Deformation and strengthening behaviors of Al–Cu–Mg alloy thick plate during hot forming-quenching integrated process
Source abstract
Abstract
The deformation and effective die quenching are critical to ensure the final dimensional accuracy and strength of the thick-walled curved components in hot forming-quenching integrated process. The deformation behavior of an Al–Cu–Mg alloy plate during bending-quenching process was thus analyzed at different temperatures and die clearances. The strengthening behavior along thickness and radial directions was evaluated under different heating and die quenching conditions. The strengthening mechanism was revealed by microstructure observation. It is found that the smaller die clearance and higher heating temperature contribute to improve the dimensional accuracy. The water-cooled die quenching can ensure the effective quenching of a bended specimen with 25 mm in thickness, being at the strengthening level of peak aging. And, the effective quenching thickness reaches 50 mm at least. Dynamic recovery is the main restoration mechanism in the integrated process. The hardness reduces while air cooling due to the formation of coarse S precipitates with average size exceeding 750 nm. Finally, a large-size tapered thick plate component with superior dimensional accuracy was successfully fabricated under the guidance of the obtained results.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Metal Forming Simulation Techniques · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Fundamentals and processes of fluid pressure forming technology for complex thin-walled components10.1016/j.eng.2020.08.014 ↗
2. Hot damage evolution in a high strength aluminum alloy during hot forming: a study using the Gurson-Tvergaard-Needleman model10.1016/j.jmrt.2021.07.066 ↗
3. Recent developments in advanced aircraft aluminium alloys10.1016/j.matdes.2013.12.002 ↗
4. NASA's space launch system takes shape: progress toward safe, affordable exploration
5. Study on microstructure and fracture characteristics of 5083 aluminum alloy thick plate10.1016/j.jallcom.2020.153960 ↗
6. Distortion caused by residual stresses in machining aeronautical aluminum alloy parts: recent advances10.1007/s00170-016-9066-6 ↗
7. A review on forming techniques for manufacturing lightweight complex-shaped aluminum panel components
8. Lin · 2008
9. Effects of hot forming cold die quenching and inter-pass solution treatment on the evolution of microstructure and mechanical properties of AA2024 aluminum alloy after equal channel angular pressing10.1016/j.jmrt.2019.11.092 ↗
10. A review on hot stamping10.1016/j.jmatprotec.2010.07.019 ↗
11. Effects of hot forming cold die quenching and solution treatment on formability and pressing load during equal channel angular deformation of AA2024 aluminum alloy10.1016/j.jmrt.2020.03.085 ↗
12. Experimental investigation of novel fast-ageing treatments for AA6082 in supersaturated solid solution state10.1016/j.jallcom.2019.151934 ↗
13. Investigation of deformation and failure features in hot stamping of AA6082: experimentation and modelling10.1016/j.ijmachtools.2011.07.005 ↗
14. Deformation of AA6016 aluminum alloy sheets at high temperature and strain rate10.4028/www.scientific.net/MSF.783-786.114 ↗
15. Formability and failure mechanisms of AA2024 under hot forming conditions10.1016/j.msea.2010.11.084 ↗
16. Formability evaluation for sheet metals under hot stamping conditions by a novel biaxial testing system and a new materials model10.1016/j.ijmecsci.2016.11.022 ↗
17. An experimental and numerical investigation on the formability of AA7075 sheet in hot stamping condition10.1007/s00170-017-0419-6 ↗
18. Experimental investigation on hot forming–quenching integrated process of 6A02 aluminum alloy sheet10.1016/j.msea.2013.02.058 ↗
19. Influence of thermal deformation parameters on mechanical properties and microstructure evolution of AA7075 aluminum alloy during hot stamping-quenching process
20. The effect of hot form quench (HFQ®) conditions on precipitation and mechanical properties of aluminum alloys10.1016/j.msea.2019.06.027 ↗
21. Formability and strengthening mechanism of solution treated Al-Mg-Si alloy sheet under hot stamping conditions10.1016/j.jmatprotec.2015.10.016 ↗
22. Investigations on warm forming of AW-7020-T6 alloy sheet10.1016/j.jmatprotec.2014.03.024 ↗
23. Hot stamping of high-strength aluminum alloy aircraft parts using quick heating10.1016/j.cirp.2017.04.117 ↗
24. Feasibility study on direct flame impingement heating applied for the solution heat treatment, forming and cold die quenching technique10.1016/j.jmapro.2018.10.020 ↗
25. Numerical study of the solution heat treatment, forming, and in-die quenching (HFQ) process on AA575410.1016/j.ijmachtools.2014.07.008 ↗
26. Prediction of thinning behavior for complex-shaped, lightweight alloy panels formed through a hot stamping process
27. Advances in FEM Simulation of HFQ® AA6082 tailor welded blanks for automotive applications10.1088/1757-899X/418/1/012036 ↗
28. Hot forming and quenching pilot process development for low cost and low environmental impact manufacturing
29. Review on sheet metal forming process of aluminium alloys
30. Integrated hot forming and heat treatment process on Al6061 tailor rolled blank10.1007/s12541-017-0016-5 ↗
31. Feasibility study on application of hot forming quenching to patchwork blanks using two-stage refilled friction stir spot welding10.1016/j.jmapro.2019.03.012 ↗
32. Development of a partition panel of an Al6061 sheet metal part for the improvement of formability and mechanical properties by hot forming quenching10.1177/1687814017691213 ↗
33. Application of hot forming cold die quenching for facilitating equal channel angular pressing of AA2024 aluminum alloy10.1016/j.jallcom.2019.03.059 ↗
34. The thermodynamics of and strengthening due to coclusters: general theory and application to the case of Al-Cu-Mg alloys10.1016/j.actamat.2009.01.021 ↗
35. Precipitates and intermetallic phases in precipitation hardening Al-Cu-Mg-(Li) based alloys10.1179/174328005X14357 ↗
36. Double-peak age strengthening of cold-worked 2024 aluminum alloy10.1016/j.actamat.2012.11.039 ↗