The evolution of precipitates and mechanical properties in rapidly solidified 2195 Al–Cu–Li alloy during thermal exposure
Source abstract
Abstract
The thermal stability of Al–Cu–Li alloy is critical to the quality and reliability of aerospace structural components. In this work, the microstructure and properties of rapidly solidified Al–Cu–Li alloy (T84) thermally exposed at 150 °C, 175 °C, 200 °C and 225 °C for 500 h were systematically studied. The results show that the T84 alloy exhibits excellent thermal stability with increased strength after thermally exposed at 150 °C, which is attributed to the increased number density of the T1 phase -Al2CuLi. With the further increase of thermal exposure temperature, the size of the T1 phase increases, the number density decreases significantly, and coarse precipitates such as T2 phase-Al6CuLi3 are formed. Meanwhile, the grain boundary precipitates coarsen and the precipitation free zones widen. The strengthening mechanism of the T1 phase transforms from shear mechanism to by-passing mechanism, and its contribution to yield strength decreases dramatically. In addition, the calculated activation energy indicates that coarsening of the T1 phase is controlled by the diffusion of Cu atoms.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (55)
Show source-provided references
1. Strengthening mechanisms, deformation behavior, and anisotropic mechanical properties of Al-Li alloys: a review10.1016/j.jare.2017.12.004 ↗
2. Aluminum lithium alloys (Al-Li-Cu-X)-New generation material for aerospace applications10.4028/www.scientific.net/AMM.440.104 ↗
3. The effect of thermal exposure on the electrical conductivity and static mechanical behavior of several age hardenable aluminum alloys10.1016/j.engfailanal.2006.12.008 ↗
4. The effects of prolonged thermal exposure on the mechanical properties and fracture toughness of C458 aluminum–lithium alloy10.1016/j.engfailanal.2004.10.008 ↗
5. Materials selection in design of structures and engines of supersonic aircrafts: a review10.1016/j.matdes.2012.10.001 ↗
6. Embrittlement of Al–Li–Cu–Mg alloys at slightly elevated temperatures: microstructural mechanisms of hardening10.1016/S0921-5093(00)00912-6 ↗
7. Influence of Mg and Li content on the microstructure evolution of AlCuLi alloys during long-term ageing10.1016/j.actamat.2016.09.036 ↗
8. Microstructural stability during low temperature exposure of alloys within the Al–Li–Cu–Mg system10.1016/j.msea.2007.10.020 ↗
9. Microstructural stability of binary Al Li alloys at low temperatures10.1016/S1359-6454(96)00294-7 ↗
10. Effects of Mg and Sc additions on the microstructure, mechanical properties, and thermal stability of a cast Al-2Li-2Cu-0.2Zr alloy after thermal exposure10.1016/j.jallcom.2019.02.062 ↗
11. The influence of precipitation on plastic deformation of Al–Cu–Li alloys10.1016/j.actamat.2013.03.015 ↗
12. The influence of Cu/Li ratio on precipitation in Al–Cu–Li–x alloys10.1016/j.actamat.2012.12.041 ↗
13. Microstructural evolution during aging of an AlCuLiAgMgZr alloy10.1016/1359-6454(95)00319-3 ↗
14. Enhanced strength and ductility in an Al–Cu–Li alloy via long-term ageing10.1016/j.msea.2021.141092 ↗
15. Influence of thermal exposure on the microstructure evolution and mechanical behaviors of an Al-Cu-Li alloy10.1016/j.matdes.2023.111767 ↗
16. Thermal stability of the lightweight 2099 Al-Cu-Li alloy: tensile tests and microstructural investigations after overaging10.1016/j.matdes.2017.01.058 ↗
17. Effects of overaging on microstructure and tensile properties of the 2055 Al-Cu-Li-Ag alloy10.1016/j.msea.2017.09.051 ↗
18. Microstructural evolution and mechanical properties of 2195 Al-Li alloy processed by rapid solidification and thermo-mechanical processing10.1016/j.jallcom.2023.169794 ↗
19. Improved strength and ductility of rapidly solidified 2195 alloy by pre-rolling combined with double aging and interrupted aging10.1016/j.msea.2023.145023 ↗
20. The transition from discontinuous to continuous recrystallization in some aluminium alloys: II – annealing behaviour10.1016/j.actamat.2004.03.031 ↗
21. Effects of heat treatment on the microstructure and mechanical properties of AA2618 DC cast alloy10.1016/j.matdes.2014.04.045 ↗
22. The nanoscale strain assignment behavior of icosahedral quasicrystalline phase T2-Al6CuLi3 in cast Al-Li alloys10.1016/j.jallcom.2021.159096 ↗
