Role of the internal oxidation layer in the liquid metal embrittlement during the resistance spot welding of the Zn-coated advanced high strength steel
Source abstract
Abstract
Advanced high strength steel (AHSS) with the Zn coating can produce high susceptibility of liquid metal embrittlement (LME) particularly when the resistance spot welding (RSW) is involved. The internal oxidation layer formed in the subsurface of AHSS is believed to be one of the most important factors to control the Zn-assisted LME susceptibility. The role of the internal oxidation layer in the formation of the LME for the resistance spot welded joint of the Zn-coated AHSS was comprehensively investigated in the present study. The results showed that increasing the dew point of the annealing atmosphere from −40 to −10 °C can successfully produce the internal oxidation layer in the subsurface of the steel. The Zn-coated AHSS without the internal oxidation layer revealed higher LME susceptibility during the RSW compared with the one with internal oxidation layer. In particular, the elements Si and O exhibit a synchronous segregation tendency, forming an internal oxidation layer in the subsurface of the steel. The internal oxidation layer together with the internal oxides distributed at the grain boundaries can decrease the penetration motivation of the liquid Zn, reducing the LME susceptibility.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced Welding Techniques Analysis · Welding Techniques and Residual Stresses · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (54)
Show source-provided references
1. Thermo-kinetic design of retained austenite in advanced high strength steels10.1016/j.actamat.2018.04.040 ↗
2. Medium Mn transformation-induced plasticity steels: recent progress and challenges10.1016/j.scriptamat.2016.07.013 ↗
3. Microstructural characterization of a 1100 MPa complex-phase steel10.1016/j.jmrt.2021.12.106 ↗
4. Microstructure-mechanical properties relationships for quenching and partitioning (Q&P) processed steel10.1016/j.actamat.2016.04.048 ↗
5. Design of tough, ductile direct quenched and partitioned advanced high-strength steel with tailored silicon content10.1016/j.jmrt.2022.01.073 ↗
6. High temperature deformation behaviors of hot dip 55 wt% Al-Zn coated steel10.1016/j.apsusc.2020.145550 ↗
7. Role of aluminum on liquid metal embrittlement susceptibility for Zn-Al-Mg/Sn coated hot-formed steels10.1016/j.jmrt.2022.05.092 ↗
8. The effect of silicon content on liquid-metal-embrittlement susceptibility in resistance spot welding of galvanized dual-phase steel10.1016/j.jmapro.2020.07.008 ↗
9. Si effect on Zn-assisted liquid metal embrittlement in Zn-coated TWIP steels: importance of Fe-Zn alloying reaction10.1016/j.surfcoat.2020.125809 ↗
10. Role of Si content in the element segregation of galvanized QP980 advanced high strength steel10.1007/s11837-022-05284-2 ↗
11. Role of liquid Zn and α-Fe(Zn) on liquid metal embrittlement of medium Mn steel: an ex-situ microstructural analysis of galvannealed coating during high temperature tensile test10.1016/j.surfcoat.2020.126069 ↗
12. Embrittlement of heat treated steels when tempered at 250 to 400 °C
13. Atomic-scale investigation of liquid-metal-embrittlement crack-path: revealing mechanism and role of grain boundary chemistry10.1016/j.actamat.2020.116519 ↗
14. Zn penetration in liquid metal embrittled TWIP steel10.1007/s11661-016-3475-x ↗
15. Towards an explanation of liquid metal embrittlement cracking in resistance spot welding of dissimilar steels10.1016/j.matdes.2020.109055 ↗
16. Impact of liquid metal embrittlement cracks on resistance spot weld static strength10.1080/13621718.2018.1518363 ↗
17. Kinetic, volumetric and structural effects induced by liquid Ga penetration into ultrafine grained Al10.1016/j.actamat.2015.07.061 ↗
18. Pathway to understand liquid metal embrittlement (LME) in Fe-Zn couple: from fundamentals toward application10.1016/j.pmatsci.2021.100798 ↗
19. Identification of a bilayer grain boundary complexion in Bi-doped Cu10.1016/j.scriptamat.2012.10.012 ↗
20. Zn-induced liquid metal embrittlement and mechanical properties of advanced high-strength steel with resistance spot weld10.1016/j.msea.2022.143088 ↗
