance enhancement of titanium alloy (Ti-6Al-4V) by ball burnishing process10.1016/j.jmrt.2016.03.007 ↗
45. Surface improvement of shafts by the deep ball-burnishing technique10.1016/j.surfcoat.2011.11.045 ↗
46. Cyclic deformation and near surface microstructures of shot peened or deep rolled austenitic stainless steel AISI 30410.1016/S0921-5093(98)01121-6 ↗
47. Finite element modeling of the surface roughness of 5052 Al alloy subjected to a surface severe plastic deformation process10.1016/j.actamat.2004.08.031 ↗
48. Surface integrity enhancement of austenitic stainless steel treated by ultrasonic burnishing with two burnishing tips10.1007/s43452-020-00074-6 ↗
49. Microstructural evolution and characteristics of bonding zone in multilayer laser cladding of Fe-based coating10.1016/j.jmatprotec.2018.08.005 ↗
50. Directed energy deposition and characterization of high-carbon high speed steels
51. Influence of in-situ synthesized carboborides on microstructure evolution and the wear resistance of laser clad Fe-base composite coatings10.1016/j.matchar.2020.110326 ↗
52. Mechanical properties and electrochemical corrosion resistance of multilayer laser cladded Fe-based composite coatings on 4Cr5MoSiV1 steel10.1016/j.jmatprotec.2020.116736 ↗
53. Gigacycle fatigue behavior by ultrasonic nanocrystalline surface modification10.1166/jnn.2012.6329 ↗
54. Plastic strain-induced grain refinement at the nanometer scale in copper10.1016/j.actamat.2006.07.013 ↗
55. Microstructure and surface properties of 17-4PH stainless steel by ultrasonic surface rolling technology10.1016/j.surfcoat.2017.04.052 ↗
56. The usability and preliminary effectiveness of ultrasonic nanocrystalline surface modification technique on surface properties of silicon carbide10.1016/j.apsusc.2014.05.089 ↗
57. Surface nanocrystallization by ultrasonic nano-crystal surface modification and its effect on gas nitriding of Ti6Al4V alloy10.1016/j.msea.2018.08.089 ↗
58. Modeling of surface roughness effect on dry contact friction in metal forming10.1007/s00170-011-3305-7 ↗
59. Tribological behavior of UHMWPE against TiAl6V4 and CoCr28Mo alloys under dry and lubricated conditions10.1016/j.jmbbm.2016.07.002 ↗
60. Influence of ball burnishing on surface quality and tribological characteristics of polymers under dry sliding conditions10.1016/j.triboint.2010.10.005 ↗
61. Local heat treatment with and without ultrasonic nanocrystal surface modification of Ti-6Al-4V alloy: mechanical and tribological properties10.1016/j.surfcoat.2017.07.064 ↗
62. Effect of grain size on friction and wear behavior of Ti3SiC210.1016/S0043-1648(99)00348-8 ↗