Tensile behavior of the designed SiCf/Ti2AlNb/Ti17 composites
Source abstract
Abstract
SiCf/Ti2AlNb-reinforced Ti17 (SiCf/Ti2AlNb/Ti17) composites were fabricated through hot isostatic pressing. The designed SiCf/Ti2AlNb/Ti17 composites exhibited excellent tensile properties, with tensile strengths of 1657 MPa at room temperature and 1830 MPa at 450 °C. The microstructure, fracture morphology, and longitudinal section of the composites were characterized by X-ray diffraction, scanning electron microscopy, and electron backscatter diffraction techniques. The fracture process of SiCf/Ti2AlNb/Ti17 composites during room-temperature tensile tests was as follows: the SiCf/Ti2AlNb reaction layer first fractured, the crack extended into the Ti2AlNb matrix, the Ti2AlNb matrix crack extended to the adjacent reaction layer and promoted fiber fracture, the crack extended to the Ti2AlNb/Ti17 interface, ultimately the Ti17 capsule fractured. The fracture process of SiCf/Ti2AlNb/Ti17 composites during 450 °C tensile tests was as follows: the SiCf/Ti2AlNb reaction layer first fractured, multiple fiber fractures occurred, and the crack in the reaction layer entered the Ti2AlNb matrix, the crack extended to the Ti2AlNb/Ti17 interface, eventually the Ti17 capsule fractured. The room-temperature tensile fracture was fitted to the LLS model, while the tensile fracture at 450 °C was fitted to the GLS model. The different fracture processes indicated that the SiCf/Ti2AlNb/Ti17 composites were suitable for exploiting fiber strength at 450 °C and therefore exhibited excellent tensile strength.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. High cycle and very high cycle fatigue of TC17 titanium alloy: stress ratio effect and fatigue strength modeling10.1016/j.ijfatigue.2022.107299 ↗
2. Effect of microstructure on fracture toughness and fatigue crack growth behavior of Ti17 alloy10.3390/met6080186 ↗
3. Microstructure and interfacial strength of SiC fiber-reinforced Ti17 alloy composites with different consolidation temperatures10.1007/s12598-018-1002-5 ↗
4. Experimental investigation of laser peening on Ti17 titanium alloy for rotor blade applications10.1016/j.apsusc.2015.05.098 ↗
5. Rapid W/SiC reaction induced by laser surface remelting within SiCf/Ti17 composites10.1016/j.matlet.2022.133505 ↗
6. Study on tensile behavior of SiCf/TC17 composites
7. Multi-scale analyses of phase transformation mechanisms and hardness in linear friction welded Ti17(α + β)/Ti17(β) dissimilar titanium alloy joint
8. Interfacial reactions and matrix microstructure evolution in SiCf/Ti composites dominated by primary structure of Ti matrix10.1016/j.ceramint.2019.05.347 ↗
9. Interfacial reactions in SiCf/C/Ti17 composites dominated by texture of carbon coatings10.1016/j.carbon.2017.08.065 ↗
10. The effect of modulated matrix microstructure on the deformation behavior in SiCf/Ti17 composites10.1016/j.matlet.2019.01.122 ↗
11. Failure mechanism of continuous fiber-reinforced titanium matrix composite bling under rotational loading10.1016/j.jmrt.2022.03.006 ↗
12. Experimental and theoretical assessment of the residual stresses in SiC monofilament reinforced Ti-17 matrix composites
13. Research on hot deformation behavior of As-forged TC17 titanium alloy10.1007/s11665-021-05942-7 ↗
14. Tensile and very high cycle fatigue behaviors of a compressor blade titanium alloy at room and high temperatures10.1016/j.msea.2021.141049 ↗
15. Thermodynamic and microstructural study of Ti2AlNb oxides at 800 °C10.1038/s41598-018-31196-w ↗
16. Interfacial bonding mechanism of linear friction welded dissimilar Ti2AlNb–Ti60 joint: grain intergrowth induced by combined effects of dynamic recrystallization, phase transformation and elemental diffusion10.1016/j.jmrt.2023.04.184 ↗
17. Deformation and life analysis of composite flywheel disk systems10.1016/S1359-8368(02)00032-X ↗
18. Effect of heat treatment on the microstructure and properties of CVD SiC fiber10.1016/j.jmst.2017.02.009 ↗
19. Micromechanical modelling of deformation and failure in Ti–6Al–4V/SiC composites10.1016/S1359-6454(01)00246-4 ↗
20. Ultimate strengths of fibrereinforced ceramics and metals10.1016/0010-4361(93)90005-S ↗
21. Phase transformation and microstructure control of Ti2AlNb-based alloys: a review10.1016/j.jmst.2020.11.022 ↗
22. Temperature-dependent evolution of interfacial zones in SiCf/C/Ti17 composites10.1039/C7RA09530A ↗
23. Effect of C/Mo duplex coating on the interface and tensile strength of SiCf/Ti-21Al-29Nb composites10.1016/j.jallcom.2017.06.039 ↗
24. Effect of the interfacial reaction layer thickness on the thermal residual stresses in SiCf/Ti–6Al–4V composites10.1016/j.msea.2008.01.007 ↗
25. Effect of fiber volume fraction on longitudinal tensile properties of SiCf/Ti-6Al-4V composites10.1007/s11595-017-1592-z ↗
26. In-situ investigation on dislocation slip concentrated fracture mechanism of linear friction welded dissimilar Ti17(α+β)/Ti17(β) titanium alloy joint10.1016/j.msea.2023.144991 ↗
27. Interfacial reaction in SiCf/C/TiAl matrix composites10.1016/j.jmrt.2021.03.072 ↗
28. Development and characterization of newcoatings for improvedbalance of mechanical properties of titaniummatrix composites10.1016/S0921-5093(98)00903-4 ↗
29. Effects of manufacturing environments on the residual stresses in a SiC/Ti metal-matrix composite10.1515/secm-2015-0089 ↗
30. Role of matrix microstructure on room-temperature tensile properties and fiber-strength utilization of an orthorhombic ti-alloy-based composite10.1007/s11661-997-0134-2 ↗
31. Formation of interfacial reaction products in SCS-6 SiC/Ti2AlNb composites10.1016/j.scriptamat.2004.05.020 ↗
32. Optimization of C/TiC duplex diffusion barrier coatings for SiC/Ti composites based on interfacial structure evolution exploration10.1016/j.ceramint.2018.06.072 ↗
33. A progressive damage model for unidirectional fibre-reinforced composites based on fragmentation, Part I: formulation10.1016/j.compscitech.2005.04.012 ↗