Brazing of Ti-coated SiC using a CoFeCrNiCu high entropy alloy filler via electric field-assisted sintering
Source abstract
Abstract
Electric field-assisted sintering technology (FAST) was used to join SiC ceramic by using a CoFeCrNiCu high-entropy alloy filler. A thin Ti film was deposited on SiC surface by physical vapor deposition to reduce the residual thermal stress in the joint. The microstructure, bending strength, and bonding mechanism were systematically investigated. It was found that a discontinuous TiC layer could be formed at the interface and the interfacial reaction products changed with different brazing temperatures. A joint with a bending strength of 72 MPa was achieved at 1200 °C, which is 73% higher than that of the SiC brazed without Ti coating. This work provides a new insight in the interfacial design of ceramic brazing with high mechanical properties.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. Liquid phase sintering and characterization of SiC ceramics10.1016/j.ceramint.2018.03.083 ↗
2. Radiation-tolerant joining technologies for silicon carbide ceramics and composites10.1016/j.jnucmat.2013.10.002 ↗
3. KD-S SiCf/SiC composites with BN interface fabricated by polymer infiltration and pyrolysis process10.1007/s40145-018-0268-2 ↗
4. Interfacial characterization in the brazing of silicon nitride to niobium joining using a double interlayer10.1016/j.matchar.2017.07.026 ↗
5. Laser-induced metallization of porous Si3N4 ceramic and its brazing to TiAl alloy10.1111/jace.15937 ↗
6. Wetting behavior and brazing of titanium-coated SiC ceramics using Sn0.3Ag0.7Cu filler10.1111/jace.16827 ↗
7. Brazing of carbon fiber reinforced SiC composite and TC4 using Ag–Cu–Ti active brazing alloy10.1016/j.msea.2009.09.024 ↗
8. Influence of interfacial reaction on reactive wettability of molten Ag-Cu-X wt.%Ti filler metal on SiC ceramic substrate and mechanism analysis10.1016/j.apsusc.2017.12.106 ↗
9. Brazing of silicon carbide ceramics with Ni-Si-Ti powder mixtures10.1007/s41779-017-0061-7 ↗
10. Effect of Ti addition on the wetting and brazing of Sn0.3Ag0.7Cu filler on SiC ceramic10.1111/jace.16245 ↗
11. Interfacial microstructure characterization and strength evaluation of Si3N4/Si3N4 joints with Si–Mg composite filler for high-temperature applications10.1016/j.ceramint.2021.04.252 ↗
12. Joining of alumina ceramics using silicon–magnesium composite filler for high-temperature applications10.1080/13621718.2020.1714874 ↗
13. A new high entropy alloy brazing filler metal design for joining skutterudite thermoelectrics to copper10.1016/j.jallcom.2020.157750 ↗
14. Laser brazing of a nickel-based superalloy using a Ni-Mn-Fe-Co-Cu high entropy alloy filler metal10.1016/j.matlet.2017.12.003 ↗
15. Evaluation of dissimilar metal joining of aluminum alloy to stainless steel using the filler metals with a high-entropy design10.1016/j.jmapro.2020.08.031 ↗
16. Application of the eutectic high entropy alloy Nb0.73CoCrFeNi2.1 for high temperature joints10.1007/s40194-020-00944-w ↗
17. Interfacial microstructure and mechanical properties of ZrB2-SiC-C ceramic and GH99 superalloy joints brazed with a Ti-modified FeCoNiCrCu high-entropy alloy10.1016/j.matdes.2016.02.055 ↗
18. Effects of the elemental composition of high-entropy filler metals on the mechanical properties of dissimilar metal joints between stainless steel and low carbon steel10.1016/j.jmrt.2020.08.028 ↗
19. A novel high entropy CoFeCrNiCu alloy filler to braze SiC ceramics10.1016/j.jeurceramsoc.2020.03.044 ↗
20. Brazing ZrB2-SiC ceramics to Nb with a novel CoFeNiCrCu high entropy alloy10.1016/j.jeurceramsoc.2020.08.050 ↗
