Study on Cu6Sn5 morphology and grain orientation transition at the interface of (111) nt-Cu and liquid Sn
Source abstract
Abstract
Nanotwinned copper (nt-Cu) is considered to be very desirable choice for a pad material in system-in-package (SiP) devices due to its excellent anti-electromigration and anti-element migration properties. However, complex diffusion reactions exist between nt-Cu and Sn-based solder. Especially, morphology and grain orientation transition of intermetallic compounds (IMCs) appeared after multiple reflow processes. There is a lack of deep understanding of the mechanisms of the above processes. In this paper, nt-Cu was obtained by direct-current electroplating as a pad material with (111) preferred orientation, and a two-step soldering process including dip-soldering and reflow was designed to investigate the influence of temperature on IMCs morphology. The thermodynamic and molecular dynamic simulations were used to analyze the evolution mechanism of the above process. During dip-soldering process, the size of the atomic clusters was influenced by temperature, resulting in the formation of scalloped and roof-like Cu6Sn5 grains at the solidification stage. The roof-like Cu6Sn5 solder joints had a 10.7% higher shear strength and a 15% slower growth rate compared with the scalloped Cu6Sn5 solder joints. Furthermore, roof-like Cu6Sn5 had a (-12-10) preferred orientation. However, the orientation of Cu6Sn5 grains transitioned to (0001) during reflow process. Molecular dynamics simulations showed that (0001)-oriented Cu6Sn5 grains had the lowest surface energy. The decrease in surface energy was the driving force for the grain orientation transition. This work shows that the influence of temperature on interfacial IMCs could be used to form nt-Cu/Sn/nt-Cu micro-solder joints with controlled Cu6Sn5 morphology and orientation, which can significantly enhance their shear strength and reliability.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Aluminum Alloys Composites Properties · 3D IC and TSV technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (58)
Show source-provided references
1. Interconnect-based design methodologies for three-dimensional integrated circuits10.1109/JPROC.2008.2007473 ↗
2. TXV Technology: the cornerstone of 3D system-in-packaging10.1007/s11431-022-2119-3 ↗
3. Recent advances and new trends in flip chip technology10.1115/1.4034037 ↗
4. A review of SiC power module packaging technologies: challenges, advances, and emerging issues10.1109/JESTPE.2019.2951801 ↗
5. Advances in the fabrication processes and applications of wafer level packaging10.1115/1.4027397 ↗
6. Eliminate Kirkendall voids in solder reactions on nanotwinned copper10.1016/j.scriptamat.2012.10.024 ↗
7. Anomalous growth of interfacial intermetallic compounds on (111)-oriented nanotwinned Cu substrate
8. The self-healing of Kirkendall voids on the interface between Sn and (111) oriented nanotwinned Cu under thermal aging10.1016/j.apsusc.2022.152900 ↗
9. Formation of nearly void-free Cu3Sn intermetallic joints using nanotwinned Cu metallization10.1063/1.4874608 ↗
10. Microstructure and formation mechanisms of nanotwins in the shear band in a FeCoNiCrMo0.2 high-entropy alloy10.1016/j.jmrt.2022.08.054 ↗
11. Defect substructure energy landscape in polycrystalline Al under large deformation: insights from molecular dynamics10.1016/j.jmrt.2022.12.131 ↗
12. Ultrahigh strength and high electrical conductivity in copper10.1126/science.1092905 ↗
13. Extra strengthening and work hardening in gradient nanotwinned metals10.1126/science.aau1925 ↗
14. Nucleation of dislocations and twins in fcc nanocrystals: dynamics of structural transformations10.1016/j.jmst.2018.09.025 ↗
15. Microstructure and hardness of electrodeposited copper microcylinders in through-silicon via by direct current power10.1049/mnl.2015.0519 ↗
16. Nano-scale twinned Cu with ultrahigh strength prepared by direct current electrodeposition10.1016/j.msea.2019.04.107 ↗
17. Electrodeposition of nanotwin Cu by pulse current for through-Si-via (TSV) process10.1166/jnn.2016.12244 ↗
18. Grain growth in electroplated (111)-oriented nanotwinned Cu10.1016/j.scriptamat.2014.06.008 ↗
19. Unidirectional growth of microbumps on (111)-oriented and nanotwinned copper10.1126/science.1216511 ↗
20. Observation of atomic diffusion at twin-modified grain boundaries in copper10.1126/science.1160777 ↗
21. Growth characteristics and formation mechanisms of Cu6Sn5 phase at the liquid-Sn0.7Cu/(111)(Cu) and liquid-Sn0.7Cu/(001)(Cu) joint interfaces10.1016/j.actamat.2015.11.034 ↗
22. Three-dimensional placement rules of Cu6Sn5 textures formed on the (111)(Cu) and (001)(Cu) surfaces using electron backscattered diffraction10.1016/j.matdes.2016.01.037 ↗
