Microstructure evolution and creep behavior of nitrogen-bearing austenitic Fe–Cr–Ni heat-resistant alloys with various carbon contents
Source abstract
Abstract
In the petrochemical industry, centrifugal cast Fe–Cr–Ni heat-resistant alloy tubes are critical components that are exposed to severe conditions for long-time service. The life of the alloy tubes is primarily limited by creep damages, which can evolve into catastrophic failures. In order to improve the creep properties in a low-cost approach, the influence of N + C content on the microstructure evolution and creep behavior of the 25Cr35NiNb alloys has been studied in this work. Creep tests were carried out at 1173 K (900 °C) and 1323 K (1050 °C) with different stress levels. Microstructure investigation on precipitates revealed that the C/N ratio significantly affects the content and morphology of Cr-rich carbides and the phase transition of Nb-rich carbonitrides after thermal exposure. By adopting the threshold stress analysis, the true creep activation energy and stress exponent of all the alloys were found to be ∼270 kJ mol−1 and ∼5, respectively, which indicated that dislocation climb is the rate-controlling mechanism of creep. Furthermore, the tailored novel N-bearing alloy possessed superior comprehensive properties of creep resistance and damage tolerance compared to the 25Cr35NiNb grade alloys. Our current findings not only realize improved creep properties by the combined modification of N addition and C/N ratio, but also provide new insights into understanding the microalloying mechanisms of high-temperature materials in general.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: High Temperature Alloys and Creep · Nuclear Materials and Properties · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. Precipitation and hot deformation behavior of austenitic heat-resistant steels: a review10.1016/j.jmst.2017.01.025 ↗
2. Effect of high temperature service on the complex through-wall microstructure of centrifugally cast HP40 reformer tube10.1016/j.matchar.2021.111070 ↗
3. Failure analyses of centrifugal casting ethylene pyrolysis furnace tubes from microporosity defects10.1016/j.engfailanal.2019.04.059 ↗
4. Experimental observation and crystallographic description of M7C3 carbide transformation in Fe-Cr-Ni-C HP type alloy10.1016/j.actamat.2015.08.056 ↗
5. Enhanced high-temperature oxidation resistance of low-cost Fe–Cr–Ni medium entropy alloy by Ce-adulterated10.1016/j.jmrt.2021.12.087 ↗
6. Microstructural and failure analysis of welded primary reformer furnace tube made of HP-Nb micro alloyed heat resistant steel10.1016/j.engfailanal.2016.05.023 ↗
7. Microstructural evolution in creep aged of directionally solidified heat resistant HP-Nb steel alloyed with tungsten and nitrogen10.1016/j.msea.2016.02.046 ↗
8. Titanium micro addition in a centrifugally cast HPNb alloy: high temperature mechanical properties10.1016/j.msea.2015.03.085 ↗
9. Influence of niobium addition on the high temperature mechanical properties of a centrifugally cast HP alloy10.1016/j.msea.2015.01.049 ↗
10. Use of titanium and zirconium in centrifugally cast heat resistant steel10.1179/174328407X168766 ↗
11. Phase transformations in Fe–Ni–Cr heat-resistant alloys for reformer tube applications10.1080/02670836.2018.1449177 ↗
12. Gavriljuk · 1999
13. Effects of metal composition and temperature on the yield strength of nitrogen strengthened stainless steels10.1016/0921-5093(95)10031-8 ↗
14. Influence of nitrogen and grain size on deformation behaviour of austenitic stainless steels10.1179/mst.1997.13.7.560 ↗
15. Precipitation of σ-phase in high-nitrogen austenitic 18Cr–18Mn–2Mo–0.9N stainless steel during isothermal aging10.1016/j.scriptamat.2004.02.013 ↗
