Immersion and electrochemical corrosion properties and combined corrosion mechanism of TC4 alloy by keyhole TIG welding
Source abstract
Abstract
In this study, the effect of heat input on the microstructure and its correlation with the immersion corrosion properties of TC4 welded joints by Keyhole tungsten inert gas (TIG) process was researched. The combined corrosion mechanism between immersion corrosion and electrochemical corrosion was established. The results showed that immersion corrosion formed a passivation film on the surface of the welded joint and formed a minimal number of pitting pits. After immersion, electrochemical corrosion testing was carried out. Due to the existence of the passivation film, the self-corrosion potential increased from-0.6 V ∼ −0.2 V–0.1 V–0.6 V, and the self-corrosion current density decreased and the fitting impedance of the film increased. These all showed that the corrosion resistance of the joint was enhanced after immersion. However, due to the combined effect of immersion corrosion and electrochemical corrosion, the potential difference between the surface passivation film and the internal metal was sufficiently large to induce pitting corrosion on the surface. After the breakdown of the passivation film, spot corrosion pits formed. Microcracks propagated along the primary β grain boundary and the α′ phase interface, and continuous corrosion for a long time may even lead to cracking failure of the welded joints. With the increase of heat input, the self-corrosion potential and the self-corrosion current density of immersion corrosion increased firstly and then decreased. The fitting film resistance value of the impedance decreased firstly and then increased. The aforementioned findings indicated that as the heat input increased, the corrosion properties of the joints firstly deteriorated and then improved.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Welding Techniques and Residual Stresses · Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. Electrochemical corrosion, wear and cell behavior of ZrO2/TiO2 alloyed layer on Ti-6Al-4V10.1016/j.bioelechem.2018.01.011 ↗
2. High-strength titanium alloys for aerospace engineering applications: a review on melting-forging process10.1016/j.msea.2022.143260 ↗
3. Current research and development status of dissimilar materials laser welding of titanium and its alloys :A review10.1016/j.optlastec.2020.106090 ↗
4. Surface modification methods for titanium and its alloys and their corrosion behavior in Biological environment: a review10.1007/s40735-019-0229-5 ↗
5. A review on heat treatment efficiency in metastable β titanium alloys: the role of treatment process and parameters10.1016/j.jmrt.2020.10.088 ↗
6. High-strength titanium alloys for aerospace engineering applications: a review on melting-forging process10.1016/j.msea.2022.143260 ↗
7. A comparative study of pulsed Nd: YAG laser welding and TIG welding of thin Ti6Al4V titanium alloy plate10.1016/j.msea.2012.06.016 ↗
8. Comparison of keyhole and conventional gas tungsten arc welds in commercially pure titanium10.1016/S0921-5093(00)01408-8 ↗
9. Sustaining the open keyhole in slow-falling current edge during K-TIG process: principle and parameters10.1016/j.ijheatmasstransfer.2017.04.092 ↗
10. Stabilization of weld pool through jet flow argon gas backing in C-Mn steel keyhole TIG welding10.1016/j.jmatprotec.2017.07.008 ↗
11. Impact of microstructure evolution on the corrosion behaviour of the Ti–6Al–4V alloy welded joint using high-frequency pulse wave laser10.1016/j.jmrt.2023.04.077 ↗
12. Influence of welding parameters on mechanical and corrosion properties of Ti6Al4V alloy10.1016/j.matpr.2023.06.001 ↗
13. Effect of pulsed gas tungsten arc welding on corrosion behavior of Ti–6Al–4V titanium alloy10.1016/j.matdes.2007.06.009 ↗
