Effect of laser energy density on microstructure and properties Cu–Fe–P immiscible alloys fabricated by laser selective melting: heterogeneous and high strength and magnetic

Min Xie, Fei Li, Shengfeng Zhou, Liangliang Lu, Fan Peng, Longjiang Zhang, Yaozhong Zhang, Yang Lu

Abstract

Through the incorporation of phosphorus (P) as a third component, an in-situ formation of a magnetic phase with a nanotwin structure was achieved. The utilization of selective laser melting (SLM) enabled the synthesis of a Cu-Fe-P immiscible alloy that exhibits an integrated structure and function. The microstructure predominantly consists of a magnetic heterogeneous Fe-P-rich phase, comprising a mixture of Fe2P and a small quantity of Fe3P, which is distributed within the ε-Cu Cu-rich matrix in alternating "fiber-layer" and "particle-shape" forms. Additionally, the fibrous Fe2P phase exhibited precipitation of α-Fe, while the Fe-P-rich phase experienced the precipitation of high-density nanotwinned Cu (nt-Cu) particles. The microstructure density and structural characteristics of Cu-Fe-P immiscible alloys were enhanced through the adjustment of laser energy density, leading to improvements in their mechanical and magnetic properties. It was observed that the microstructure density initially increased and then decreased with increasing laser energy density. The highest relative density of the Cu-Fe-P immiscible alloy microstructure (98%) was achieved at a laser energy density of 53 J/mm3. Furthermore, the influence of laser energy density on the mechanical and soft magnetic properties of Cu-Fe-P immiscible alloys was examined. The findings indicate that the mechanical and soft magnetic properties of these alloys are affected by the laser energy density. The findings indicate that the compact Cu-Fe-P immiscible alloys exhibit favorable compression mechanical properties and soft magnetic properties. Specifically, the ultimate compressive stress can reach 890.5±20 MPa, while the failure strain can reach 20.5±2%. Additionally, the coercivity is observed to be as low as 20.0 Oe, the magnetic saturation strength as high as 93.5 emu/g, and the residual magnetization at 1.1 emu/g.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Metallic Glasses and Amorphous Alloys

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Influence of Al addition on microstructure and properties of Cu-Fe-based coatings by laser induction hybrid rapid cladding10.1557/jmr.2014.64 ↗
2. Carbon nanotube- and Fep-reinforced copper-matrix composites by laser induction hybrid rapid cladding10.1016/j.scriptamat.2013.12.006 ↗
3. Investigation of Cu-Fe-based coating produced on copper alloy substrate by laser induction hybrid rapid cladding10.1016/j.optlastec.2013.12.013 ↗
4. Fe-shell/Cu-core encapsulated metallic phase change materials prepared by aerodynamic levitation method10.1016/j.apenergy.2014.07.054 ↗
5. Synthesis of Fep/Cu-Cup/Fe duplex composite coatings by laser cladding10.1016/j.matdes.2016.02.125 ↗
6. A bridge from monotectic alloys to liquid-phase-separated bulk metallic glasses: design, microstructure and phase evolution10.1016/j.actamat.2012.12.031 ↗
7. Enhanced corrosion resistance of Kirkendall-effect-induced hollow Fep-reinforced Cu-matrix immiscible alloys by laser powder deposition10.1016/j.jallcom.2018.11.215 ↗
8. Phase diagram of Fe-Cu-Si ternary system above 1523 K10.1361/105497199770335695 ↗
9. Effects of supercooling and cooling rate on the microstructure of Cu-Co-Fe alloys10.1007/s10853-006-5598-8 ↗
10. Design and formation mechanism of self-organized core/shell structure composite powder in immiscible liquid system
11. Enhanced strength and ductility of friction stir processed Cu-Al alloys with abundant twin boundaries10.1016/j.scriptamat.2013.01.003 ↗
12. Grain size dependence of tensile properties in ultrafine-grained Cu with nanoscale twins10.1016/j.scriptamat.2010.10.015 ↗
13. Three strategies to achieve uniform tensile deformation in a nanostructured metal10.1016/j.actamat.2003.12.022 ↗
14. Strengthening materials by engineering coherent internal boundaries at the nanoscale10.1126/science.1159610 ↗
15. In-situ Fe2P reinforced bulk Cu-Fe immiscible alloy with nanotwinned Cu produced by selective laser melting10.1016/j.jallcom.2020.155592 ↗
16. Nucleation and growth of γ-Fe precipitate in Cu-2%Fe alloy aged under high magnetic field10.1016/j.jallcom.2015.12.046 ↗
17. The microstructure and magnetic properties of nano-scale Fe magnetic particles precipitated in a Cu–Fe alloy10.3139/146.110288 ↗
18. TiB2- and Fe2P with nanotwins-reinforced Cu-based immiscible composites fabricated by selective laser melting: formation mechanism and wear behavior10.1016/j.jallcom.2021.158716 ↗
19. Effect of TiC particles on the liquid-liquid decomposition of Al-Pb alloys10.1016/j.matdes.2015.11.090 ↗
20. Development of a new class of high strength copper alloy using immiscibility route in Cu-Fe-Si system: evolution of hierarchical multi-scale microstructure10.1016/j.msea.2018.03.026 ↗
21. Interfacial tension, wetting and nucleation in Al-Bi and Al-Pb monotectic alloys10.1016/j.actamat.2011.07.031 ↗
22. The effect of atmosphere on the structure and properties of a selective laser melted Al-12Si alloy10.1016/j.msea.2014.01.012 ↗
23. Microstructure, residual stress, and mechanical properties evolution of a Cu-Fe-P alloy under different conditions10.1016/j.jmrt.2023.05.015 ↗
24. Tensile properties of copper with nano-scale twins10.1016/j.scriptamat.2005.01.033 ↗
25. Simultaneous improvement in strength and plasticity of Ti-24Nb-4Zr-8Sn manufactured by selective laser melting10.1016/j.matdes.2018.07.036 ↗
26. Low temperature deformation detwinning—a reverse mode of twinning10.1002/adem.201000123 ↗
27. Nano-sized twins induce high rate sensitivity of flow stress in pure copper10.1016/j.actamat.2005.01.031 ↗
28. Plastic deformation mechanisms in nanotwinned metals
29. On the fracture toughness of advanced materials10.1002/adma.200803322 ↗
30. Fracture behavior of heterogeneous nanostructured 316L austenitic stainless steel with nanotwin bundles10.1016/j.actamat.2018.02.065 ↗
31. The deformation of plastically non-homogeneous materials10.1080/14786437008238426 ↗
32. Tensile behavior and fracture in nickel and carbon doped nanocrystalline nickel10.1016/S0921-5093(00)01392-7 ↗