journal article·2022-07Open access

Microstructure and mechanical behaviors of Ti3AlC2 triggered in-situ Al3Ti and TiC reinforced 2024Al composite

Yuanbo Wang, Zhenying Huang, Wenqiang Hu, Qun Yu, Hongjie Wang, Xue Li, Davoud Dastan, Yang Zhou

Abstract

In this work, 2024Al matrix composite reinforced by in-situ Al3Ti and TiC was fabricated using hot-press sintering Ti3AlC2 and 2024Al powders. The effect of Ti3AlC2 precursor additions (10, 20 and 30 vol.%) on microstructure and mechanical properties of Al3Ti-TiC/2024Al composites were investigated. It was found that Ti3AlC2 decomposed into submicron TiC particles at 950 °C, while Al atoms reacted with Ti to form Al3Ti. In-situ Al3Ti and submicron TiC were homogeneously distributed in 2024Al matrix. The high temperature tensile and compressive behavior of the in-situ Al3Ti-TiC/2024Al composites was tested in the temperature range of 25–400 °C. The results indicated that the tensile and compressive properties of the material showed temperature dependence. The 20 vol.% Ti3AlC2/2024Al composite exhibit a higher tensile yield strength of 368 MPa with a noticeable elongation of 5.4% at room temperature compared to the pure 2024Al (tensile yield strength is 146 MPa with elongation of 8.5%). At 300 and 400 °C, the tensile yield strength of the as-sintered 30 vol.% Ti3AlC2/2024Al composite was determined to be 176 and 126 MPa, increased by 96% and 293%, respectively, compared with that of pure 2024Al alloy. The excellent tensile property of Al3Ti-TiC/2024Al composites can be ascribed to the synergistic strengthening effect in term of dislocation density, load transfer and dispersion strengthening.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: MXene and MAX Phase Materials · Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. Preparation, thermal analysis and mechanical properties of in-situ Al2O3/SiO2(p)/Al composites fabricated by using zircon tailing sand10.1016/j.matdes.2016.03.064 ↗
2. Microstructure and mechanical characterization of in situ synthesized AA6061/(TiB2+Al2O3) hybrid aluminum matrix composites10.1016/j.jallcom.2018.01.016 ↗
3. In situ aluminum matrix composites fabricated from Al–Ni2O3 system through microwave synthesis10.1016/j.matchemphys.2015.01.021 ↗
4. Superior high-temperature tensile properties of aluminum matrix composites reinforced with carbon nanotubes10.1016/j.carbon.2022.02.009 ↗
5. High-temperature tensile and tribological behavior of hybrid (ZrB2+Al3Zr)/AA5052 in situ composite. Metallurgical and materials transactions10.1007/s11661-016-3635-z ↗
6. A comprehension review of dry sliding wear on aluminum matrix composites10.1016/j.matpr.2021.11.312 ↗
7. Dynamic cutting force model for cutting SiCp/Al composites considering particle characteristics stochastic models10.1016/j.ceramint.2021.09.066 ↗
8. Selective laser melting of SiCp/Al composites: densification, microstructure, and mechanical and tribological properties10.1016/j.ceramint.2021.07.263 ↗
9. Microstructure, mechanical properties and machinability of particulate reinforced Al matrix composites: a comparative study between SiC particles and high-entropy alloy particles10.1016/j.jmrt.2020.09.034 ↗
10. Evaluation of microstructure and mechanical properties of Al-TiC metal matrix composite prepared by conventional, microwave and spark plasma sintering methods10.3390/ma10111255 ↗
11. The deformation of B 4 C particle in the B 4 C/2024Al composites after high velocity impact10.1016/j.micron.2014.07.006 ↗
12. Enhanced strength and ductility in ZrB2/2024Al nanocomposite with a quasi-network architecture10.1016/j.jallcom.2018.11.214 ↗
13. Selective laser melting of nano-TiB 2 decorated AlSi10Mg alloy with high fracture strength and ductility10.1016/j.actamat.2017.02.062 ↗
14. Microstructural, mechanical, and wear properties characterization and strengthening mechanisms of Al7075/SiCnp composites processed through ultrasonic cavitation assisted stir-casting10.1016/j.msea.2020.140553 ↗
15. The challenge of ceramic/metal microcomposites and nanocomposites10.1016/j.pmatsci.2006.09.003 ↗
16. Ti2AlC triggered in-situ ultrafine TiC/Inconel 718 composites: microstructure and enhanced properties10.1016/j.jmst.2020.04.002 ↗
17. Effect of initial Ti powders size on the microstructures and mechanical properties of Al3Ti/2024 Al composites prepared by ultrasonic assisted in-situ casting10.1016/j.jallcom.2016.10.039 ↗
18. Effect of reaction temperature on the microstructures and mechanical properties of high-intensity ultrasonic assisted in-situ Al3Ti/2024 Al composites10.1016/j.jallcom.2016.01.121 ↗
19. Design, microstructure and high temperature properties of in-situ Al3Ti and nano-Al2O3 reinforced 2024Al matrix composites from Al-TiO2 system10.1016/j.jallcom.2018.09.376 ↗
20. Ti3AlC2 coatings deposited by liquid plasma spraying10.1016/j.surfcoat.2016.04.076 ↗
