The microstructure and wear behavior of an Al–7Si alloy reinforced with in situ Al3Ti particulates were studied. The effects of Sr modification and heat treatment were also investigated. Sr and Al3Ti particulates had clear effects on modifying the morphology of eutectic Si and the microstructure of the Al–Si alloy, playing a key role in improving the hardness and wear properties of the Al3Ti/Al–7Si–Sr composite. T6 heat treatment was performed to spheroidized coarse eutectic Si, reducing stress concentration and further improving the hardness and wear properties of the composites. Among them, the Al3Ti/Al–7Si–Sr composite displayed the highest hardness and the lowest friction coefficient in both as-cast and T6 heat treated states attributed to the combined effects of Sr modification and Al3Ti reinforcement.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Influence of Ti addition on wear properties of Al–Si eutectic alloys10.1016/S0043-1648(01)00687-1 ↗
2. A parametric study of the relationship between microstructure and wear resistance of Al–Si alloys10.1016/j.wear.2006.03.043 ↗
3. Study on wear properties of aluminium–silicon piston alloy10.1016/S0924-0136(01)00869-X ↗
4. Influence of wear parameters on friction performance of A356 aluminum–graphite/granite particulates reinforced metal matrix hybrid composites10.1016/j.heliyon.2019.e01770 ↗
5. Wear performance of A356 matrix composites reinforced with different types of reinforcing particulates10.1007/s11665-017-2901-6 ↗
6. Tailoring in-situ TiB2 particulates in aluminum matrix composites10.1016/j.msea.2017.08.047 ↗
7. In situ fabrication of Al3Ti particulate reinforced aluminium alloy metal-matrix composites10.1016/j.msea.2003.08.049 ↗
8. The role of strontium in modifying aluminium-silicon alloys10.1016/j.actamat.2012.03.031 ↗
9. Eutectic modification and microstructure development in Al–Si Alloys10.1016/j.msea.2005.09.055 ↗
10. Effects of solution treatment on microstructures and micro-hardness of a Sr-modified Al–Si–Mg alloy10.1016/j.msea.2018.04.049 ↗
11. Heat treatment as a route to tailor the yield-damping properties in A356 alloys10.1016/j.msea.2018.05.042 ↗
12. Heat-treatment induced defect formation in α-Al matrix in Sr-modified eutectic Al–Si alloy10.1016/j.jallcom.2017.09.324 ↗
13. Effects of processing parameters on the microstructures and mechanical properties of in situ (Al3Ti+Al2O3)/Al composites fabricated by hot pressing and subsequent friction-stir processing10.1007/s11661-014-2221-5 ↗
14. Microstructures and mechanical properties of Al3Ti/Al composites produced in situ by high shearing technology10.1002/adem.201800259 ↗
15. Microstructures and mechanical properties of in-situ Al3Ti/2024Al composites after solution and subsequent aging treatment10.1016/j.msea.2018.03.089 ↗
16. 3D micromechanical simulation of the mechanical behavior of an in-situ Al3Ti/A356 composite10.1016/j.compositesb.2019.107115 ↗
17. The in-situ formation of Al3Ti reinforcing particulates in an Al–7wt%Si alloy and their effects on mechanical properties10.1016/j.jallcom.2019.04.064 ↗
18. In situ formed Al3Ti particulates in Al alloy matrix and their effects on the microstructure and mechanical properties of 7075 alloy10.1557/jmr.2014.123 ↗
19. Development of Al3Ti and Al3Zr intermetallic particulate reinforced aluminum alloy AA6061 in situ composites using friction stir processing10.1016/j.matdes.2014.06.008 ↗
20. Effect of Sr-grain refining-Si interactions on the microstructural characteristics of Al–Si hypoeutectic alloys
21. Eutectic morphology evolution and Sr-modification in Al–Si based alloys studied by 3D phase-field simulation coupled to Calphad data10.1088/1757-899X/84/1/012084 ↗
22. X-ray nano-diffraction study of Sr intermetallic phase during solidification of Al–Si hypoeutectic alloy10.1063/1.4865496 ↗
23. Mechanical properties and fracture of in-situ Al3Ti particulate reinforced A356 composites10.1016/j.msea.2019.03.044 ↗
24. Effects of strontium and heat treatment on the wear-corrosion property of Al–7Si–0.3Mg alloy10.1016/j.matchemphys.2012.05.015 ↗
25. Improvement in tensile strength and load bearing capacity during dry wear of Al–7Si alloy by combined grain refinement and modification10.1016/j.msea.2004.12.053 ↗
26. Ultrasound assisted in-situ casting technique for synthesizing small-sized blocky Al3Ti particulates reinforced A356 matrix composites with improved mechanical properties10.1016/j.jallcom.2018.02.010 ↗
27. Substitution behavior of Si in Al3Ti (D022): a first-principles study
28. Processing and tensile properties of A356 composites containing in situ small-sized Al3Ti particulates10.1016/j.msea.2017.11.005 ↗
29. Dry wear and friction properties of an A356/SiC foam interpenetrating phase composite10.1016/j.wear.2011.07.008 ↗
30. Contact and rubbing of flat surfaces10.1063/1.1721448 ↗
31. Tribological properties of A356 Al–Si alloy composites under dry sliding conditions10.1108/ILT-06-2011-0047 ↗
32. Dry sliding tribological properties of a dendrite-reinforced Zr-based bulk metallic glass matrix composite10.1016/j.jmst.2014.05.004 ↗
33. A novel bronze-impregnated carbon strip containing Al2O3 particulates for subway current collectors10.1016/j.wear.2011.01.032 ↗
34. Solute adsorption and entrapment during eutectic Si growth in A–Si-based alloys10.1016/j.actamat.2014.09.040 ↗
35. Evaluation of microstructure and wear behavior of friction stir processed cast aluminum alloy10.1016/j.matchar.2011.11.007 ↗
36. Effect of grain refinement and modification on the dry sliding wear behaviour of eutectic Al–Si alloys10.1016/j.triboint.2008.05.012 ↗
37. Effect of temperature on the wear behavior of Al–7Si–TiB2 in-situ composites10.1007/s11661-008-9696-x ↗
38. Effect of grain refining and Sr-modification interactions on the impact toughness of Al–Si–Mg cast alloys10.1016/j.matdes.2013.10.029 ↗
39. Thermal stability and its effects on the mechanical properties of rapidly solidified Al–Ti alloys10.1016/S0921-5093(00)00886-8 ↗
40. Micro structural features and mechanical properties of Al–Al3Ti composite fabricated by in-situ powder metallurgy route10.1016/j.jallcom.2008.05.068 ↗
41. Strengthening mechanisms in ultrasonically processed aluminium matrix composite with in-situ Al3Ti by salt addition10.1016/j.compositesb.2017.12.005 ↗