Preparation and performance of Sn-based composite solder joints by solid-liquid low-temperature solder bonding technology
Source abstract
Abstract
In the era of big data, the advantages of 3D packaging are becoming increasingly significant. In addition, the mismatch between the coefficient of thermal expansion (CTE) of the PCB and BGA components leads to dynamic warpage of the system, and the expansion and innovation of low-temperature soldering have been a new trend. We developed a fully mixed solder joint of a SAC305(Sn-3.0Ag-0.5Cu wt.%) solder ball and Sn–58Bi(wt.%) solder paste by solid-liquid low-temperature solder bonding technology. The mixing degree and diffusion process of the two were calculated and simulated by mathematical calculation and COMSOL Multiphysics. The results show that a completely mixed solder joint can be obtained after reflow at 210 °C for 5 min. The average shear strength of the composite solder joints was 63.68 ± 1.12 MPa, which was about twice that of the single SAC305 and Sn58Bi solder joints, and the shear fracture was a composite mode of brittle and ductile fracture, which appeared in the IMC and the solder, respectively. After complete mixing, the solder wettability angle was less than 26.68°, with outstanding wetting properties. No phase transition occurred after aging, the distribution of each phase remained uniform, and no enrichment of the brittle phase was observed at the interface. The shear strength decreased slightly with aging time, and the reduction value was less than 10 MPa, which has good reliability.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Low melting point solders based on Sn, Bi, and in elements
2. Effect of Joule heating and current crowding on electromigration in mobile technology10.1063/1.4974168 ↗
3. Enhancement of structure and properties of Sn58Bi solder by AlN ceramic particles10.1016/j.jmrt.2022.06.001 ↗
4. Growth behavior and reliability of interfacial IMC for Sn58Bi/Cu and Sn58Bi–AlN/Cu solder joints applied in IGBT modules10.1016/j.jmrt.2022.11.013 ↗
5. Mechanical properties and microstructure evolution of Cu/Sn58Bi/Cu solder joint reinforced by B4C nanoparticles
6. Scaling effect of interfacial reaction on intermetallic compound formation in Sn/Cu pillar down to 1 μm diameter10.1016/j.actamat.2016.07.004 ↗
7. Abnormal migration behavior and segregation mechanism of Bi atoms undergoing liquid–solid electromigration10.1007/s10853-019-03448-1 ↗
8. Material innovation opportunities for 3D integrated circuits from a wireless application point of view10.1557/mrs.2015.9 ↗
9. A metastable phase of tin in 3D integrated circuit solder microbumps10.1016/j.scriptamat.2015.02.009 ↗
10. Reliability challenges in 3D IC packaging technology10.1016/j.microrel.2010.09.031 ↗
11. Demystifying 3D ICs: the pros and cons of going vertical10.1109/MDT.2005.136 ↗
12. Synergistic effect of electromigration and Joule heating on system level weak-link failure in 2.5 D integrated circuits10.1063/1.4932598 ↗
13. Thermo-mechanical reliability analysis of a RF SiP module based on LTCC substrate10.1016/j.microrel.2017.10.003 ↗
14. Yoshida · 2006 · 6
15. Solder reflow process induced residual warpage measurement and its influence on reliability of flip-chip electronic packages10.1016/j.microrel.2005.06.007 ↗
16. Microstructure and mechanical properties of Sn-In and Sn-Bi solders
17. Microstructure and creep of eutectic indium/tin on copper and nickel substrates10.1007/BF02655434 ↗
18. Microstructure evolution and shear strength of tin-indium-xCu/Cu joints10.3390/met12010033 ↗
19. Characterization of eutectic Sn-Bi solder joints10.1007/BF02655427 ↗
20. Effect of in on microstructure, thermodynamic characteristic and mechanical properties of Sn–Bi based lead-free solder10.1016/j.jallcom.2015.01.219 ↗
21. Comparison of electroplated eutectic Bi/Sn and Pb/Sn solder bumps on various UBM systems10.1109/6104.980035 ↗
22. Improved mechanical properties induced by in and in & Zn double additions to eutectic Sn58Bi alloy10.1007/s10854-019-01056-y ↗
23. Effects of Ni addition on mechanical properties of Sn58Bi solder alloy during solid-state aging10.1016/j.msea.2016.05.015 ↗
24. Interfacial reactions between molten Sn–Bi–X solders and Cu substrates for liquid solder interconnects10.1016/j.actamat.2006.02.030 ↗
25. Use of hop (Humulus lupulus) agricultural by-products for the reduction of aqueous lead (II) environmental health hazards10.1016/S0304-3894(01)00363-6 ↗
26. A review: on the development of low melting temperature Pb-free solders10.1016/j.microrel.2014.02.025 ↗
27. Influence of TiO2 nanoparticles on IMC growth in Sn–3.0 Ag–0.5 Cu–xTiO2 solder joints in reflow process10.1016/j.jallcom.2012.12.019 ↗
28. Intermetallic compound growth suppression at high temperature in SAC solders with Zn addition on Cu and Ni–P substrates10.1016/j.jallcom.2011.09.024 ↗
29. Development of new multicomponent Sn–Ag–Cu–Bi lead-free solders for low-cost commercial electronic assembly10.1016/j.jallcom.2014.12.034 ↗
30. Solder joint reliability on mixed SAC-BiSn ball grid array solder joints formed with resin reinforced Bi-Sn metallurgy solder pastes
31. Sn-3.0 Ag-0.5 Cu/Sn-58Bi composite solder joint assembled using a low-temperature reflow process for PoP technology10.1016/j.matdes.2019.108144 ↗
32. Phase diagram of Ag–Pb–Sn system10.1016/j.calphad.2020.101997 ↗
33. Interface reaction between copper and molten tin–lead solders10.1016/S1359-6454(01)00146-X ↗
34. Interfacial reaction in Cu/Sn/Cu system during the transient liquid phase soldering process10.1016/j.actamat.2010.10.053 ↗
35. Concurrent nucleation, formation and growth of two intermetallic compounds (Cu6Sn5 and Cu3Sn) during the early stages of lead-free soldering10.1016/j.actamat.2011.10.053 ↗
36. Growth mechanisms of Cu3Sn on polycrystalline and single crystalline Cu substrates
37. Effect of interfacial strength between Cu6Sn5 and Cu3Sn intermetallics on the brittle fracture failure of lead-free solder joints with OSP pad finish10.1109/ECTC.2011.5898627 ↗
38. A new low-temperature solder assembly technique to replace eutectic Sn-Bi solder assembly10.3390/mi13060867 ↗
39. Effect of isothermal aging on the microstructure, shear behavior and hardness of the Sn58Bi/Sn3.0Ag0.5Cu/Cu solder joints10.1016/j.rinp.2019.102701 ↗