23. Study of icosahedral quasi-crystalline phase T2-Al6CuLi3 and transformation in 2A97 Al-Li alloy fabricated by laser additive manufacturing10.1016/j.matlet.2022.132014 ↗
24. Modeling the strengthening response to aging process of heat-treatable aluminum alloys containing plate/disc- or rod/needle-shaped precipitates10.1016/S0921-5093(02)00398-2 ↗
25. Effect of creep ageing on the corrosion behaviour of an Al–Cu–Li alloy10.1016/j.corsci.2022.110314 ↗
26. Quantitative description of the T-1 formation kinetics in an Al-Cu-Li alloy using differential scanning calorimetry, small-angle X-ray scattering and transmission electron microscopy10.1080/14786435.2013.878047 ↗
27. First-principles insights into complex interplays among nano-phases in an Al-Cu-Li-Zr alloy10.1016/j.actamat.2022.118304 ↗
28. The kinetics of precipitation from supersaturated solid solutions10.1016/0022-3697(61)90054-3 ↗
29. Theorie der Alterung von Niederschlägen durch Umlösen (Ostwald-Reifung)[J]. Zeitschrift für Elektrochemie
30. The coarsening behaviour of θ″ and θ′ precipitates in two Al-Cu alloys10.1016/0001-6160(71)90076-9 ↗
31. Bénière · 2001 · 2159
32. Theoretical and experimental study of precipitation and coarsening kinetics of θ′ phase in Al–Cu alloy10.1016/j.vacuum.2021.110263 ↗
33. The volume free energy change associated with precipitate nucleation10.1016/0036-9748(70)90172-9 ↗
34. Influence of predeformation and agEing of an Al–Zn–Mg alloy—II. Modeling of precipitation kinetics and yield stress10.1016/S1359-6454(98)00296-1 ↗
35. Impurity diffusion activation energies in Al from first principles10.1103/PhysRevB.79.054304 ↗
36. Diffusion coefficients of some solutes in fcc and liquid Al: critical evaluation and correlation10.1016/S0921-5093(03)00624-5 ↗
37. Impurity diffusion in aluminum10.1103/PhysRevB.1.3264 ↗
38. Aging behavior and precipitate characterization of a high Zn-containing Al-Zn-Mg-Cu alloy with various tempers10.1016/j.matdes.2016.03.150 ↗
39. Precipitation kinetics in metallic alloys: experiments and modeling10.1016/j.actamat.2021.117338 ↗
40. Diffusion-controlled lengthening of Widmanstätten plates10.1016/S1359-6454(03)00008-9 ↗
41. Atom probe tomography and transmission electron microscopy characterisation of precipitation in an Al–Cu–Li–Mg–Ag alloy10.1016/j.ultramic.2010.12.004 ↗
42. Microstructural evolution during ageing of Al–Cu–Li–x alloys10.1016/j.actamat.2013.12.001 ↗
43. Grain boundary precipitate free zones in Al-Li alloys10.1016/0001-6160(87)90253-7 ↗
44. Grain boundary segregation and precipitation in aluminium alloys10.1016/S1359-6462(00)00577-7 ↗
45. Improving the strength and ductility of Al–Mg–Si–Cu alloys by a novel thermo-mechanical treatment10.1016/j.msea.2014.04.009 ↗
46. Regulation of precipitation behavior among T1, S', and θ' phases in Al–Cu–Li-(Mg–Ag) alloys by optimizing Ag/Mg ratios10.1016/j.msea.2023.145158 ↗
47. Quantification and modelling of the microstructure/strength relationship by tailoring the morphological parameters of the T1 phase in an Al–Cu–Li alloy10.1016/j.actamat.2014.04.046 ↗
48. Quantitative analysis of the influences of pre-treatments on the microstructure evolution and mechanical properties during artificial ageing of an Al–Cu–Li–Mg–Ag alloy10.1016/j.msea.2020.139253 ↗
49. The effect of shear-resistant, plate-shaped precipitates on the work hardening of Al alloys: towards a prediction of the strength–elongation correlation10.1016/j.actamat.2009.08.034 ↗
50. Strengthening mechanisms of T1 precipitates and their influence on the plasticity of an Al–Cu–Li alloy10.1016/j.msea.2014.03.024 ↗
51. Quantitative effects of pre-deformation prior to non-isothermal aging on the mechanical properties-microstructure relationships in an Al-3.51Cu-1.01Li alloy10.1016/j.matdes.2022.111137 ↗
52. Strengthening effect of unshearable particles of finite size: a computer experimental study10.1016/S1359-6454(99)00179-2 ↗
53. Impact of thermal exposure on the microstructure and mechanical properties of a twin-roll cast Al-Mn-Fe-Si strip10.1016/j.jmst.2021.07.022 ↗
54. Grain boundary ductile fracture in precipitation hardened aluminum alloys10.1016/0001-6160(87)90001-0 ↗
55. Effects of heat treatment and pre-stretching on the mechanical properties and microstructure evolution of extruded 2050 Al–Cu–Li alloy10.1016/j.msea.2022.143236 ↗