Microstructural and mechanical properties of inconel 600/ZrB2-SiC joints brazed with AgCu/Cu-foam/AgCu/Ti multi-layered composite filler
Source abstract
Abstract
A set of AgCu/Cu-foam/AgCu/Ti multi-layered composite fillers was designed and employed to braze the Inconel 600 alloy and ZrB2-SiC ceramic. Microstructures, formation mechanism and shear strengths of the joints were investigated in detail with and without the addition of Ti foil. The shear strengths of the brazed joints were improved substantially with the presence of Ti foils. A maximum gain of 150 % was reached from 77 MPa to 198 MPa after introducing the Ti foil and brazing the joint at a 1173 K for 15 min. The mechanical property enhancement is attributed to a newly formed TiC phase, release of residual stress, and barrier effect of Cu foam to inhibit formation of Ti-Ni intermetallic compounds.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Joining ceramics to metals using metallic foam10.1016/j.msea.2008.06.007 ↗
2. Strain energy distribution in ceramic to metal joints10.1016/S1359-6454(01)00352-4 ↗
3. Preparation of high solid loading, low viscosity ZrB2-SiC aqueous suspensions using PEI as dispersant10.1016/j.ceramint.2012.08.073 ↗
4. Fabrication and characterization of B4C-ZrB2-SiC ceramics with simultaneously improved high temperature strength and oxidation resistance up to 1600 degrees C10.1016/j.ceramint.2016.01.202 ↗
5. Brazing of C/C composites to Ti6Al4V using graphene nanoplatelets reinforced TiCuZrNi brazing alloy10.1016/j.matlet.2016.07.111 ↗
6. Joining of ZrB2-based ultra-high-temperature ceramic composites using Pd-based braze alloys
7. Carbon nanotubes-reinforced Ni foam interlayer for brazing SiO2-BN with Ti6Al4V alloy using TiZrNiCu brazing alloy10.1016/j.ceramint.2017.11.136 ↗
8. Microstructural evolution and thermal stress relaxation of Al2O3/1Cr18Ni9Ti brazed joints with nickel foam10.1016/j.vacuum.2017.10.030 ↗
9. Brazing ZTA ceramic to TC4 alloy using the Cu foam as interlayer10.1016/j.vacuum.2018.05.038 ↗
10. Brazing ZrB2-SiC ceramics to Inconel 600 alloy without and with Cu foam10.1016/j.jmapro.2019.03.023 ↗
11. AgCuTi/graphene-reinforced Cu foam: a novel filler to braze ZrB2-SiC ceramic to Inconel 600 alloy10.1016/j.ceramint.2019.08.293 ↗
12. Calculations of mixing enthalpy and mismatch entropy for ternary amorphous alloy10.2320/matertrans1989.41.1372 ↗
13. Microstructure and strengthening mechanism of Si3N4/Invar joint brazed with TiNp-doped filler10.1016/j.msea.2015.10.038 ↗
14. Brazing of Inconel 600 by active filler metal10.1179/1432891714Z.000000000968 ↗
15. Effect of brazing temperature on the shear strength of Inconel 600 joint10.1007/s00170-014-5900-x ↗
16. The effects of additive elements on the microstructure characteristics and mechanical properties of Cr–Fe–C hard-facing alloys10.1016/j.jallcom.2010.03.127 ↗
17. (Fe, Cr)7C3/Fe surface gradient composite: microstructure, microhardness, and wear resistance10.1016/j.matchemphys.2014.06.026 ↗
18. Effects of rod carbide size, content, loading and sliding distance on the friction and wear behaviors of (Cr,Fe)7C3-reinforced α-Fe based composite coating produced via PTA welding process10.1016/j.surfcoat.2014.03.029 ↗
19. Brazing joining of Ti3AlC2 ceramic and 40Cr steel based on Ag-Cu-Ti filler Metal10.1016/j.jmatprotec.2017.08.017 ↗
20. Effect of holding time on microstructure and mechanical properties of ZrO2/TiAl joints brazed by Ag–Cu filler metal10.1016/j.matdes.2015.08.020 ↗
21. Microstructure and brazing mechanism of porous Si3N4/Invar joint brazed with Ag-Cu-Ti/Cu/Ag-Cu multi-layered filler10.1016/j.jmst.2017.07.001 ↗
22. Brazing of SiO2f/SiO2 composite modified with few-layer graphene and Invar using AgCuTi alloy10.1016/j.matdes.2015.08.146 ↗
23. Microstructure and shear strength of ZrB2-SiC/Ti-6Al-4V joint by TiCuZrNi with Cu foam10.1016/j.ceramint.2019.02.074 ↗
24. Microstructure and mechanical properties of Al2O3 ceramic and Ti6Al4V alloy joint brazed with inactive Ag-Cu and Ag-Cu+B10.1016/j.jeurceramsoc.2016.02.033 ↗
25. Microstructural evolution mechanisms of Ti600 and Ni-25%Si joint brazed with Ti-Zr-Ni-Cu amorphous filler foil10.1016/j.jmatprotec.2016.10.021 ↗
26. Microstructural evolution mechanisms of Ti600 and Ni-25%Si joint brazed with Ti-Zr-Ni-Cu amorphous filler foil10.1016/j.jmatprotec.2016.10.021 ↗
27. Reaction-composite brazing of carbon fiber reinforced SiC composite and TC4 alloy using Ag-Cu-Ti-(Ti+C) mixed powder10.1016/j.msea.2012.11.031 ↗
28. ZrB2-SiC/Ti6Al4V joints: wettability studies using Ag- and Cu-based braze alloys10.1007/s10853-012-6790-7 ↗
29. Brazing joining of Ti3AlC2 ceramic and 40Cr steel based on Ag-Cu-Ti filler Metal10.1016/j.jmatprotec.2017.08.017 ↗
30. In-Situ synthesized TiC nano-flakes reinforced C/C composite-Nb brazed joint10.1016/j.jeurceramsoc.2017.11.059 ↗
31. Brazing of CBN grains with Ag-Cu-Ti/TiX composite filler-the effect of TiX particles on microstructure and strength of bonding layer10.1016/j.matdes.2016.03.033 ↗
32. Synthesis of titanium carbide/chromium carbide multilayers by the co-evaporation of multiple ingots by electron beam physical vapor deposition10.1016/S0257-8972(02)00404-8 ↗