Effect of Ce content on the microstructure and mechanical properties of squeeze-cast Al–5Mg-2.2Si-0.6Mn alloys
Source abstract
Abstract
The effect of Ce in amount of 0–0.5 wt.% on the microstructure and mechanical properties of the squeeze-cast Al–5Mg-2.2Si-0.6Mn alloys produced by squeeze casting technique was explored. The microstructure was observed by optical microscopy and scanning electron microscopy. The hardness and mechanical properties of the alloys were measured by Vickers hardness and tensile test. The microstructure of the squeeze-cast Al–5Mg-2.2Si-0.6Mn alloys is composed mainly of α-Al, Al–Mg2Si eutectic cells, the bulky lath-shaped Al8CeMn4 phase, Al2Mn3 and Al5Mn2Si5 phases after Ce is added. The results show that the addition of Ce leads to the grain refinement, which can improve the mechanical properties. When adding superfluous Ce, the formation of coarse and brittle Al8CeMn4 phase seriously reduces the mechanical properties of the alloy. With the increase of Ce content, the secondary dendrite arm spacing of different alloys decreases first and then increases, hence the hardness and tensile properties increase first and then decrease. The most remarkable improvement in the mechanical properties was acquired in the alloy with 0.10 wt.% Ce addition, the hardness reaches 48.1 HV, the ultimate tensile strength, yield strength and elongation are 265.5 MPa, 185.8 MPa and 5.8%, respectively.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. Estimating increasing diversity and dissipative loss of critical metals in the aluminum automotive sector, Resources10.1016/j.resconrec.2019.06.016 ↗
2. Evaluation and analysis of new-energy vehicle industry policies in the context of technical innovation in China10.1016/j.jclepro.2020.125126 ↗
3. Impacts of vehicle weight reduction via material substitution on life-cycle greenhouse gas emissions10.1021/acs.est.5b03192 ↗
4. Recent development in aluminium alloys for the automotive industry10.1016/S0921-5093(99)00653-X ↗
5. High-pressure die-cast (HPDC) aluminium alloys for automotive applications10.1533/9780857095466.109 ↗
6. Features of structure formation and changes in the mechanical properties of cast Al-Mg-Si-Mn alloy with the addition of (Ti + Zr)10.14311/AP.2015.55.0282 ↗
7. Effects of Zr, Ti and Sc additions on the microstructure and mechanical properties of Al-0.4Cu-0.14Si-0.05Mg-0.2Fe alloys10.1016/j.jmst.2018.05.011 ↗
8. Microstructure characteristics and mechanical properties of new aerospace Al-Mg-Mn alloys with Al3(Sc1−xZrx) or Al3(Er1−xZrx) nanoparticles10.1016/j.matchar.2019.04.032 ↗
9. Effect of La addition on microstructure and mechanical properties of hypoeutectic Al-7Si aluminum alloy10.1007/s41230-021-0137-4 ↗
10. Effects of Nd on microstructure and mechanical properties of cast Al-Si-Cu-Ni-Mg piston alloys10.1016/j.jallcom.2016.10.300 ↗
11. Effects of rare earth elements on microstructure and tensile properties of Al-Si-Cu alloy at 250 °C10.1007/s41230-021-1020-z ↗
12. Effect of Zr, Cr and Sc on the Al-Mg-Si-Mn high-pressure die casting alloys10.1016/j.msea.2019.05.038 ↗
13. Effect of Sc and Zr on microstructures and mechanical properties of as-cast Al-Mg-Si-Mn alloys10.1016/S1003-6326(08)60309-X ↗
14. Multi-alloying effect of Sc, Zr, Cr on the Al-Mg-Si-Mn high-pressure die casting alloys10.1016/j.matchar.2020.110537 ↗
15. Microalloying of Sc, Ni, and Ce in an advanced Al-Zn-Mg-Cu alloy10.1007/s11661-999-0154-1 ↗
16. Effect of cerium and yttrium on aging processes in alloys of the Al-Mg system
17. Achievement of high strength and ductility in Al-Si-Cu-Mg alloys by intermediate phase optimization in as-cast and heat treatment conditions10.3390/ma13030647 ↗
18. Effect of ε-Al3Ni phase on mechanical properties of Al–Si–Cu–Mg–Ni alloys at elevated temperature10.1016/j.msea.2019.138794 ↗
19. Effect of cerium on microstructure, mechanical properties and corrosion properties of Al-Zn-Mg alloy10.1016/j.jre.2020.07.010 ↗
20. Effect of heat treatment on microstructure, hardness and corrosion resistance of 7075 Al alloys fabricated by SLM10.1016/j.jmapro.2020.10.071 ↗
21. Fundamentals of solidification in aluminum castings10.1007/BF03355567 ↗
22. Fundamentals of solidification10.1002/crat.2170210909 ↗