journal article·2022-11Open access

Combined effect of tungsten inert gas welding and roller expansion processes on mechanical and metallurgical characteristics of heat exchanger tube-to-tubesheet joints

Dinu Thomas Thekkuden, Abdel-Hamid Ismail Mourad, Tholkappiyan Ramachandran, Abdel-Hakim Bouzid, Ravi Kumar, Ahmed Alzamly

Abstract

Tube-to-tubesheet joints are one of the major vulnerable locations prone to cracks in heat exchangers. The manufacturing processes of these joints have an important role in providing structural integrity to the heat exchangers. The main objective of this work is to study the impact of the combined effect of tungsten inert gas weld and expansion percentages of 3%, 5% and 7% on the structural integrity of carbon steel-based tube-to-tubesheet joints. The results show that the pull-out strength of hybrid welded and expanded using 3%, 5% and 7% expansion percentages has exceeded the tube axial strength. The minimum leak path of the welds was satisfactorily above two-thirds of the tube wall thickness. Vickers hardness was restricted at the adjacent regions of weld to below 250 HV. The microstructural studies indicate that the higher the expansion percentage, the smaller the grains at the inner tube surface and the higher the extent the fine grains formed from the inner tube surface. The effect of expansion on the grains at the inner and outer tube surfaces of the transition zone and the unexpanded zone was found negligible. The absence of grain refinement on the outer tube surface using light expansion at a 3% expansion percentage indicated that the contact pressure was inadequate on the tube-to-tubesheet interface. The hardness at the expanded zone and transition zone of the inner tube surface was higher than at the outer tube surface due to the plastic deformation caused by the intensive roller expansion pressure.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Hydrogen embrittlement and corrosion behaviors in metals · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (48)

Show source-provided references
1. Review of common failures in heat exchangers–Part I: mechanical and elevated temperature failures10.1016/j.engfailanal.2020.104396 ↗
2. Failure analysis of stress corrosion cracking in heat exchanger tubes during start-up operation10.1016/j.engfailanal.2015.02.005 ↗
3. Stress corrosion cracking of Ni-resist ductile iron used in manufacturing brine circulating pumps of desalination plants10.1016/j.engfailanal.2008.06.013 ↗
4. Failure analysis of heat exchanger using internal rotary inspection system (IRIS)10.1007/s11668-020-01093-4 ↗
5. Failure analysis on abnormal leakage between tubes and tubesheet of spiral-wound heat exchanger for nuclear power plant10.1016/j.engfailanal.2020.104900 ↗
6. Repair of tube–tubesheet weld cracks in a cracked gas/steam heat exchanger10.1007/s11668-011-9482-8 ↗
7. Failure analysis on leaked titanium tubes of seawater heat exchangers in recirculating cooling water system of coastal nuclear power plant10.1016/j.engfailanal.2019.03.018 ↗
8. Failure analysis of tube-to-tubesheet welded joints in a shell-tube heat exchanger10.1016/j.csefa.2016.06.002 ↗
9. Design, manufacturing and repair of tube-to-tubesheet welds of steam generators of CPR1000 units10.1016/j.nucengdes.2018.04.003 ↗
10. Failure analysis of titanium heater tubes and stainless steel heat exchanger weld joints in nitric acid loop10.1016/j.engfailanal.2019.02.016 ↗
11. Failure analysis of dissimilar weld in heat exchanger10.1016/j.csefa.2017.05.003 ↗
12. Failure analysis of leakage at tube-to-tubesheet joints of a waste heat boiler10.1016/j.engfailanal.2021.105639 ↗
13. Failures and leak inspection techniques of tube-to-tubesheet joints: a review10.1016/j.engfailanal.2021.105798 ↗
14. Residual stresses in roller expanded tube-tubesheet joints with large initial clearance and grooves10.1115/1.4003465 ↗
15. Analysis of residual stresses in the transition zone of tube-to-tubesheet joints
16. A case study on procedure standardization of heat exchanger retubing in KSA oil and gas industries10.1007/s11668-020-00965-z ↗
17. Massey · 2012 · 1
18. Impact of grooves in hydraulically expanded tube-to-tubesheet joints
19. Axial strength of tube-to-tubesheet joints: finite element and experimental evaluations10.1115/1.1398555 ↗
20. Tube expansion and diffusion bonding of 316L stainless steel tube-to-tube sheet joints using a commercial roller tube expander10.1016/j.jmatprotec.2016.03.008 ↗
21. Experimental study of hydraulically expanded tube-to-tubesheet joints for shell-and-tube heat exchangers10.1016/j.proeng.2015.12.220 ↗
22. Impact of expansion pressure on wall thinning and contact pressure for hydraulically expanded tube-to-tubesheet joints: numerical analysis.
23. Investigation of welded structures on mechanical properties of 304L welded tube-to-tubesheet joints10.1016/j.engfailanal.2015.03.003 ↗
24. Influence of neighbouring tube expansion on the residual stress of tubesheet with single-row holes10.1016/j.ijpvp.2022.104651 ↗
25. A study of neighbouring tube expansion effect on the residual contact pressure of tube-to-tubesheet joints10.1016/j.ijpvp.2018.06.011 ↗
26. Comparative study of tube to tubesheet welding qualification on heat exchanger10.1186/s44147-022-00099-z ↗
27. Boiler · 2004 · 48
28. Boiler · 2019 · 585
29. Assuring tube-to-tubesheet joint tightness and strength
30. Reliability factors and tightness of tube-to-tubesheet joints10.1115/1.2842171 ↗
31. An overview of welding aspects and challenges during manufacture of intermediate heat exchangers for 500MWe prototype fast breeder reactor10.1016/j.proeng.2014.11.026 ↗
32. Fatigue life of underwater wet welded low carbon steel SS40010.1016/j.heliyon.2020.e03366 ↗
33. On the yield point phenomenon in low-carbon steels with ferrite-cementite microstructure10.1016/j.msea.2016.07.033 ↗
34. Microstructure and mechanical properties of spray formed 7055 aluminum alloy by underwater friction stir welding10.1016/j.matdes.2013.11.071 ↗
35. Acicular ferrite formation in a medium carbon steel with a two stage continuous cooling10.1016/S1359-6462(99)00149-9 ↗
36. Gas tungsten arc and laser beam welding processes effects on duplex stainless steel 2205 properties10.1016/j.msea.2012.04.012 ↗
37. Critical stress for cleavage fracture in continuously cooled medium carbon V-microalloyed steel10.1016/j.mspro.2014.06.199 ↗
38. Study of the microstructure and mechanical property relationships of shielded metal arc and TIG welded S235JR steel joints10.1016/j.msea.2021.142320 ↗
39. Modelling the evolution of microstructure in steel weld metal
40. Void formation and plastic deformation mechanism of a cold-rolled dual-phase steel during tension10.1007/s40195-019-00967-3 ↗
41. Influence of Bauschinger effect on the residual contact pressure of hydraulically expanded tube-to-tubesheet joints10.1016/j.ijpvp.2016.07.002 ↗
42. Contact pressure in rolled tube-tubesheet joints10.1016/0029-5493(91)90131-Z ↗
43. Modeling the effects of initial tube-tubesheet clearance, wall reduction and material strain hardening on rolled joint strength
44. Basic guidelines of tube expanding n.d. https://www.tcwilson.com/t/tube-rolling-basic-guidelines.
45. Milliams · 2003
46. Beer · 2019
47. Effects of alloying elements on the microstructure and inclusion formation in HSLA multipass welds10.1016/j.matchar.2006.03.004 ↗
48. Ferrite phase analysis based on low-angle grain boundary density in low carbon linepipe steel