Evolution of corrosion degradation in galvanised steel bolts exposed to a tropical marine environment
Source abstract
Abstract
The time-dependent degradation of galvanised steel bolts subjected to marine atmospheric exposure for a maximum period of 2 years in the Wenchang marine environment of Hainan province, South China, was investigated. The results showed that the zinc coating used as a protective surface finish deteriorated quickly due to the harsh environmental conditions. The deterioration of the zinc coating resulted in premature corrosion of the underlying steel substrate as early as 6 months. The main Zn corrosion products found at the initial exposure time were simonkollite (Zn5(OH)8Cl2·H2O), hydrozincite (Zn5(OH)6(CO3)2), and zincite (ZnO). At subsequent exposure times, major steel corrosion products such as lepidocrocite (γ-FeOOH), akaganeite (β-FeOOH), goethite (α-FeOOH), magnetite (Fe3O4), and maghemite (γ-Fe2O3) were detected. Fe3O4/γ-Fe2O3 was consistently found in the rust formed at both the exposed and crevice thread regions between 6 and 24 months of exposure. Based on the geometry of the bolt fastener, the corrosion rate and phase composition distribution varied between the two regions. Differences in oxygen exposure levels, corrosion kinetics, and electrochemical stability of the corrosion products were primary factors in these distinctive corrosion behaviours.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Concrete Corrosion and Durability · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. A review of recent developments in coating systems for hot-dip galvanized steel10.3389/fmats.2020.00074 ↗
2. Electrochemical monitoring of the degradation of galvanized steel in simulated marine atmosphere10.1016/j.corsci.2018.11.013 ↗
3. Electrochemical corrosion monitoring of galvanized steel under cyclic wet-dry conditions10.1016/S0010-938X(99)00057-8 ↗
4. Corrosion failure analysis of galvanized steel pipes in a closed water cooling system10.1016/j.engfailanal.2017.10.008 ↗
5. Microstructure characterization and corrosion resistance of zinc coating obtained on high-strength grade 10.9 bolts using a new thermal diffusion process10.3390/ma12091400 ↗
6. Atmospheric corrosion model for galvanized steel structures10.5006/1.3315903 ↗
7. Atmospheric corrosion of galvanized steel and precipitation runoff from zinc in a marine environment10.1590/S0103-50532013000300013 ↗
8. Atmospheric corrosion rates of copper, galvanized steel, carbon steel and aluminum in the metropolitan region of Salvador, BA, Northeast Brazil10.1016/j.proeng.2012.07.408 ↗
9. An assessment of climate change effects on atmospheric corrosion rates of steel structures10.1179/1743278213Y.0000000087 ↗
10. Atmospheric corrosion of zinc Part 2: marine atmospheres10.1179/000705900101501362 ↗
11. Atmospheric corrosion of galvanized steel and aluminium in marine and marine-industrial environments of Saudi Arabia10.1002/maco.200704075 ↗
12. Atmospheric corrosion performance of hot-dip galvanized bolts for fastening weathering steel guiderail
13. Corrosion and protection of galvanized steel in power grid10.1088/1755-1315/508/1/012059 ↗
14. Corrosion and corrosion products of hot dipped galvanized steel during long term atmospheric exposure at different sites world-wide10.1016/j.corsci.2017.06.025 ↗
15. Long-term use of galvanized steel in external applications. Aspects of patina formation, zinc runoff, barrier properties of surface treatments, and coatings and environmental fate10.1007/s10661-010-1377-8 ↗
16. Degradation mechanism of galvanized steel in wet-dry cyclic environment containing chloride ions10.1016/S0010-938X(03)00153-7 ↗
17. Atmospheric corrosion evaluation of electrogalvanized, hot-dip galvanized and galvannealed interstitial free steels using accelerated field and cyclic tests10.1016/j.surfcoat.2016.04.021 ↗
18. Perforation of coated steel panels on automobiles and its corrosion mechanism10.3323/jcorr1991.50.115 ↗
19. Insight to atmosphere corrosion behavior of Q345NH steel in Wenchang tropical marine environment10.1016/j.jmrt.2023.04.128 ↗
20. Understanding the role of alloyed Cu and P in the initial rust composition of weathering steel formed in a simulated coastal-industrial atmosphere10.1016/j.corsci.2021.109912 ↗
21. Deposition processes and properties of coatings on steel fasteners – a review10.1007/s40544-019-0304-4 ↗
22. Quantitative phase analysis of galvannealed coatings by coulometric stripping10.1023/A:1003435824284 ↗
23. The influence of microstructure and chemical composition of carbon and low alloy steels in CO2 corrosion. A state-of-the-art appraisal10.1016/S0261-3069(03)00158-4 ↗
24. Corrosion behavior of field-exposed zinc in a tropical marine atmosphere10.5006/1177 ↗
25. Synergistic effect of NaCl and SO2 on the initial atmospheric corrosion of zinc under wet–dry cyclic conditions10.1007/s40195-018-0863-9 ↗
26. Corrosion behaviour of carbon steel fasteners in neutral chloride solution10.1007/s40195-021-01284-4 ↗
27. Long-term atmospheric corrosion of zinc10.1016/j.corsci.2006.08.003 ↗
28. Zhang · 1996 · vol. 7
29. Insights into the characteristics of corrosion products formed on the contact and exposed regions of C1045 steel bolt and nut fasteners exposed to aqueous chloride environments10.1016/j.jmst.2022.06.037 ↗
30. RIR-measurement and use in quantitative XRD10.1017/S0885715600013257 ↗
31. Characterization of zinc-rich powder coatings by EIS and Raman spectroscopy10.1016/S0257-8972(02)00147-0 ↗
32. Synthesis and vibrational spectroscopic characterisation of synthetic hydrozincite and smithsonite10.1016/j.poly.2007.07.002 ↗
33. Underpaint corrosion of zinc-coated steel sheet studied by in situ Raman spectroscopy10.1016/0010-938X(93)90356-L ↗
34. On the formation of β-FeOOH (akaganéite) in chloride-containing environments10.1016/j.corsci.2006.06.003 ↗
35. An attempt to classify the morphologies presented by different rust phases formed during the exposure of carbon steel to marine atmospheres10.1016/j.matchar.2016.04.027 ↗
36. Monitoring the development of rust layers on weathering steel using in situ Raman spectroscopy under wet-and-dry cyclic conditions10.1007/s10008-015-2825-8 ↗
37. Raman spectroscopy of iron oxides and (oxy)hydroxides at low laser power and possible applications in environmental magnetic studies10.1111/j.1365-246X.2009.04122.x ↗
38. Characterization of iron oxides commonly formed as corrosion products on steel10.1023/A:1011076308501 ↗
39. Insight into atmospheric corrosion evolution of mild steel in a simulated coastal atmosphere10.1016/j.jmst.2020.11.021 ↗
40. Atmospheric corrosion performance of structural steel bolts in the Wenchang marine environment , South China10.1016/j.engfailanal.2023.107352 ↗
41. Studies on the initial stages of zinc atmospheric corrosion in the presence of chloride10.1016/j.corsci.2005.12.007 ↗
42. Atmospheric corrosion behavior of carbon steel and galvanized steel after exposure in eretan and ciwaringin, West Java Province, Indonesia10.22146/ijc.46755 ↗
43. The effect of magnesium on the corrosion of hot‐dip galvanized steel in chloride10.1002/maco.201307278 ↗
44. Corrosion products formed on confined hot-dip galvanized steel in accelerated cyclic corrosion tests10.5006/1.3319098 ↗
45. Atmospheric corrosion10.1016/B978-075065924-6/50011-8 ↗