Enhanced biocompatibility of a Ni–Cr alloy prepared by selective laser melting: a preliminary in vitro study
Source abstract
Abstract
Against a general consensus regarding the high toxicity and low biocompatibility of cast nickel–chromium (Ni–Cr) alloys, the in vitro biocompatibility of selective laser melting (SLM)-fabricated Ni–Cr alloys was investigated and compared with that of cast alloy. Using a single Ni–Cr alloy powder, two SLM alloys with high (SLM_a) and low (SML_b) porosity were prepared by adjusting the laser process parameters in addition to a cast alloy. The alloys were studied in terms of their microstructure, metal ion release, and cell response. All three alloys were composed of only the γ (face-centered cubic) phase. However, both SLM alloys showed more homogeneous dispersion of Ni, Cr, and molybdenum elements and finer grain formation than the cast alloy. Immersion test results indicated that both SLM alloys (in particular, SML_b) exhibited a significantly lower Ni ion release than the cast alloy (P < 0.001). A water-soluble tetrazolium salt-8 assay also showed that the viability of L929 mouse fibroblasts was significantly higher for both SLM groups (in particular, SML_b) than for the cast alloy group (P < 0.001). Thus, the combined results of this in vitro study suggest that the SLM-processed Ni–Cr alloys exhibited greatly enhanced biocompatibility in comparison with the cast alloy.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Dental materials and restorations · Additive Manufacturing Materials and Processes · Bone Tissue Engineering Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (18)
Show source-provided references
1. In vitro evaluation of marginal, axial, and occlusal discrepancies in metal ceramic restorations produced with new technologies10.1016/j.prosdent.2016.03.013 ↗
2. Influence of porcelain firing and cementation on the marginal adaptation of metal–ceramic restorations prepared by different methods10.1016/j.prosdent.2016.08.016 ↗
3. Metal–ceramic alloys in dentistry: a review10.1111/j.1532-849X.2008.00377.x ↗
4. Effect of microstructural evolution and elevated temperature on the mechanical properties of Ni–Cr–Mo alloys10.1016/j.jallcom.2014.09.036 ↗
5. Casting alloys10.1016/j.cden.2003.12.010 ↗
6. The effect of oxidation heat treatment of porcelain bond strength in selected base metal alloys10.1016/0022-3913(91)90502-N ↗
7. Preliminary evaluation of mechanical properties of Co–Cr alloys fabricated by three new manufacturing processes10.11607/ijp.4298 ↗
8. Base metal alloys used for dental restorations and implants10.1016/j.cden.2007.04.001 ↗
9. In vitro biocompatibility of Co–Cr alloy fabricated by selective laser melting or traditional casting techniques10.1016/j.matlet.2012.08.032 ↗
10. Microstructures and mechanical properties of Co–Cr dental alloys fabricated by three CAD/CAM-based processing techniques10.3390/ma9070596 ↗
11. Comparison of in vitro biocompatibility of a Co–Cr dental alloy produced by new milling/post-sintering or traditional casting technique10.1016/j.matlet.2016.05.053 ↗
12. Degradation and cytotoxicity of lotus-type porous pure magnesium as potential tissue engineering scaffold material10.1016/j.matlet.2010.06.015 ↗
13. Effect of chemical composition on the corrosion behavior of Ni–Cr–Mo dental casting alloys10.1002/jbm.10080 ↗
14. In vitro determination of titanium and other metals released from intra-osseous dental implants into the mucosa10.1039/C5AY01359C ↗
15. Effect of fluoride content on ion release from cast and selective laser melting-processed Co–Cr–Mo alloys10.1016/j.prosdent.2013.12.022 ↗
16. Characteristic of intermetallic phases in cast dental CoCrMo alloy
17. Selective laser melting technique of Co–Cr dental alloys: a review of structure and properties and comparative analysis with other available techniques10.1111/jopr.12268 ↗
18. Corrosion of nickel-based dental casting alloys10.1016/j.dental.2006.06.011 ↗