Investigate on the phase interfaces and performance evaluation of TiB2p/Al–Si–Cu–Zn (T6) composites
Source abstract
Abstract
In this paper, the microstructures, mechanical properties, and corrosion behavior of xTiB2/Al–9Si–3Cu-0.8Zn composites after T6 heat treatment were invested in detail through the combination of different technologies, including optical microscopy (OM), X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), tensile testing, corrosion testing, etc. The research results showed that the average size of the α-Al grains gradually decreased with the increase of TiB2 particles (TiB2p) content. In addition, there was a semi-coherent relationship between TiB2p and the α-Al matrix, and the nanoscale precipitates were identified as θ and θʹ phases by virtue of their crystal orientation relationship. Tensile testing results revealed that an increase in TiB2 content caused the elastic modulus, yield strength and tensile strength of the composites to increase and then decrease. And with a TiB2p content of 4 wt%, they reached 85.7 GPa, 360 MPa and 398 MPa, reflecting increases of 26.2%, 60.0%, and 30.9%, respectively. The contributions of thermal mismatch, grain boundary and Orowan strengthening mechanisms to the overall yield strength of the 4%TiB2/Al–9Si–3Cu–0.8Zn composite were 72.1, 3.8, and 35.6 MPa, respectively. Unfortunately, the corrosion resistance of xTiB2/Al–9Si–3Cu–0.8Zn composites gradually decreased with increasing TiB2p content. The corrosion morphology analysis indicated that the agglomeration of TiB2p and Si weakened the protection afforded by the oxide film, evolving into a point of nucleation for the subsequent corrosion reaction. Moreover, point–pair correlation was observed between the TiB2p and Al matrix, exacerbating the corrosion. The results implied that extra factors be considered in industrial application of TiB2 ceramic particles in a metallic system.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Enhanced strength and ductility of A356 alloy due to composite effect of near-rapid solidification and thermo-mechanical treatment10.1016/j.msea.2019.03.039 ↗
2. Effects of the addition of trace amounts of Sc on the microstructure and mechanical properties of Al-11.6Si alloys10.1016/j.msea.2018.03.016 ↗
3. Morphological transformation mechanism of eutectic Si phases in Al-Si alloys by nano-AlNp10.1016/j.jallcom.2018.06.223 ↗
4. Processing, multiscale microstructure refinement and mechanical property enhancement of hypoeutectic Al–Si alloys via in situ bimodal-sized TiB2 particles10.1016/j.msea.2020.139081 ↗
5. 3D imaging and quantification of porosity and intermetallic particles in strontium modified Al-Si alloys10.1016/j.jallcom.2017.08.146 ↗
6. Microstructure evolution and enhanced mechanical properties of eutectic Al-Si die cast alloy by combined alloying Mg and La10.1016/j.matdes.2015.10.078 ↗
7. Er addition to Al-Si-Mg-based casting alloy: effects on microstructure, room and high temperature mechanical properties10.1016/j.jallcom.2017.03.076 ↗
8. Effect of cooling rate and Mg content on the Al-Si eutectic for Al-Si-Cu-Mg alloys10.1016/j.matchar.2014.06.009 ↗
9. Effect of Si, Cu and processing parameters on Al-Si-Cu HPDC castings10.1016/j.jmatprotec.2017.06.043 ↗
10. Effects of Cu content and Cu/Mg ratio on the microstructure and mechanical properties of Al-Si-Cu-Mg alloys10.1016/j.jallcom.2015.07.090 ↗
11. Effects of heat treatments and minor addition of small amounts of Cu and Mg on the microstructure and mechanical properties of Al-Si-Cu and Al-Si-Mg cast alloys10.1016/j.jallcom.2018.12.365 ↗
12. Laser solid forming additive manufacturing TiB2 reinforced 2024Al composite: microstructure and mechanical properties10.1016/j.msea.2018.12.072 ↗
13. Effect of semi-solid forging on microstructure and mechanical properties of in-situ cast Al-Cu-TiB2 composites10.1016/j.jallcom.2017.04.113 ↗
