Microstructure and mechanical properties of laser butt welds of selective laser melted Ta10W alloy plates with different forming directions
Source abstract
Abstract
This study investigates the anisotropy effect of Ta10W alloy manufactured by selective laser melting (SLM) on the microstructure and mechanical properties of the three butt welds. The welds were characterized by formation, microstructure, microhardness, room temperature (RT) strength, high temperature (HT) strength, and fracture morphology. Results indicate that Ta10W manufactured by SLM exhibits anisotropy in microstructure and properties, leading to notable differences in the welds' microstructure and mechanical properties. When the base metal's X-axis aligns with the welding direction, the weld forms columnar sub-grains, whereas aligning the base metal's Z-axis with the welding direction results in equiaxed sub-grains in the weld. These distinct microstructures influence the maximum RT strength, with the X+X weld displaying significantly higher strength (751.33 MPa) compared to the X+Z (672.00 MPa) and Z+Z (667.25 MPa) welds. Fracture analysis reveals a transition from cleavage fracture to intergranular fracture in three welds. The microhardness and HT strength of the welds exhibit an inapparent difference, with the microhardness of approximately 305 HV0.2/15 and the HT (1800 °C) strength of around 110.50 MPa.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · Additive Manufacturing and 3D Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Effect of solution treatment on the microstructure of dissimilar welding joints of Ta-10W and GH312810.1088/2053-1591/ac0b78 ↗
2. Review of selective laser melting: materials and applications10.1063/1.4935926 ↗
3. The metallurgy and processing science of metal additive manufacturing10.1080/09506608.2015.1116649 ↗
4. Selective laser melting of aluminum and titanium matrix composites: recent progress and potential applications in the aerospace industry10.3390/aerospace7060077 ↗
5. Low- and high-cycle fatigue resistance of Ti-6Al-4V ELI additively manufactured via selective laser melting: mean stress and defect sensitivity10.1016/j.ijfatigue.2017.10.021 ↗
6. Varestraint weldability testing of additive manufactured alloy 71810.1080/13621718.2018.1437338 ↗
7. Review: laser welding of dissimilar materials (Al/Fe, Al/Ti, Al/Cu)-Methods and techniques, microstructure and properties10.3390/ma15010122 ↗
8. Seam properties of overlap welding strategies from copper to aluminum using green laser radiation for battery tab connections in electric vehicles10.3390/ma16031069 ↗
9. An overview on welding of Inconel 718 alloy-effect of welding processes on microstructural evolution and mechanical properties of joints10.1016/j.matchar.2021.110997 ↗
10. Conventional versus additive manufacturing in the structural performance of dense alumina-zirconia ceramics: 20 years of research, challenges and future perspectives10.1016/j.jmapro.2022.02.041 ↗
11. Ying · 2015
12. Microstructure and anisotropic mechanical properties of selective laser melted Ti6Al4V alloy under different scanning strategies10.1016/j.msea.2021.142236 ↗
13. Microstructure and mechanical properties of 3D-GH3536/R-GH3128 butt joint welded by fiber laser welding with focus rotation10.1016/j.jmrt.2022.03.073 ↗
14. Microstructure and properties of 3D-GH3625 electron beam welded
15. Laser welding of SLM-manufactured tubes made of IN625 and IN71810.3390/ma12182967 ↗
16. Laser welding of a selective laser melted Ni-base superalloy: microstructure and high temperature mechanical property10.1016/j.msea.2018.12.081 ↗
17. Study on the microstructure and fatigue behavior of a laser-welded Ni-based alloy manufactured by selective laser melting method10.1007/s11665-020-04844-4 ↗
18. Weldability, microstructure and mechanical properties of laser-welded selective laser melted 304 stainless steel joints10.1016/j.jmst.2019.04.017 ↗
19. Wang · 2017
20. Laser welding properties of In718 alloy prepared by selective laser melting
21. Cao · 2006
22. Effects of processing parameters on the densification, microstructure and mechanical properties of pure tungsten fabricated by optimized selective laser melting: from single and multiple scan tracks to bulk parts10.1016/j.ijrmhm.2021.105490 ↗
23. Non-equilibrium microstructure, crystallographic texture and morphological texture synergistically result in unusual mechanical properties of 3D printed 316L stainless steel
24. Anisotropy of nickel-based superalloy K418 fabricated by selective laser melting10.1016/j.pnsc.2018.07.001 ↗
25. Texture, anisotropy in microstructure and mechanical properties of IN738LC alloy processed by selective laser melting (SLM)10.1016/j.msea.2014.10.003 ↗
26. A study on the metal flow in full penetration laser beam welding for titanium alloy10.1016/j.commatsci.2003.11.002 ↗
27. Simulation and experiment for dynamics of laser welding keyhole and molten pool at different penetration status10.1007/s00170-020-06489-y ↗
28. Towards a map of solidification cracking risk in laser welding of austenitic stainless steels10.1016/j.phpro.2015.11.033 ↗
29. A review of laser powder bed fusion additive manufacturing of aluminium alloys: microstructure and properties
30. Drastic improvement in mechanical properties and weldability of 316L stainless steel weld joints by using electromagnetic vibration during GTAW process10.1016/j.jmapro.2018.05.002 ↗
31. Effect of welding processes on microstructural and mechanical properties of dissimilar weldments between conventional austenitic and high nitrogen austenitic stainless steels10.1016/j.jmapro.2016.10.008 ↗
32. Strain-rate dependence of the dynamic softening in a duplex stainless steel10.1016/j.matchar.2020.110219 ↗
33. Texture, microstructure and mechanical properties of laser beam welded AISI 2507 super duplex stainless steel10.1016/j.matchemphys.2022.126490 ↗
34. Microstructure evolution and mechanical properties of the dissimilar joint between IN718 and STS30410.1016/j.msea.2020.140262 ↗
35. Effect of anisotropy in thermal conductivity on grain boundary migration under temperature gradient–A phase field study10.1016/j.matlet.2021.130517 ↗
36. Research on the thermal conductivity of metals based on first principles
37. The effect of ultrasmall grain sizes on the thermal conductivity of nanocrystalline silicon thin films
38. Yang · 2004
39. Effects of casting methods on microstructure, thermal conductivity and mechanical properties of A356 aluminum alloy
40. Effects of Nd: YAG laser welding on microstructure and texture of aluminum-lithium Alloys
41. Additively manufactured hierarchical stainless steels with high strength and ductility10.1038/nmat5021 ↗
42. Effect of the morphology of long-period stacking ordered phase on mechanical properties and corrosion behavior of cast Mg-Zn-Y-Ti alloy10.1016/j.jallcom.2018.06.056 ↗
43. Effect of laser remelting on the microstructure and mechanical properties of AerMet100 steel fabricated by laser cladding10.1016/j.msea.2022.142951 ↗
44. Tensile properties and fracture behavior of ATI 718Plus alloy at room and elevated temperatures10.1007/s11661-021-06329-y ↗
45. Influence of heat treatment on oxygen content and mechanical properties of TaW10 alloy fabricated by hot isostatic pressing