Fabrication of Ti–Al–Cu new alloys by inductive sintering, characterization, and corrosion evaluation
Source abstract
Abstract
The current work reports the manufacturing and electrochemical characterization of Ti–5%Al–5%Cu, Ti–5%Al–10%Cu, and Ti–5%Al–20%Cu alloys, which were fabricated using mechanical alloying technique. The corrosion of these alloys after varied immersion periods of time in 3.5% NaCl solution was studied using electrochemical impedance spectroscopy (EIS), potentiodynamic polarization, and potentiostatic current time measurements. The phase analyses of the alloys were investigated using X-ray diffraction. Scanning electron microscopy (SEM) was employed to observe the surface morphology of the corroded surfaces whereas the composition of the corrosion products formed on the alloys surfaces was examined using energy dispersive X-ray spectroscopy (EDX). The uniform corrosion of these alloys was found to greatly decrease with the increase of Cu content from 5 wt% to 20 wt%, this occurrence is due to decreasing the values of corrosion current (jCorr) together with corrosion rate (RCorr) and increasing the corrosion resistance (RP). Prolonging the immersion time up to 48 h was found to further increase the values of RP and decrease the values of jCorr and RCorr. Both the electrochemical and the spectroscopic investigations indicated that the increase of Cu content and prolonging the immersion time have significantly decreased all corrosion parameters and increase the corrosion resistance of the alloys in NaCl solution. Keywords: Ti-base alloys, Corrosion, Mechanical alloying, Electrochemical techniques
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Intermetallics and Advanced Alloy Properties · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. Corrosion behavior of two cp titanium dental implants connected by cobalt chromium metal superstructure in artificial saliva and the influence of immersion time10.20964/2016.07.77 ↗
2. Application of titanium and titanium alloys to fixed dental prostheses10.1016/j.jpor.2019.04.011 ↗
3. Microstructure evolution and tensile properties of Ti–6.5Al–2Zr–Mo–V alloy processed with thermo hydrogen treatment10.1016/j.msea.2014.09.104 ↗
4. Effect of heat treatment temperature and exposure period of time on the corrosion of AZ31 alloy and Mg–Ti coupling in sodium chloride solutions
5. Selective laser melting of Ti alloys and Ti matrix composites for biomedical applications: a review10.1002/adem.201500419 ↗
6. Characterization of passive films formed on Ti during anodic oxidation10.1016/j.electacta.2011.07.129 ↗
7. Corrosion of Ti alloys in high temperature near anaerobic seawater10.1016/j.corsci.2015.12.011 ↗
8. Titanium carbide nanofibers-reinforced aluminum compacts, a new strategy to enhance mechanical properties
9. Microstructure and corrosion behaviour of laser metal deposited Ti6Al4V/Cu composites in 3.5% sea water10.1016/j.matpr.2015.07.028 ↗
10. Corrosion behavior of Ti–6Al–4V alloy treated by plasma immersion ion implantation process10.1016/j.surfcoat.2006.03.054 ↗
11. Oxidation behavior and corrosion resistance of Ti–10Ta–10Nb alloy10.1016/j.surfcoat.2008.06.074 ↗
12. Ti its alloys: properties and applications for use as an oral biomaterial: a review
13. Tailoring the surface functionalities of titania nanotube arrays10.1016/j.biomaterials.2009.09.074 ↗
14. Corrosion behaviour of Ti–6Al–4V alloy in concentrated hydrochloric and sulphuric acids10.1023/B:JACH.0000040447.26482.bd ↗
15. Effects of processing on microstructure and mechanical properties of Ti–6Al–4V fabricated using electron beam melting (EBM), part 1: Distance from build plate and part size10.1016/j.msea.2013.02.064 ↗