14. Microstructure and mechanical properties of an in-situ TiB2/Al-Zn-Mg-Cu-Zr composite fabricated by Melt-SHS process10.1016/j.msea.2018.02.025 ↗
15. High as-cast strength die-cast AlSi9Cu2Mg alloy prepared by nanoparticle strengthening with industrially acceptable ductility10.1016/j.jallcom.2020.156873 ↗
16. High modulus Al-Si-Mg-Cu/Mg2Si-TiB2 hybrid nanocomposite: microstructural characteristics and micromechanics-based analysis10.1016/j.jallcom.2016.10.016 ↗
17. Atomic structure and interface chemistry in a high-stiffness and high-strength Al–Si–Mg/TiB2 nanocomposite10.1016/j.msea.2019.138072 ↗
18. Edge-to-edge matching and its applications10.1016/j.actamat.2004.11.007 ↗
19. Influence of TiB2 particles on aging behavior of in-situ TiB2/Al-4.5Cu composites10.1016/j.msea.2018.02.099 ↗
20. Mechanical properties enhanced by deformation–modified precipitation of θ'-phase approximants in an Al-Cu alloy10.1016/j.msea.2016.08.068 ↗
21. Precipitation behavior in an Al–Cu–Mg–Si alloy during ageing10.1016/j.msea.2019.138369 ↗
22. Enhanced age-hardening behavior in Al–Cu alloys induced by in-situ synthesized TiC nanoparticles10.1016/j.jmst.2018.09.029 ↗
23. Corrosion behavior of stir-cast Al-TiB2 metal matrix composites
24. Microstructural, mechanical and corrosion behaviour of Al–Si alloy reinforced with SiC metal matrix composite10.1177/0021998319856679 ↗
25. Electrochemical behavior of Al-B4C metal matrix composites in NaCl solution10.3390/ma8095314 ↗
26. Impact behavior of in situ TiB2/Al composite at various temperatures10.1007/s10853-011-5454-3 ↗
27. Effect of friction stir processing on corrosion of Al-TiB2 based composite in 3.5 wt.% sodium chloride solution
28. Quantitative study of particle size distribution in an in-situ grown Al-TiB2 composite by synchrotron X-ray diffraction and electron microscopy10.1016/j.matchar.2015.03.003 ↗
29. The nucleation sites of primary Si in Al-Si alloys after addition of boron and phosphorus10.1016/j.jallcom.2004.09.003 ↗
30. On the growth mechanism of the primary silicon particle in a hypereutectic Al-20 wt%Si alloy using synchrotron X-ray tomography10.1016/j.matdes.2017.09.062 ↗
31. Precipitation processes in Al-Cu-Mg alloys micro-alloyed with Si10.1007/BF02830331 ↗
32. Investigation and measurement of porosity in Al + 4.5Cu/6wt%TiB2 in situ composite: optimization and statistical modelling10.1016/j.jmrt.2020.05.045 ↗
33. The superior elevated-temperature mechanical properties of Al-Cu-Mg-Si composites reinforced with in situ hybrid-sized TiCx-TiB2 particles10.1016/j.msea.2018.05.024 ↗
34. Preparation, microstructures and mechanical properties of in-situ (TiB2 + ZrB2)/AlSi9Cu3 composites10.1016/j.jallcom.2016.02.243 ↗
35. Influence of dislocation–solute atom interactions and stacking fault energy on grain size of single-phase alloys after severe plastic deformation using high-pressure torsion10.1016/j.actamat.2014.01.036 ↗
36. Effects of stress state, strain rate, and temperature on fracture behavior of in situ TiB2/2024 Al composite10.1016/j.mechmat.2020.103641 ↗
37. An investigation on grain refinement mechanism of TiB2 particulate reinforced AZ91 composites and its effect on mechanical properties10.1016/j.jallcom.2018.11.253 ↗
38. Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy10.1016/j.actamat.2013.09.042 ↗
39. Effects of in-situ synthesized TiB2 on crystallographic orientation, grain size and nanohardness of AA6061 alloy by laser surface alloying10.1016/j.matlet.2019.06.075 ↗
40. Nanocrystalline Al–Mg alloy with ultrahigh strength and good ductility10.1016/j.scriptamat.2005.09.028 ↗
41. Microstructures and mechanical properties of ultrafine grained 7075 Al alloy processed by ECAP and their evolutions during annealing10.1016/j.actamat.2004.06.017 ↗
42. Numerical simulation of fracture behavior of in-situ TiB2 particle reinforced 2024-T4 aluminum matrix composites