14. Microstructure and corrosion resistance of fusion zone in Ti-6Al-4V alloy welded using pulsed- and continuous-wave lasers10.1016/j.corsci.2023.111269 ↗
15. Microstructure and corrosion behavior of linear friction welded TA15 and TC17 dissimilar joint10.1016/j.matchar.2022.111871 ↗
16. Influence of heat treatments on corrosion behavior of Ti64 friction welds10.1016/j.cdc.2022.100940 ↗
17. Effect of microstructure evolution of Ti6Al4V alloy on its cavitation erosion and corrosion resistance in artificial seawater10.1016/j.jmst.2021.06.005 ↗
18. Pitting behavior of Ti-15-3 titanium alloy with different surface in salt spray studied using electrochemical noise10.1016/j.jmrt.2021.08.072 ↗
19. Mechanical properties and fatigue failure mechanisms of purely self-piercing riveted (SPR) and hybrid (SPR-bonded) joints under salt spray environment10.1016/j.jmrt.2022.08.024 ↗
20. A microstructural, mechanical and electrochemical/stress corrosion cracking investigation of a Cr-modified Ti–6Al–4V alloy10.1016/j.jmrt.2023.05.213 ↗
21. Characterization of corrosion behavior of TA2 titanium alloy welded joints in seawater environment
22. Reconstruction of parent microstructures in TRIP titanium alloys10.1016/j.scriptamat.2022.115248 ↗
23. Effect of cooling rate on the high strain rate properties of boron steel10.1016/j.ijimpeng.2009.05.009 ↗
24. Microstructural characterization and formation of α′ martensite phase in Ti–6Al–4V alloy butt joints produced by friction stir and gas tungsten arc welding processes10.1016/j.matdes.2012.12.024 ↗
25. Corrosion evaluation of Ti–6Al–4V manufactured by electron beam melting in Ringer's physiological solution: an in vitro study of the passive film10.1007/s10800-022-01683-0 ↗
26. Formation and control of martensite in Ti-6Al-4V alloy produced by selective laser melting10.1016/j.matdes.2016.06.117 ↗
27. A review on heat treatment efficiency in metastable β titanium alloys: the role of treatment process and parameters10.1016/j.jmrt.2020.10.088 ↗
28. Germain · Acta Mater · 2012 · 60 · 455110.1016/j.actamat.2012.04.034 ↗
29. David Pérez-Ruiz · Mech Syst Signal Process · 2022 · 168
30. Effects of heat input on microstructure evolution, mechanical and corrosion properties of TC4 alloy by keyhole TIG welding10.1016/j.jmrt.2023.11.047 ↗
31. Electrochemical corrosion behavior of TA2 titanium alloy welded joint in Cl- containing solutions10.20964/2021.09.08 ↗
32. Effect of hydrogen charging on microstructural evolution and corrosion behavior of Ti-4Al-2V-1Mo-1Fe alloy10.1016/j.jmst.2020.06.010 ↗
33. Effect of weld heat input on corrosion of dissimilar welded pipeline steels under simulated coating disbondment protected by cathodic protection10.1016/j.jmrt.2019.12.044 ↗
34. Effects of laser welding on the microstructure evolution and corrosion resistance of a novel nitrogen-containing austenitic stainless steel QN210910.1016/j.jmrt.2023.03.012 ↗
35. Microstructure evolution and corrosion mechanism of in situ synthesized TiC/TC4 alloy nanocomposites fabricated by laser powder bed fusion10.1016/j.ceramint.2022.09.257 ↗
36. Effect of microstructural heterogeneity on corrosion fatigue crack growth behavior of 60-mm thick-plate TC4 titanium alloy NG-GTAW welded joint10.1016/j.ijfatigue.2022.107030 ↗
37. The influence of niobium and vanadium on passivity of titanium-based implants in physiological solution10.1016/S0142-9612(03)00252-7 ↗
38. Diffusion impedance of electroactive materials, electrolytic solutions and porous electrodes: Warburg impedance and beyond10.1016/j.electacta.2018.05.136 ↗
39. Repassivation of titanium and surface oxide film regenerated in simulated bioliquid10.1002/(SICI)1097-4636(19980615)40:4<530::AID-JBM3>3.0.CO;2-G ↗
40. Corrosion characterization of titanium alloys by electrochemical techniques10.1016/j.electacta.2005.02.121 ↗