Exploring the improvement of strength and cryogenic impact toughness in hot-rolled high Mn austenitic steel for cryogenic application
Source abstract
Abstract
In general, there is a steep decrease in cryogenic (−196 °C) impact absorbed energy of high Mn austenitic steels after aging at 600–800 °C, which is also the temperature range of aging precipitation. Thus, the precipitation hardening is hardly used in hot-rolled high Mn austenitic steel for cryogenic application and its effect on cryogenic impact toughness is also not understood up to now. In the present work, A high Mn austenitic steel alloyed with Al and V was designed, and the effect of aging temperature on the evolution of microstructure and mechanical properties was investigated by means of electron backscattered diffraction, transmission electron microscopy and X-ray diffraction. The grain size is nearly not affected by aging temperature, exhibiting similar grain size of 6.7–8.1 μm, but the volume fraction and size of precipitated particles greatly depend on aging temperature. The average particle size slightly increases from 5.6 to 6.7 nm with increasing aging temperature from 550 to 650 °C, whereas the precipitated particles are greatly coarsened at 700 °C and the average particle size reaches 16.3 nm. These fine particles can provide a sufficient precipitation hardening of about 200 MPa, leading to a high yield strength of 587 MPa. Meanwhile, this strong precipitation hardening only slight lowers cryogenic impact absorbed energy from 132 to 97 J, also implying that the above-mentioned aging brittle effect should be suppressed or very weak.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Metallurgy and Material Forming
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. High manganese austenitic steel for cryogenic applications
2. Interpretation of cryogenic-temperature Charpy impact toughness by microstructural evolution of dynamically compressed specimens in austenitic 0.4C–(22–26)Mn steels10.1016/j.actamat.2014.11.027 ↗
3. Effects of Mn and Al contents on cryogenic-temperature tensile and Charpy impact properties in four austenitic high-Mn steels10.1016/j.actamat.2015.08.027 ↗
4. Effects of Mn addition on tensile and Charpy impact properties in austenitic Fe-Mn-C-Al-based steels for cryogenic applications10.1007/s11661-014-2513-9 ↗
5. Grain size dependence of twinning behaviors and resultant cryogenic impact toughness in high manganese austenitic steel10.1016/j.jmrt.2020.12.030 ↗
6. Hierarchical microstructure design of a bimodal grained twinning-induced plasticity steel with excellent cryogenic mechanical properties10.1016/j.actamat.2018.06.019 ↗
7. Deformation microstructures as well as strengthening and toughening mechanisms of low-density high Mn steels for cryogenic applications10.1016/j.jmrt.2021.05.018 ↗
8. The effects of recrystallization on strength and impact toughness of cold-worked high-Mn austenitic steels10.3390/met9090948 ↗
9. High carbon alloyed design of a hot-rolled high-Mn austenitic steel with excellent mechanical properties for cryogenic application10.1016/j.msea.2021.141959 ↗
10. Role of vanadium additions on tensile and cryogenic-temperature Charpy impact properties in hot-rolled high-Mn austenitic steels10.1016/j.msea.2021.141063 ↗
11. Microstructure and mechanical properties of a hot-rolled high manganese TWIP steel containing 0.3%V10.2355/isijinternational.ISIJINT-2019-578 ↗
12. Influence of final rolling temperature on microstructure and mechanical properties in a hot-rolled TWIP steel for cryogenic application10.1016/j.msea.2018.03.111 ↗
13. Twinning-induced plasticity (TWIP) steels10.1016/j.actamat.2017.06.046 ↗
14. High manganese austenitic twinning induced plasticity steels: a review of the microstructure properties relationships10.1016/j.cossms.2011.04.002 ↗
15. Stacking fault energy and plastic deformation of fully austenitic high manganese steels: effect of Al addition10.1016/j.msea.2010.02.058 ↗
