Corrosion behavior of cold-rolled metastable Cr–Mn–Ni–N austenitic stainless steel in acidic NaCl solution
Source abstract
Abstract
The microstructure and corrosion behavior of metastable austenitic stainless steel (MASS) 14Cr10Mn in acidic 1 wt.% NaCl solution were investigated by X-ray diffraction (XRD), electron back scatter diffraction (EBSD), scanning electron microscope (SEM), X-ray photoelectron spectroscopy (XPS) and electrochemical measurement techniques. Cold rolling deformation noticeably increases the contents of martensites and microdefects in the steel. All specimens show active–passive transition during the anodic polarization process. With changing the cold rolling reduction from 0% to 20%, the active corrosion rate markedly increases about 55%, whereas the pitting potential slightly decreases about 80 mV. The cold rolling deformation clearly facilitates the preferential dissolution of Fe and Cr as well as the enrichment of Cu on the metal surface in the corrosion process. The small shallow grooves and pits form at the deformation band regions.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (67)
Show source-provided references
1. Effect of preheating temperature on surface cracking of high nitrogen CrMn austenitic stainless steel10.1016/S1005-0302(10)60127-2 ↗
2. Dependence of corrosion resistance on grain boundary characteristics in a high nitrogen CrMn austenitic stainless steel10.1016/j.jmst.2017.09.016 ↗
3. Nitrogen-alloyed, metastable austenitic stainless steel for automotive structural applications10.1081/AMP-120027498 ↗
4. Application of cost-effective stainless steel for automotive components10.1080/10426910903179989 ↗
5. Influence of grain refinement on the corrosion behavior of metallic materials: a review10.1007/s12613-021-2308-0 ↗
6. On nitrogen diffusion during solution treatment in a high nitrogen austenitic stainless steel10.1016/j.jmrt.2019.12.064 ↗
7. Inverse effect of strain rate on mechanical behavior and phase transformation of super austenitic stainless steel10.1016/j.scriptamat.2006.08.064 ↗
8. Electrochemical and corrosion behaviour of cold rolled AISI 301 in 1M H2SO4
9. The mechanism of pitting initiation and propagation at deformation bands intersection of cold-rolled metastable stainless steel in acidic ferric chloride solution10.1007/s10853-019-03922-w ↗
10. Influence of strain-induced martensite in the anodic dissolution of austenitic stainless steels in acid medium10.1016/j.corsci.2012.11.033 ↗
11. Comparison of rolled and heat treated SS304 in chloride solution using electrochemical and XPS techniques10.1016/S0010-938X(03)00099-4 ↗
12. Influence of cold-worked structure on electrochemical properties of austenitic stainless steels10.1007/s11661-007-9224-4 ↗
13. Accumlation of copper layer on a surface in the anodic polarization of stainless steel containing Cu at different temperatures10.1016/0013-4686(94)00365-8 ↗
14. The effects of prior-deformation on anodic dissolution kinetics and pitting behavior of 316L stainless steel10.1016/S1452-3981(23)15930-X ↗
15. Effects of plastic strains on passivation behavior of different austenitic stainless steel grades10.1088/2053-1591/aaea2d ↗
16. Effect of deformation-induced martensite on pitting corrosion of SUS304 stainless steel in H2SO4-NaCl solution10.2320/jinstmet1952.54.10_1078 ↗
17. Influence of cold work on pitting corrosion behavior of a high nitrogen stainless steel10.1149/1.2939213 ↗
18. Application of Volta potential mapping to determine metal surface defects10.1016/j.electacta.2007.05.077 ↗
19. Influence of thermal and mechanical surface modifications induced by laser shock processing on the initiation of corrosion pits in 316L stainless steel10.1007/s10853-007-1502-4 ↗
20. Relationship between the martensite phase transition and pitting susceptibility of AISI-321 stainless steel in acidic solutions of NaCl10.1007/s11003-005-0052-7 ↗
21. Effects of cold work and sensitization treatment on the corrosion resistance of high nitrogen stainless steel in chloride solutions10.1016/j.electacta.2008.09.053 ↗
22. Effect of stress and strain on corrosion resistance of duplex stainless steel10.1016/j.ijpvp.2013.04.025 ↗
23. Pitting resistance of cold-worked commercial austenitic stainless steels in solution simulating seawater10.1149/1.2128863 ↗
24. Influence of the cold working induced martensite on the electrochemical behavior of AISI 304 stainless steel surfaces10.1016/j.jmrt.2018.10.004 ↗
25. Effect of cold-working in the passive behavior of 304 stainless steel in sulfate media10.1149/1.1516774 ↗
26. Corrosion behaviors of two types of commercial stainless steel after plastic deformation10.1016/S1005-0302(10)60133-8 ↗
27. Effect of austenite stability on the pitting corrosion resistance of cold worked stainless steels10.1016/j.corsci.2008.12.026 ↗
28. Corrosion behavior of deformed low-nickel stainless steel in groundwater solution10.1016/j.engfailanal.2019.01.073 ↗
29. Enhanced plasma nitriding efficiency and properties by severe plastic deformation pretreatment for 316L austenitic stainless steel10.1016/j.jmrt.2021.08.082 ↗
30. Martensite transformation behavior and mechanical properties of cold-rolled metastable Cr-Mn-Ni-N austenitic stainless steels10.1016/j.msea.2018.03.113 ↗