21. Effect of type-B liquid metal embrittlement cracks on high-cycle fatigue properties of spot-welded 1180 TRIP steel10.1080/13621718.2021.1872289 ↗
22. Effect of type-C liquid metal embrittlement on mechanical properties of spot-welded TRIP steel10.1016/j.jmrt.2021.06.041 ↗
23. Investigation on shearing strength of resistance spot-welded joints of dissimilar steel plates with varying welding current and time10.1016/j.jmrt.2021.12.079 ↗
24. Early stages of liquid-metal embrittlement in an advanced high-strength steel
25. Role of spot weld electrode geometry on liquid metal embrittlement crack development10.1016/j.jmapro.2019.11.015 ↗
26. Effect of multiple pulse resistance spot welding schedules on liquid metal embrittlement severity10.1115/1.4044099 ↗
27. Evaluation of surface crack in resistance spot welds of Zn-coated steel10.2320/matertrans.M2013244 ↗
28. Reduction in liquid metal embrittlement cracking using weld current ramping10.1007/s40194-019-00790-5 ↗
29. Supercritical area and critical nugget diameter for liquid metal embrittlement of Zn-coated twining induced plasticity steels10.1016/j.scriptamat.2015.07.006 ↗
30. Surface breaking cracks in resistance spot welds of dual phase steels with electrogalvanised and hot dip zinc coating10.1179/1362171812Y.0000000068 ↗
31. Effect of deformation on the electrochemical behavior of hot-dip galvanized steel sheets10.1016/j.apsusc.2007.04.045 ↗
32. Corrosion behavior and failure mechanism of electromagnetic pulse welded joints between galvanized steel and aluminum alloy sheets10.1016/j.jmapro.2021.02.039 ↗
33. A review on recent approaches in the field of hot dip zinc galvanizing process10.1016/j.surfcoat.2014.12.054 ↗
34. Thermodynamic consideration on selective surface oxidation of high strength steels prior to hot-dip galvanizing10.1007/s11998-011-9334-1 ↗
35. Changing oxide layer structures with respect to the dew point prior to hot-dip galvanizing of δ-TRIP steel10.1016/j.surfcoat.2017.12.046 ↗
36. Wettability of MnxSiyOz by liquid Zn-Al alloys10.1007/s11663-010-9366-4 ↗
37. Impact of selective oxidation during inline annealing prior to hot-dip galvanizing on Zn wetting and hydrogen-induced delayed cracking of austenitic FeMnC steel10.1016/j.surfcoat.2011.07.081 ↗
38. Investigation into the surface selective oxidation of dual-phase steels by XPS, SAM and SIMS10.1002/sia.1639 ↗
39. Effect of annealing atmosphere on the galvanizing behavior of a dual-phase steel10.1016/j.msea.2006.09.116 ↗
40. On the reactive wetting of a medium-Mn advanced high-strength steel during continuous galvanizing10.1016/j.surfcoat.2018.10.028 ↗
41. The role of internal oxides on the liquid metal embrittlement cracking during resistance spot welding of the dual phase steel10.1007/s11661-020-05702-7 ↗
42. Embrittlement of a zinc coated high manganese TWIP steel10.1016/j.msea.2012.02.049 ↗
43. Liquid zinc embrittlement of twinning-induced plasticity steel10.1016/j.scriptamat.2011.12.040 ↗
44. Liquid Zn assisted embrittlement of advanced high strength steels with different microstructures10.1007/s12540-016-5579-7 ↗
45. Liquid metal embrittlement susceptibility of two Zn-coated advanced high strength steels of similar strengths10.1016/j.msea.2021.141569 ↗
46. 2020
47. Galvanizability of high-strength steels for automotive applications10.1007/s11661-001-1042-5 ↗
48. Effect of hot-dip galvanizing process on selective oxidation and galvanizability of medium manganese steel for automotive application10.3390/coatings10121265 ↗
49. Characterization of surface layers of oxidation-reduction treated Si and Mn added advanced high strength steel10.1016/j.surfcoat.2019.125172 ↗
50. Effect of water pressure and soaking time on the selective oxidation of DP980 advanced high strength steel10.1016/j.apsusc.2018.05.034 ↗
51. Effect of Si/Mn ratio on galvannealing behavior of Si-added steel10.2355/isijinternational.ISIJINT-2018-063 ↗
52. Effect of internal oxidation on the weldability of CMnSi steels10.1007/s40194-019-00798-x ↗
53. Tailoring of oxide morphology and crystallinity on advanced high-strength steel surfaces prior hot-dip galvanizing10.1016/j.actamat.2014.03.037 ↗
54. Zn penetration and its coupled interaction with the grain boundary during the resistance spot welding of the QP980 steel10.1016/j.scriptamat.2022.114832 ↗