Abstract
This article aims to minimize the adverse impact of Z-pins on the in-plane properties of unidirectional carbon fiber reinforced polymer (CFRP) composites while enhancing their interlaminar fracture toughness by using CF Z-pins. A novel method was developed for implanting fine Z-pins of 0.1 mm diameter with semi-embedded length in the thickness center of laminate in an ultra-low distribution density of hexagonal array pattern. Mechanical properties and failure mechanisms of different Z-pinned composites were analyzed. Taking traditional CFRP as a reference, the semi-embedded Z-pinned CFRP has considerably increased (by 123%) propagation GIC and negligibly reduced in-plane mechanical properties. Correspondingly, the Z-pinned CFRP with full-thickness embedded length shows a rise of 244% in the propagation GIC and a reduction of less than 9% in the in-plane properties. The failure modes indicate that pull-outs of Z-pins and their fractures both contribute to the enhancement of the fracture toughness of Z-pinned laminates, which are influenced by the distribution density and the embedded length of pins. It manifests that shortening the embedded length of pins can narrow the scope of waviness in planar fibers and relieve the induced stress concentration, which is conducive to improving the retention ratio of in-plane mechanical properties of Z-pinned composites. Finally, with 0.10% areal density, a better balance between interlaminar and in-plane properties of Z-pinned composites is successfully achieved for those with semi-embedded pins. Moreover, the Z-pin enhancement effect on interlaminar toughness is limited by its lower areal distribution density.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Mechanical Behavior of Composites · Fiber-reinforced polymer composites · Tribology and Wear Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Preparation, development, outcomes, and application versatility of carbon fiber-based polymer composites: a review10.1007/s42114-018-0072-z ↗
2. High-force dynamic mechanical analysis of composite sandwich panels for aerospace structures
3. Application of composite materials in inductive charging systems for electric vehicles10.1177/0021998318824637 ↗
4. Interlaminar fracture properties of carbon fibre epoxy matrix composites interleaved with polyethylene terephthalate (PET) films
5. A comparative study on interlaminar properties of l-shaped Two-Dimensional (2D) and Three-Dimensional (3D) woven composites10.1007/s10443-018-9745-6 ↗
6. Enhancing the fracture toughness of laminated composites through carbon nanotube belt stitching10.1016/j.compscitech.2020.108632 ↗
7. Mechanical properties of woven laminates and felt composites using carbon fibers. Part 2: interlaminar properties10.1016/j.compscitech.2004.03.013 ↗
8. Fabrication and thermo-electro and mechanical properties evaluation of helical multiwall carbon nanotube-carbon fiber/epoxy composite laminates10.3390/polym13091437 ↗
9. Improved interfacial property of carbon fiber composites with carbon nanotube and graphene oxide as multi-scale synergetic reinforcements10.1016/j.compositesa.2019.105573 ↗
10. Pullout performance of circumferentially notched Z-pins in carbon fiber reinforced laminates10.1016/j.compositesa.2018.05.002 ↗
11. Comparative study of the mode I and mode II delamination fatigue properties of Z-pinned aircraft composites10.1016/j.matdes.2014.08.072 ↗
12. A review of methods for improving interlaminar interfaces and fracture toughness of laminated composites
13. Comparative study of metal and composite Z-pins for delamination fracture and fatigue strengthening of composites10.1016/j.engfracmech.2016.01.003 ↗
14. Manufacturing process and performance of dry carbon fabrics reinforced with rectangular and circular Z-pins10.1177/0021998313495070 ↗
15. Synergistic delamination toughening of composites using multi-scale carbon reinforcements10.1016/j.compositesb.2018.10.031 ↗
16. Influence of through-thickness reinforcement aspect ratio on mode I delamination fracture resistance10.1016/j.compstruct.2015.01.032 ↗
17. Mechanical properties of composite laminates reinforced with rectangular Z-pins in monotonic and cyclic tension10.1016/j.compositesa.2018.03.004 ↗
18. Dynamic inter-fibre failure of unidirectional composite laminates with through-thickness reinforcement10.1016/j.compscitech.2019.04.004 ↗
19. Tuning interlaminar fracture toughness of fine Z-pin reinforced polymer composite10.1016/j.matdes.2021.110293 ↗
20. Effect of Ø 0.11 mm Z-pinning on the properties of composite laminates via an ultrasound guided insertion process10.1016/j.compscitech.2021.108906 ↗
21. Properties and failure mechanisms of Z-pinned laminates in monotonic and cyclic tension10.1016/j.compositesa.2005.11.013 ↗
22. The strength of composite bonded T-joints transversely reinforced by carbon pins10.1016/j.compstruct.2011.08.026 ↗
23. Tension fatigue of fibre-dominated and matrix-dominated laminates reinforced with Z-pins10.1016/j.ijfatigue.2009.09.001 ↗
24. Microstructure and flexural properties of Z-pinned carbon fiber-reinforced aluminum matrix composites10.3390/ma12010174 ↗
25. Minimizing the in-plane damage of Z-pinned composite laminates via a pre-hole pin insertion process10.1016/j.compscitech.2020.108413 ↗
26. Strengthening of composite T-joints using Ø 0.11 mm Z-pins via an ultrasound-guided insertion process