16. Effect of Ni content on the tensile properties and strain-induced martensite transformation for 304 stainless steel10.1016/j.msea.2010.12.022 ↗
17. Understanding martensite and twin formation in austenitic steels: a model describing TRIP and TWIP effects10.1016/j.actamat.2017.02.004 ↗
18. Grain size-dependent mechanical properties of a high-manganese austenitic steel10.1007/s40195-018-0828-z ↗
19. Enhancing strength and cryogenic toughness of high manganese TWIP steel plate by double strengthened structure design10.1016/j.msea.2020.139397 ↗
20. Evolution of microstructures and mechanical properties during solution treatment of a Ti–V–Mo-containing high-manganese cryogenic steel10.1016/j.matchar.2017.11.054 ↗
21. Interpretation of significant decrease in cryogenic-temperature Charpy impact toughness in a high manganese steel10.1016/j.msea.2018.09.043 ↗
22. The influence of stacking fault energy on the microstructural and strain-hardening evolution of Fe–Mn–Al–Si steels during tensile deformation10.1016/j.actamat.2015.08.030 ↗
23. Modelling of TWIP effect on work-hardening [J]10.1016/S0921-5093(00)02019-0 ↗
24. New twinning route in face-centered cubic nanocrystalline metals10.1038/s41467-017-02393-4 ↗
25. A mechanism for the growth of deformation twins in crystals10.1080/14786445108561272 ↗
26. Dislocation reactions during deformation twinning in Cu-11at.% Al single crystals10.1016/0001-6160(80)90154-6 ↗
27. Formation of deformation twins in f.c.c. crystals10.1016/0001-6160(73)90085-0 ↗
28. Twin-dislocation and twin–twin interactions during cyclic deformation of a nickel-base single crystal TMS-82 superalloy10.1016/j.ijfatigue.2014.04.012 ↗
29. On the deformation twinning mechanisms in twinning-induced plasticity steel10.1016/j.actamat.2017.09.043 ↗
30. Dislocation interaction and twinning-induced plasticity in face centered cubic Fe-Mn-C micro-pillars10.1016/j.actamat.2017.04.043 ↗
31. Quantitative measurements of grain boundary excess volume from HAADF-STEM micrographs10.1016/j.actamat.2016.01.033 ↗
32. Effects of α/γ orientation relationship on VC interphase precipitation in low-carbon steels10.1016/j.scriptamat.2013.03.020 ↗
33. Size and orientation effects in partial dislocation-mediated deformation of twinning-induced plasticity steel micro-pillars10.1016/j.actamat.2015.06.065 ↗
34. On the effect of chemical composition on yield strength of TWIP steels10.1016/j.msea.2017.01.080 ↗
35. The strength of austenitic stainless steels
36. Effect of chemical composition on work hardening of Fe-Mn-C TWIP steels10.1179/026708309X12535382371852 ↗
37. State-of-the-knowledge on TWIP steel10.1179/1743284711Y.0000000095 ↗
38. The recrystallization process in some polycrystalline metals
39. Single crystal elastic constants of high-manganese transformation-and twinning-induced plasticity steels determined by a new method utilizing nanoindentation10.1016/j.msea.2013.04.049 ↗
40. Effect of iron on mechanical activation and structural evolution of hematite–graphite mixture10.1016/j.jallcom.2008.04.061 ↗
41. X-ray line broadening from field aluminium and wolfram10.1016/0001-6160(53)90006-6 ↗
42. Precipitation hardening of a FeMnC TWIP steel by vanadium carbides
43. Precipitation strengthening in high manganese austenitic TWIP steels10.3139/146.110508 ↗
44. The effect of vanadium micro-alloying on the microstructure and the tensile behavior of TWIP steel10.1016/j.msea.2017.04.083 ↗
45. Interactions between deformation-induced defects and carbides in a vanadium-containing TWIP steel10.1016/j.scriptamat.2012.02.002 ↗
46. Thermodynamic modeling of the stacking fault energy of austenitic steels10.1016/j.actamat.2010.10.037 ↗
47. Continuum understanding of twin formation near grain boundaries of FCC metals with low stacking fault energy10.1038/s41524-017-0023-1 ↗
48. Temperature dependence of deformation behaviors in high manganese austenitic steel for cryogenic applications10.3390/ma14185426 ↗