31. Effect of cold deformation on the electrochemical behaviour of 304L stainless steel in contaminated sulfuric acid environment10.1016/j.apsusc.2017.07.057 ↗
32. Orientation dependent behavior of tensile-creep deformation of hot rolled Ti65 titanium alloy sheet10.1016/j.jmst.2020.10.021 ↗
33. Effect of pre-solution treatment on deformation behavior of AZ80-Ag magnesium alloy10.1016/j.jmrt.2020.07.058 ↗
34. Atomic emission spectroelectrochemistry applied to dealloying phenomena: I. The formation and dissolution of residual copper films on stainless steel10.1016/j.electacta.2009.01.037 ↗
35. Electrochemical and surface analytical approach to passive film on 200 series stainless steels formed in sulfuric acid10.2355/isijinternational.49.1902 ↗
36. Corrosion behaviour of copper containing low alloy steels in sulphuric acid10.1016/j.corsci.2011.09.012 ↗
37. Pitting corrosion of Cr–Mn–N steel in sulphuric acid media10.1007/s10800-005-9070-2 ↗
38. Pitting corrosion behaviour of austenitic stainless steels – combining effects of Mn and Mo additions10.1016/j.corsci.2008.04.005 ↗
39. Microstructural changes in AISI 304L stainless steel due to surface machining: effect on its susceptibility to chloride stress corrosion cracking10.1016/j.jnucmat.2010.05.028 ↗
40. Impact of surface condition on sulphide stress corrosion cracking of 316L stainless steel10.1016/j.corsci.2013.02.002 ↗
41. Electrochemical corrosion behavior of 2205 duplex stainless steel in hot concentrated seawater under vacuum conditions10.1016/j.corsci.2019.108383 ↗
42. Electronic properties of the passive films formed on CoCrFeNi and CoCrFeNiAl high entropy alloys in sodium chloride solution10.1016/j.jmrt.2020.10.002 ↗
43. Study of oxide protective layers on stainless steel by AES, EDS and XPS10.1002/sia.2718 ↗
44. Effect of surface passivation on corrosion resistance and antibacterial properties of Cu-bearing 316L stainless steel10.1016/j.apsusc.2016.06.036 ↗
45. Effect of dissolved oxygen on electrochemical corrosion behavior of 2205 duplex stainless steel in hot concentrated seawater10.1016/j.jmst.2020.06.030 ↗
46. Effect of Mn additions on the corrosion behaviour of TWIP Fe-Mn-Al-Si austenitic steel in chloride solution10.1016/j.corsci.2019.04.026 ↗
47. Electrochemical corrosion behaviour of a novel submicron-grained austenitic stainless steel in an acidic NaCl solution10.1016/j.msea.2006.05.138 ↗
48. Effect of deformation-induced martensitic transformation on the plastic behavior of metastable austenitic stainless steel10.2320/matertrans1989.30.33 ↗
49. Effect of deformation-induced martensite on the general corrosion of SUS304 stainless steel in H2SO4-NaCl solution10.2320/jinstmet1952.55.6_660 ↗
50. Stress corrosion cracking of cold-worked austenitic stainless steels10.1016/0010-938X(82)90055-5 ↗
51. Effect of deformation-induced phase transformation on AISI 316 stainless steel corrosion resistance10.1016/j.engfailanal.2017.05.031 ↗
52. Texture evolution and phase transformation of 25Cr-6Mo-5Ni experimental duplex stainless steel during hot and cold rolling10.1016/j.jmrt.2017.01.001 ↗
53. Effect of stress on electrochemical characteristics of pre-cracked ultrahigh strength stainless steel in acid sodium sulphate solution10.1016/j.corsci.2014.08.023 ↗
54. Effect of residual stress on corrosion sensitivity of carbon steel studied by SECM10.1007/s40242-014-4099-6 ↗
55. Comparative studies on the corrosion properties of a Fe–Mn–Al–Si steel and an interstitial-free steel10.1016/j.corsci.2008.07.024 ↗
56. The effect of Cu addition on the electrochemical corrosion and passivation behavior of stainless steels10.1016/j.electacta.2010.04.015 ↗
57. Effects of Cu on the passive film stability of Fe–20Cr–xCu (x=0, 2, 4wt.%) alloys in H2SO4 solution10.1016/j.electacta.2012.10.058 ↗
58. The influence of minor alloying elements (Nb Ni and Cu)on the corrosion resistivity of ferritic stainless steel in sulfuric acid solution10.1016/0010-938X(86)90085-5 ↗
59. The effect of copper on the anodic dissolution behaviour of austenitic stainless steel in acidic chloride solution10.1016/0010-938X(92)90049-9 ↗
60. Mechanism of copper action on pitting phenomena observed on stainless steels in chloride media10.1016/j.corsci.2004.05.024 ↗
61. Effect of alloying Cu on the corrosion resistance of stainless steels in chloride media10.1016/S0010-938X(01)00008-7 ↗
62. Pitting corrosion behaviour of austenitic stainless steels with Cu and Sn additions10.1016/j.corsci.2006.06.004 ↗
63. Inhibition of stress corrosion cracking of AISI 293 stainless steel by molybdate ions at elevated temperatures under salt crust10.1016/S0010-938X(98)00184-X ↗
64. Effects of cold deformation on electrochemical corrosion behaviors of 304 stainless steel10.1108/ACMM-12-2015-1620 ↗
65. The effect of pre-deformation on corrosion resistance of the passive film formed on 2205 duplex stainless steel10.1016/j.jallcom.2016.06.003 ↗
66. Effect of deformation-induced martensite on the pit propagation behavior of 304 stainless steel10.1108/00035590410560921 ↗
67. Effect of Cl− on the properties of the passive films formed on 316L stainless steel in acidic solution10.1016/j.jmst.2013.07.010 ↗