21. Microstructure and mechanical properties of TiC0.5 reinforced copper matrix composites10.1016/j.msea.2013.09.054 ↗
22. Microstructural characterization and compression properties of TiC0.61/Cu(Al) composite synthesized from Cu and Ti3AlC2 powders10.1016/j.jallcom.2014.02.159 ↗
23. In-situ TiC and γ′-Ni3(Al,Ti) triggered microstructural modification and strengthening of Ni matrix composite by reactive hot-press sintering pure Ni and Ti2AlC precursor10.1016/j.jallcom.2018.03.069 ↗
24. Investigation on high temperature mechanical behaviors of TiC-γ′ reinforced Ni composite10.1007/s12540-020-00615-x ↗
25. Effect of in situ formed TiCx grains on the microstructural modification of high chromium white iron10.1016/j.jallcom.2017.07.274 ↗
26. In situ formed TiCx in high chromium white iron composites: formation mechanism and influencing factors10.1016/j.jallcom.2019.02.292 ↗
27. Thermal properties of graphene/metal composites with aligned graphene[J]10.1016/j.matdes.2017.11.048 ↗
28. Interface and mechanical/thermal properties of graphene/copper composite with Mo2C nanoparticles grown on graphene10.1016/j.compositesa.2018.03.014 ↗
29. Investigation on the wear resistance and mechanical properties of Al/Ti3SiC2 composites fabricated by the spark plasma sintering10.1016/j.mtcomm.2021.102270 ↗
30. High plasticity achieved by spark plasma sintering method in aluminum matrix composites reinforced with Ti2AlC particles10.1016/j.matchar.2021.111204 ↗
31. Powder metallurgy processing and compressive properties of Ti3AlC2/Al composites10.1016/j.msea.2011.09.068 ↗
32. Preparation and characteristics of Ti3AlC2 -Al3Ti/Al composite materials synthesized from pure Al and Ti3AlC2 powders10.1016/j.matchar.2021.111298 ↗
33. Phase equilibria at 1000°C in the AI-C-Si-Ti quaternary system: an experimental approach10.1016/S0921-5093(97)00002-6 ↗
34. High strengthening effects and excellent wear resistance of Ti3Al(Si)C2 solid solutions10.1111/ijac.13264 ↗
35. Shear strength and shear failure of layered machinable Ti3AlC2 ceramics10.1016/S0955-2219(03)00328-5 ↗
36. Reaction in Al-Ti-C powders and its relation to the formation and stability of TiC in Al at high temperatures10.1016/S1359-6462(00)00356-0 ↗
37. Microstructure and properties of Al3Zr/2024Al in situ composites after forging10.1007/s12598-015-0569-3 ↗
38. In situ (Al3Zrp+Al2O3np)/2024Al metal matrix composite with controlled reinforcement architecture fabricated by reaction hot pressing10.1016/j.msea.2013.07.002 ↗
39. Mechanical properties and fracture of in-situ Al3Ti particulate reinforced A356 composites10.1016/j.msea.2019.03.044 ↗
40. Microstructural, mechanical, and wear properties characterization and strengthening mechanisms of Al7075/SiCnp composites processed through ultrasonic cavitation assisted stir-casting10.1016/j.msea.2020.140553 ↗
41. Studies on squeeze casting of Al 2124 alloy and 2124-10% SiCp metal matrix composite10.1016/j.msea.2008.01.054 ↗
42. Preparation of 6061Al-Al 2 O 3 MMC's by stir casting and evaluation of mechanical and wear properties10.1016/j.mspro.2014.07.151 ↗
43. Interface optimization strategy for enhancing the mechanical and thermal properties of aligned graphene/Al composite[J]10.1016/j.jallcom.2021.163555 ↗
44. High strength and good ductility at elevated temperature of nano-SiCp/Al2014 composites fabricated by semi-solid stir casting combined with hot extrusion10.1016/j.msea.2014.12.089 ↗
45. Particle-reinforced aluminum matrix composites produced from powder mixtures via friction stir processing10.1016/j.compscitech.2011.01.013 ↗
46. Thermal expansion of select M > n+1 > AX > n (M=Early transition metal, A=A group element, X=C or N) phases measured by high temperature x-ray diffraction and dilatometry
47. A novel TiAl3/Al2O3 composite coating on γ-TiAl alloy and evaluating the oxidation performance10.1016/j.apsusc.2015.11.155 ↗
48. Thermal shock behavior of a novel TiCx–Ni3(Al,Ti)/Ni functionally graded composite10.1007/s12540-020-00836-0 ↗
49. Thermal expansion responses of pressure infiltrated SiC/Al metal-matrix composites10.1023/A:1018535108269 ↗
50. Strengthening mechanisms in ultrasonically processed aluminium matrix composite with in-situ Al3Ti by salt addition10.1016/j.compositesb.2017.12.005 ↗
51. Strengthening in Al alloy nano composites fabricated by ultrasound assisted solidification technique10.1016/j.msea.2015.10.118 ↗
52. Tensile behavior and strengthening mechanism in ultrafine TiC0.5 particle reinforced Cu–Al matrix composites10.1016/j.jallcom.2014.10.123 ↗
53. Prediction models for the yield strength of particle-reinforced unimodal pure magnesium (Mg) metal matrix nanocomposites (MMNCs)10.1007/s10853-013-7232-x ↗
54. Grain refinement and crack inhibition of selective laser melted AA2024 aluminum alloy via inoculation with TiC–TiH210.1016/j.msea.2021.141171 ↗