21. Microstructure and mechanical properties of ZrB2-SiC/Nb joints brazed with CoFeNiCrCuTi x high-entropy alloy filler10.1111/jace.17732 ↗
22. Joining of β-SiC by spark plasma sintering10.1016/j.jeurceramsoc.2013.12.023 ↗
23. Fast joining SiC ceramics with Ti3SiC2 tape film by electric field-assisted sintering technology10.1016/j.jnucmat.2015.08.004 ↗
24. Facile preparation of in situ coated Ti3C2Tx/Ni0.5Zn0.5Fe2O4composites and their electromagnetic performance10.1039/C7RA03402D ↗
25. Joining of CVD-SiC coated and uncoated fibre reinforced ceramic matrix composites with pre-sintered Ti3SiC2 MAX phase using Spark Plasma Sintering10.1016/j.jeurceramsoc.2016.06.025 ↗
26. Flash joining of CVD-SiC coated Cf/SiC composites with a Ti interlayer10.1016/j.jeurceramsoc.2017.05.016 ↗
27. Microstructural evolution and mechanical properties of the joint of TiAl alloys and C/SiC composites vacuum brazed with Ag–Cu filler metal10.1016/j.matchar.2011.05.007 ↗
28. Microstructures and mechanical properties of Cf/SiC composite and TC4 alloy joints brazed with (Ti–Zr–Cu–Ni)+W composite filler materials10.1016/j.compscitech.2014.03.021 ↗
29. Interfacial microstructure and mechanical properties of zirconia ceramic and niobium joints vacuum brazed with two Ag-based active filler metals10.1016/j.ceramint.2016.05.045 ↗
30. Wetting behaviour of silicon nitride ceramics by Ti–Cu alloys10.1016/j.ceramint.2006.10.022 ↗
31. Joining of Cf/SiBCN composite with CuPd-V filler alloy10.1016/j.jmst.2018.01.001 ↗
32. Wettability of transparent YAG (Y3Al5O12) by molten Ag–Cu–Ti alloys10.1016/j.jeurceramsoc.2015.03.036 ↗
33. Effect of Ti content on the wetting behavior of Sn0.3Ag0.7Cu/AlN system10.1016/j.matdes.2016.11.041 ↗
34. Joining of Ti-coated monolithic SiC using a SiCw/Ti3SiC2 filler by electric field-assisted sintering10.1016/j.jeurceramsoc.2020.10.059 ↗
35. SiC ceramics joined with an in-situ reaction gradient layer of TiC/Ti3SiC2 and interface stress distribution simulations10.1016/j.ceramint.2018.05.255 ↗
36. Study on the wetting interface of Zr-Cu alloys on the SiC ceramic surface10.1039/C9RA10723A ↗
37. Effects of surface microstructure on the active element content and wetting behavior of brazing filler metal during brazing Ti3SiC2 ceramic and Cu10.1016/j.vacuum.2018.07.043 ↗
38. Residual thermal stress of SiC/Ti3SiC2/SiC joints calculation and relaxed by post-annealing10.1111/ijac.12900 ↗
39. Joining of ceramics demonstrated by the example of SiC/Ti10.1016/0955-2219(90)90012-5 ↗
40. Joining of SiC using CoFeCrNiCuTi high entropy alloy filler by electric current field assisted sintering10.1016/j.jeurceramsoc.2021.12.063 ↗
41. Vacuum brazing of alumina to stainless steel using femtosecond laser patterned periodic surface structure10.1016/j.msea.2016.03.068 ↗
42. Survey on wetting of SiC by molten metals10.1016/j.ceramint.2010.01.001 ↗
43. Microstructure and mechanical properties of the joint between Cf/SiC composite and Invar alloy brazed with AgCuInTi filler
44. Classification of bulk metallic glasses by atomic size difference, heat of mixing and period of constituent elements and its application to characterization of the main alloying element10.2320/matertrans.46.2817 ↗
45. (Fe,Cr)7C3/Fe surface gradient composite: microstructure, microhardness, and wear resistance10.1016/j.matchemphys.2014.06.026 ↗
46. Microstructure and dry-sliding wear resistance of PTA clad (Cr, Fe)7C3/γ-Fe ceramal composite coating10.1016/j.apsusc.2005.09.008 ↗
47. Study of the complex Fe-Si phase in the Al-Si-Fe-Cu-Mg-Ni alloy
48. Graphene nanoplatelets reinforced AgCuTi composite filler for brazing SiC ceramic10.1016/j.jeurceramsoc.2018.11.046 ↗