23. Morphologies, orientation relationships and evolution of Cu6Sn5 grains formed between molten Sn and Cu single crystals10.1016/j.actamat.2008.01.055 ↗
24. Dramatic morphological change of scallop-type Cu6Sn5 formed on (001) single crystal copper in reaction between molten SnPb solder and Cu10.1063/1.2761840 ↗
25. Relationship between morphologies and orientations of Cu6Sn5 grains in Sn3.0Ag0.5Cu solder joints on different Cu pads10.1016/j.matchar.2013.12.006 ↗
26. Epitaxial Cu-Sn bulk crystals grown by electric current10.1016/j.actamat.2013.06.014 ↗
27. Morphology and orientation evolution of Cu6Sn5 grains on (001)Cu and (011)Cu single crystal substrates under temperature gradient10.1016/j.jmst.2021.03.065 ↗
28. Continuous epitaxial growth of extremely strong Cu6Sn5 textures at liquid-Sn/(111)Cu interface under temperature gradient10.1063/1.5010266 ↗
29. Dramatic morphological reservation of prism-type Cu6Sn5 formed on single crystal Cu substrates under temperature gradient
30. Microstructure control of unidirectional growth of eta-Cu6Sn5 in microbumps on <111> oriented and nanotwinned Cu10.1016/j.actamat.2013.04.056 ↗
31. Growth mechanism of interfacial IMCs on (111) preferred orientation nanotwinned Cu UBM for 3D IC packaging10.1109/ECTC32862.2020.00294 ↗
32. Growth mechanisms of Cu3Sn on polycrystalline and single crystalline Cu substrates10.1016/j.actamat.2009.06.025 ↗
33. A tool for manipulating and converting atomic data files10.1016/j.cpc.2015.07.012 ↗
34. Phase stability and thermal expansion behavior of Cu6Sn5 intermetallics doped with Zn, Au and in10.1016/j.intermet.2013.07.012 ↗
35. Cu3Sn - understanding the systematic absences10.1107/S205252061401806X ↗
36. LAMMPS-a flexible simulation tool for particle-based materials modeling at the atomic, meso, and continuum scales
37. Strain- and strain-rate-dependent mechanical properties and behaviors of Cu3Sn compound using molecular dynamics simulation10.1007/s10853-011-6144-x ↗
38. Morphology and dynamics of 2D Sn-Cu alloys on (100) and (111) Cu surfaces10.1088/0965-0393/8/3/313 ↗
39. Analysis of Cu6Sn5 grain orientations in Sn3.0Ag0.5Cu lead-free solder joints
40. Impact of different isothermal aging conditions on the IMC layer growth and shear strength of MWCNT-reinforced Sn-5Sb solder composites on Cu substrate10.1016/j.jallcom.2019.151714 ↗
41. Microstructural and shear strength properties of GNSs-reinforced Sn-1.0Ag-0.5Cu (SAC105) composite solder interconnects on plain Cu and ENIAg surface finish10.1016/j.jmrt.2021.09.067 ↗
42. Isothermal aging effects on the microstructure and solder bump shear strength of eutectic Sn37Pb and Sn3.5Ag solders10.1016/j.microrel.2005.06.006 ↗
43. The effect of reflow time on reactive wetting, evolution of interfacial IMCs and shear strength of eutectic Sn-Cu solder alloy10.1007/s10854-014-1749-x ↗
44. Interfacial reaction and mechanical reliability of eutectic Sn-0.7Cu/immersion Ag-plated Cu solder joint10.1179/174328408X374739 ↗
45. Role of Cu in dissolution kinetics of Cu metallization in molten Sn-based solders10.1063/1.1925317 ↗
46. Niu · 2011 · 22
47. Atomic-Scale investigation of electromigration with different directions of electron flow into high-density nanotwinned copper through in situ HRTEM10.1016/j.actamat.2021.117250 ↗
48. Stefanescu · 2015
49. Origins of structural and electronic transitions in disordered silicon10.1038/s41586-020-03072-z ↗
50. Comparison of transformations with inhomogeneous nucleation and transformations with inhomogeneous growth velocity10.1016/j.jmrt.2019.08.012 ↗
51. Computer simulation of site saturation and constant nucleation rate transformations on a network of Kelvin polyhedra10.1016/j.jmrt.2019.07.066 ↗
52. Early stages of intermetallic compound formation and growth during lead-free soldering10.1016/j.actamat.2010.05.028 ↗
53. Phase field simulations of morphological evolution and growth kinetics of solder reaction products10.1007/s11664-006-0184-z ↗
54. Evolution of CuSn intermetallics between molten SnAgCu solder and Cu substrate10.1016/j.actamat.2008.04.063 ↗
55. Effects of the melt state on the microstructure of a Sn-3.5% Ag solder at different cooling rates10.1016/j.apsusc.2012.02.058 ↗
56. Effect of cooling rate on growth of the intermetallic compound and fracture mode of near-eutectic Sn-Ag-Cu/Cu pad: before and after aging10.1007/s11664-004-0095-9 ↗
57. IMC microstructure modification and mechanical reinforcement of Sn-Ag-Cu/Cu microelectronic joints through an advanced surface finish technique10.1016/j.jmrt.2021.02.029 ↗
58. Kinetic analysis of the soldering reaction between eutectic SnPb alloy and Cu accompanied by ripening10.1103/PhysRevB.53.16027 ↗