16. Effects of processing on microstructure and mechanical properties of Ti–6Al–4V fabricated using electron beam melting (EBM), part 2: energy input, orientation, and location10.1016/j.msea.2013.02.065 ↗
17. Ti based biomaterials, the ultimate choice for orthopaedic implants–a review10.1016/j.pmatsci.2008.06.004 ↗
18. Point defect model and corrosion of anodic oxide coatings on Ti–6Al–4V10.1016/j.corsci.2008.02.023 ↗
19. The electrochemical corrosion behavior of TiN and (Ti, Al)N coatings in acid and salt solution10.1016/S0010-938X(02)00223-8 ↗
20. Surface characterization of oxides grown on the Ti–13Nb–13Zr alloy and their corrosion protection10.1016/j.corsci.2013.02.007 ↗
21. Corrosion characterization of Ti alloys by electrochemical techniques10.1016/j.electacta.2005.02.121 ↗
22. Machining of Ti and its alloys–a review10.1243/PIME_PROC_1990_204_047_02 ↗
23. Machinability of a near beta Ti alloy10.1177/2041297511406649 ↗
24. Comparison of the machinabilities of Ti6Al4V and TIMETAL®54M using uncoated WC–Co tools10.1016/j.jmatprotec.2009.08.026 ↗
25. Effect of heat treatment conditions on the machinability of Ti64 and Ti54M alloys10.1016/j.procir.2012.04.085 ↗
26. Cutting tool performance in machining of Ti555.3, Timetal®54M, Ti 6–2–4–6 and Ti 6–4 alloys: a review and analysis
27. Comparative machinability study on Ti54M Ti alloy in different heat treatment conditions10.1177/0954405412466234 ↗
28. Mechanical characterization of Ti–12Mo–13Nb alloy for biomedical application hot swaged and aged10.1590/1516-1439.329614 ↗
29. Effects of graphite on the corrosion behavior of aluminum-graphite composite in sodium chloride solutions10.1016/S1452-3981(23)15058-9 ↗
30. Effects of exposure time on the anodic dissolution of Monel-400 in aerated stagnant sodium chloride solutions10.1007/s10008-011-1438-0 ↗
31. Fabrication of exfoliated graphite nanoplatelets-reinforced aluminum composites and evaluating their mechanical properties and corrosion behavior10.1016/j.jaap.2011.09.003 ↗
32. 2014
33. 2014
34. Systematic analysis of the structural, elastic, and electronic properties of Ti–Cu–Me (Me=Al, Ga and In) ternary intermetallics10.1016/j.jpcs.2013.10.008 ↗
35. Effect of nickel content on the corrosion resistance of iron–nickel alloys in concentrated hydrochloric acid pickling solutions
36. Corrosion passivation in simulated body fluid of magnesium/hydroxyapatite nanocomposites sintered by high frequency induction heating10.1016/S1452-3981(23)19673-8 ↗
37. The beneficial effect of ruthenium additions on the passivation of duplex stainless steel corrosion in sodium chloride solutions10.1016/j.corsci.2009.03.022 ↗
38. Electrochemical behaviour and corrosion inhibition of Al, Al-6061 and Al–Cu in neutral aqueous solutions10.1016/S0010-938X(98)00145-0 ↗
39. Effects of 1,4-naphthoquinone on aluminum corrosion in 0.50M sodium chloride solutions10.1016/j.electacta.2005.06.018 ↗
40. Impedance studies of corrosion resistance of aluminium in chloride media
41. The chemical nature of aluminum corrosion-V. Energy transfer in aluminum dissolution10.1149/1.2123881 ↗
42. Electrochemical study of the pitting corrosion of aluminium and its alloys–II. Study of the interaction of chloride ions with a passive film on aluminium and initiation of pitting corrosion10.1016/0013-4686(89)87119-1 ↗
43. The dissolution of porous oxide films on aluminium10.1016/0013-4686(70)85002-2 ↗
44. Kinetics of the dissolution of phosphoric acid anodized aluminium as revealed from impedance measurements in phosphate media
45. Relationship between induction time for pitting and pitting potential for high-purity aluminum10.1149/1.1731487 ↗
46. Formation of Ti oxide films on Ti and Ti6Al4V by O2-plasma immersion ion implantation10.1016/S0257-8972(00)00712-X ↗
47. Inhibition of copper corrosion in 3.0% NaCl solution by N-phenyl-1,4-phenylenediamine10.1149/1.2018254 ↗