journal article·2023-05Open access

Effect of rare-earth Sc on the interface microstructure and mechanical properties of Al/steel bimetallic composites prepared by liquid–solid casting

Po Zhang, Feng Mao, Yu Wang, Chong Chen, Mei Xiong, Shizhong Wei, Tao Jiang, Changji Wang, Cheng Zhang, Zhou Wang

Abstract

In this study, scanning electron microscopy (SEM), electron backscatter diffraction analysis (EBSD), and electron probe microanalysis (EPMA) were used to investigate the impact of rare-earth Sc on the interface microstructure and mechanical properties of Al/steel bimetallic composites fabricated by liquid–solid casting. With the addition of 0.3% Sc, the morphology of eutectic Si changed from needle-like to fibrous and granular. The addition of Sc did not change the types of intermetallic compounds in the Al/steel reaction layer, which comprised the Al5Fe2, τ1-Al2Fe3Si3, Al13Fe4, τ5-Al7Fe2Si, and τ6-Al9Fe2Si2 phases. The thickness of the first layer decreased, whereas that of the second layer increased as the Sc content increased to 0.3%. Furthermore, the Al5Fe2 and τ1 phase percentages of the reaction layer decreased, whereas the Al13Fe4, τ5, and τ6 phase percentages increased. Sc was mainly enriched in the front of the ternary compound layer (τ6) near the Al side. The addition of 0.3% Sc reduced the grain size of each phase in the interfacial reaction layer and did not change the preferred orientation of the Al5Fe2, Al13Fe4, τ5, and τ6 phases, but increased the polar density of the Al13Fe4, τ5, and τ6 phases and decreased the polar density of the Al5Fe2 phase. With the addition of 0.3% Sc, the average nanohardness of the reaction layer decreased by 5% and the bonding strength increased by 48%.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Interface formation in aluminium–aluminium compound casting10.1016/j.actamat.2008.02.042 ↗
2. Review and challenges of lightweight composite hydraulic cylinder10.3901/JME.2021.24.013 ↗
3. Investigation of the effect of process parameters on surface roughness in wire EDM of titanium alloy
4. Tribological performance of additively manufactured AISI H13 steel in different surface conditions10.3390/ma14040928 ↗
5. Investigation of microstructure and wear resistance of laser-clad CoCrNiTi and CrFeNiTi medium-entropy alloy coatings on Ti sheet10.1016/j.optlastec.2021.107518 ↗
6. Surface modification of Ti-based alloy by selective laser melting of Ni-based superalloy powder10.1016/j.jmrt.2020.06.016 ↗
7. Hydrogen trapping mechanism of different duplex stainless steels alloys10.1016/j.jallcom.2015.04.176 ↗
8. Effect of Si content in hot dipping aluminium bath on Al–Fe bonding layer of aluminium piston with reinforced cast iron ring10.1179/1743284712Y.0000000034 ↗
9. Squeeze cast aluminium reinforced with mild steel inserts10.1007/BF00367873 ↗
10. Ultrasonic insert casting of aluminum alloy10.1016/S1359-6462(00)00385-7 ↗
11. New development of studying liquid-solid double-metal compound interface
12. Effect of aluminum surface treatment on structures and properties of liquid-solid diffusion bonding interface of AM60/A390
13. Influences of alloying elements on the interfacial reaction of Fe/Al: a review
14. Microstructure and mechanical properties of diffusion-bonded Mg–Al joints using silver film as interlayer10.1016/j.msea.2012.09.035 ↗
15. The enhancing effect of surface coatings on cast-in bonding of steel and titanium inserts in aluminium castings10.1080/13640461.2001.11819417 ↗
16. An investigation on diffusion bonding of aluminum and magnesium using a Ni interlayer10.1016/j.matlet.2012.06.014 ↗
17. Study on the importance of thermo-elastic effects in FE simulations of linear friction welding10.1016/j.jmapro.2020.05.051 ↗
18. Growth of intermetallic layer in the aluminide mild steel during hot-dipping10.1016/j.surfcoat.2009.09.061 ↗
19. Characterization of intermetallics in aluminum to zinc coated interstitial free steel joining by pulsed MIG brazing for automotive application10.1016/j.matchar.2015.12.030 ↗
20. Interaction between the growth and dissolution of intermetallic compounds in the interfacial reaction between solid iron and liquid aluminum10.1007/s11661-016-3667-4 ↗
21. Effects of trace Ce on strengthening and fracture mechanisms of Al-Li-Cu-Mg-Ag-Zr alloy
22. Effect of rare-earth element additions on high-temperature mechanical properties of AZ91 magnesium alloy10.1007/s11661-005-0022-6 ↗
23. Effect of La on intermetallic layer of galvalume10.1179/1743294413Y.0000000128 ↗
24. Influences of Ce on growth and microstructure of intermediate compounds of aluminum-zinc coating
25. Effect of Sc addition and T6 aging treatment on the microstructure modification and mechanical properties of A356 alloy10.1016/j.msea.2016.08.022 ↗
26. On the reaction scheme and liquidus surface in the ternary system Al-Fe-Si10.1007/s11661-007-9182-x ↗
27. Microstructural evolution of intermetallic layer in hot-dipped aluminide mild steel with silicon addition10.1016/j.surfcoat.2011.04.061 ↗
28. Effect of chromium on the formation of intermetallic phases in hot-dipped aluminide Cr–Mo steels10.1016/j.apsusc.2013.04.015 ↗
29. Crystallography of Fe2Al5 phase at the interface between solid Fe and liquid Al10.1016/j.intermet.2015.07.011 ↗
30. First principle calculations and mechanical properties of the intermetallic compounds in a laser welded steel/aluminum joint10.1016/j.optlastec.2019.105875 ↗
31. Structural studies of hot dip aluminized coatings on mild steel10.2320/matertrans1989.32.1053 ↗
32. Metallurgy of continuous hot dip aluminizing10.1179/imr.1994.39.5.191 ↗
33. Morphology and formation of Fe–Al intermetallic layers on iron hot-dipped in Al–Mg–Si alloy melt10.1016/j.intermet.2014.06.003 ↗