Microstructure, mechanical properties, and corrosion resistance of continuous heating aging 6013 aluminum alloy
Source abstract
Abstract
In this study, the effects of continuous heating aging on the microstructure, mechanical properties, and corrosion resistance of a 6013 aluminum alloy were investigated through tensile, intergranular corrosion, and electrochemical tests. The lattice characterization of precipitates and the grain boundaries were analyzed via TEM and HRTEM. The test results indicated that with increasing final aging temperature at a constant heating rate, the alloy strength increased and the intergranular corrosion depth of the alloy decreased. Precipitates formed at the beginning of the aging period were labeled GP I, and the intracrystalline precipitates formed at the peak aging period were labeled GP II. In the over aging period, the precipitates coarsened and their quantity deteriorated; further, the Q′ phase appeared during the over aging period. The size and span of the grain boundary precipitates increased with increasing final aging temperature, and the PFZ width decreased with increasing heating rate. After continuous heating aging from 120 °C to 220 °C at a heating rate of 60 °C/h, the intergranular corrosion depth of the alloy was only 94.2 μm, whereas it was 152.1 μm after the T6 process. Thus, it was determined that the sensitivity of the intergranular corrosion of alloys depends on the grain boundary structure.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Aluminium alloys for aerospace applications10.1007/978-981-10-2134-3_2 ↗
2. Characterisation and modelling of toughness in 6013-T6 aerospace aluminium alloy friction stir welds10.1016/j.msea.2008.01.044 ↗
3. Advanced characterization of microstructural changes during recrystallization in aluminum alloy 6013
4. A microstructural study of flash welded and aged 6061 and 6013 aluminum alloys10.1016/j.matchar.2006.01.002 ↗
5. Cao · 2020
6. On the intergranular corrosion and hardness evolution of 6xxx series Al alloys as a function of Si: Mg ratio, Cu content, and aging condition10.5006/2506 ↗
7. Evaluating the intergranular corrosion susceptibility of Al-Mg-Si-Cu alloys using electrochemical methods10.1002/maco.201608979 ↗
8. A high-strain-rate superplasticity of the Al-Mg-Si-Zr-Sc alloy with Ni addition10.3390/ma14082028 ↗
9. Transformation behavior of precipitates during artificial aging at 170° C in Al–Mg–Si–Cu alloys with and without Zn addition10.1007/s12598-020-01427-z ↗
10. Influence of artificial aging on mechanical properties and high stress abrasive wear behaviour of Al–Mg–Si alloy10.1007/s12540-019-00399-9 ↗
11. Effects of T6 and T78 tempers on the microstructures and properties of Al-Mg-Si-Cu alloys10.3724/SP.J.1037.2012.00509 ↗
12. The effect of low Cu additions on precipitate crystal structures in overaged Al-Mg-Si (-Cu) alloys10.1016/j.matchar.2019.110087 ↗
13. Staly · 2007
14. Non-isothermal aging: a heat treatment method that simultaneously improves the mechanical properties and corrosion resistance of ultra-high strength Al-Zn-Mg-Cu alloy10.1016/j.jallcom.2020.156286 ↗
15. Effect of aging treatment on the corrosion resistance properties of 7N01 extrusion aluminum alloy10.3390/ma14133615 ↗
16. Tian · 2020
17. Xiang · 2019
18. Effects of non-isothermal aging on mechanical properties, corrosion behavior and microstructures of Al-Cu-Mg-Si alloy10.1016/j.jallcom.2019.152960 ↗
19. Effects of non-isothermal aging process on mechanical properties and corrosion resistance of Al–Mg–Si aluminum alloy10.1002/maco.201709756 ↗
20. Initial precipitation and hardening mechanism during non-isothermal aging in an Al–Mg–Si–Cu 6005A alloy10.1016/j.matchar.2014.05.007 ↗
21. The structural and compositional evolution of precipitates in Al-Mg-Si-Cu alloy10.1016/j.actamat.2017.12.036 ↗
22. Precipitation strengthening mechanisms during natural ageing and subsequent artificial aging in an Al-Mg-Si-Cu alloy10.1016/j.msea.2018.03.006 ↗
23. Morphology of Si phase in Al-Mg-Si-Cu alloys with excess Si addition
24. Identification of precipitates in 6013 aluminum alloy (Al–Mg–Si–Cu)
25. Electrochemical aspects of exfoliation corrosion of aluminium alloys: the effects of heat treatment10.1016/j.corsci.2011.01.010 ↗
26. PART 2-alloy development and phase transformations-HRTEM observation of GP zones and metastable phase in Al-Mg-Si alloys
27. Effect of Cu content on precipitation and age-hardening behavior in Al-Mg-Si-xCu alloys10.1016/j.jallcom.2016.10.221 ↗
28. Effect of natural ageing and pre-straining on the hardening behaviour and microstructural response during artificial ageing of an Al–Mg–Si–Cu alloy10.1016/j.matdes.2016.01.119 ↗
29. Analysis of the metastable precipitates in peak-hardness aged Al-Mg-Si (-Cu) alloys with differing Si contents10.1016/j.actamat.2017.04.037 ↗
30. Influence of quenching temperature on peak aging time and hardness of Al-Mg-Si-Cu alloys strengthened by nano-sized precipitates10.1016/j.msea.2018.11.149 ↗
31. Microstructure and strengthening mechanisms in an Al-Mg-Si alloy processed by equal channel angular pressing (ECAP)10.1007/s00170-017-1310-1 ↗
32. Strengthening mechanisms in ultrafine grained Al-Mg-Si alloy processed by hydrostatic extrusion–Influence of ageing temperature10.1016/j.msea.2016.05.109 ↗
33. Molecular dynamics simulations and experimental investigations of atomic diffusion behavior at bonding interface in an explosively welded Al/Mg alloy composite plate10.1007/s40195-017-0628-x ↗
34. Evolution of the initial precipitation and strengthening mechanism of Al-Mg-Si alloys10.1007/s11837-019-03856-3 ↗
35. Grain boundary structures and their correlation with intergranular corrosion in an extruded Al-Mg-Si-Cu alloy10.1016/j.matchar.2020.110695 ↗
36. Effect of solution temperature on the corrosion behavior of 6061-T6 aluminum alloy in NaCl solution10.1007/s11665-020-04932-5 ↗
37. Mechanical properties and corrosion behavior of artificially aged Al-Mg-Si alloy10.1016/j.jmrt.2019.11.040 ↗