16. Influence of nitrogen-induced grain refinement on mechanical properties of nitrogen alloyed type 316LN stainless steel10.1016/j.jnucmat.2011.11.001 ↗
17. Competing mechanisms and modeling of deformation in austenitic stainless steel single crystals with and without nitrogen10.1016/S1359-6454(01)00296-8 ↗
18. Improving creep strength of 316L stainless steel by alloying with nitrogen10.1016/j.msea.2011.12.044 ↗
19. Recent developments in stainless steels10.1016/j.mser.2009.03.001 ↗
20. Precipitation in creep resistant austenitic stainless steels10.1179/026708301101508972 ↗
21. Effects of N and Cu on the precipitation and the creep life of 316L austenitic stainless steel at 650°C10.1016/j.msea.2016.03.054 ↗
22. Effects of N/C ratio on solidification behaviors of novel Nb-bearing austenitic heat-resistant cast steels for exhaust components of gasoline engines10.1007/s11661-016-3920-x ↗
23. Microstructure control and optimization of centrifugal casting furnace tube HP40 alloys based on CAFE model
24. Abnormal creep stress exponents in a high-pressure die casting Mg–Al−RE alloy10.1016/j.msea.2021.142203 ↗
25. Carbide transformation in carburised zone of 25Cr35NiNb+MA alloy after high-temperature service10.1080/09603409.2015.1130330 ↗
26. Effect of microstructural evolution in thermal exposure on mechanical properties of HP40Nb alloy10.1016/j.ijpvp.2021.104391 ↗
27. Ultrahigh stability and strong precipitation strengthening of nanosized NbC in alumina-forming austenitic stainless steels subjecting to long-term high-temperature exposure10.1016/j.msea.2018.09.081 ↗
28. Evolution of microstructure during tensile creep deformation of nickel-based disk superalloy10.1016/j.ijpvp.2021.104539 ↗
29. Effects of nitrogen on precipitation and tensile behaviors of 25Cr 20Ni austenitic stainless steels at elevated temperatures10.1016/j.msea.2019.03.004 ↗
30. Review of Z phase precipitation in 9-12 wt-%Cr steels10.1179/1743284715Y.0000000066 ↗
31. Enhancing creep resistance of aged Fe–Cr–Ni medium-entropy alloy via nano-sized Cu-rich and NbC precipitates investigated by nanoindentation10.1016/j.jmrt.2022.08.018 ↗
32. Variations of the microstructure and mechanical properties of HP40Nb hydrogen reformer tube with time at elevated temperature10.1016/j.matdes.2010.08.031 ↗
33. A deep learning-aided prediction approach for creep rupture time of Fe–Cr–Ni heat-resistant alloys by integrating textual and visual features10.1016/j.jmrt.2022.02.099 ↗
34. Creep resistance of Fe–Ni–Cr heat resistant alloys for reformer tube applications10.1080/02670836.2019.1648371 ↗
35. Effects of trace Pb on creep and fracture of 25Cr35Ni-Nb alloy
36. A comparative study of constitutive equations for the creep deformation of HP40Nb micro-alloyed steel10.1016/j.msea.2015.09.087 ↗
37. Sulfur effects on high-temperature creep and fracture behavior of 25Cr35Ni-Ni alloys10.1115/1.4026597 ↗
38. Creep and tensile behaviour of austenitic Fe-Cr-Ni stainless steels10.1016/j.msea.2008.04.098 ↗
39. 1991
40. Damage analysis in Fe–Cr–Ni centrifugally cast alloy tubes for reforming furnaces10.1016/j.engfailanal.2013.09.020 ↗
41. Theory of steady-state creep based on dislocation climb10.1063/1.1721875 ↗
42. Self-diffusion of the components in the FCC phase of binary solid solutions of the Fe-Ni-Cr system10.1016/0025-5416(81)90086-0 ↗
43. Creep properties and microstructure of a precipitation-strengthened ferritic Fe–Al–Ni–Cr alloy10.1016/j.actamat.2014.02.020 ↗
44. An examination of the constitutive equation for elevated temperature plasticity10.1016/S0921-5093(01)01115-7 ↗
45. Threshold stress creep behavior of alloy 617 at intermediate temperatures10.1007/s11661-014-2244-y ↗
46. Creep damage mechanics and micromechanisms
47. Creep deformation behavior of 9Cr1MoVNb (ASME Grade 91) steel10.1016/j.msea.2016.10.112 ↗