journal article·2023-01Open access

High-temperature oxidation behavior and pore structure of porous TiAl3 intermetallics at 650 °C to 900 °C

Xinyang Jiao, Yu Zhang, Qingli Wu, Zhichao Shang, Yang Yu, Xiaoxiao Zhang, Peizhong Feng

Abstract

Porous TiAl3 materials were prepared by a time- and energy-saving thermal explosion (TE) method with Ti-75 at% Al mixture powders. Cyclic oxidation tests were performed in air at 650 °C, 800 °C, and 900 °C. Only a weak peak of the oxide phase was detected by X-ray diffraction when the oxidation temperature was below 800 °C. The pore structures remained stable without pore blockage or collapse due to the thin protective oxide layer formed on the surface of the product skeleton at 650 °C, which was confirmed to be Al2O3. The thickness of the oxide scale increased with increasing the oxidation temperature from 800 °C to 900 °C. The compressive strength of the oxidized sample was inversely proportional to its corresponding porosity. Additionally, the antioxidant mechanism at high temperature was further investigated, indicating excellent oxidation resistance. Therefore, porous TiAl3 intermetallic can be considered as promising materials for applications such as filtration, separation, and catalysis at a high temperatures up to 800 °C.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Catalytic Processes in Materials Science · Advanced ceramic materials synthesis · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. Fabrication of Ti-Al micro/nanometer-sized porous alloys through the Kirkendall effect10.1002/adma.200602398 ↗
2. Nickel-aluminum diffusion: a study of evolution of microstructure and phase10.1016/j.matchar.2017.05.039 ↗
3. Visible observation and formation mechanism of porous TiAl3 intermetallics during the continuous sintering process
4. Application of porous TiAl intermetallic compound in purification of industrial TiCl4 liquid in Ti metallurgy
5. Preparation of ceramic membranes on porous Ti–Al alloy supports by an in-situ oxidation method10.1016/j.memsci.2014.10.053 ↗
6. Experimental study on the treatment of high temperature flue gas using FeAl membrane filtration materials
7. Fabrication of TiAl intermetallic phases by heat treatment of warm sprayed metal precursors10.1016/j.intermet.2013.12.011 ↗
8. Reaction behavior and pore formation mechanism of TiAl–Nb porous alloys prepared by elemental powder metallurgy10.1016/j.intermet.2013.08.001 ↗
9. Fabrication of Ti-Si intermetallic compound porous membrane using an in-situ reactive sintering process10.1016/j.matlet.2020.127786 ↗
10. Reactive synthesis and characterization of titanium aluminides produced from elemental powder mixtures10.1007/s10973-015-4815-6 ↗
11. Progress of porous Al-containing intermetallics fabricated by combustion synthesis reactions: a review10.1007/s10853-021-06035-5 ↗
12. Fe-Al intermetallic foam with porosity above 60% prepared by thermal explosion10.1016/j.jallcom.2017.10.228 ↗
13. Fabrication and characterization of highly porous FeAl-based intermetallics by thermal explosion reaction10.1002/adem.201801110 ↗
14. Synthesis, microstructure and properties of Ti–Al porous intermetallic compounds prepared by a thermal explosion reaction10.1039/C5RA04047G ↗
15. Microstructure and formation mechanism of porous Ti-Al Intermetallics prepared by pressureless sintering
16. Effect of heating rate on porous TiAl-based intermetallics synthesized by thermal explosion10.1080/10426914.2016.1232826 ↗
17. Porous NbAl3/TiAl3 intermetallic composites with controllable porosity and pore morphology prepared by two-step thermal explosion10.1016/j.jmrt.2019.05.007 ↗
18. A novel fabrication strategy for highly porous FeAl/Al2O3 composite by thermal explosion in vacuum10.1016/j.vacuum.2017.12.043 ↗
19. Rapid preparation of porous Ni–Al intermetallics by thermal explosion10.1080/00102202.2019.1576652 ↗
20. Influences of sintering parameters on shape-retention ability of porous Ni3Al intermetallic fabricated by powder metallurgy10.1016/j.intermet.2018.11.009 ↗
21. Reaction mechanism and oxidation resistance at 700–900°C of high porosity NiAl intermetallic10.1016/j.corsci.2021.109731 ↗
22. Diffusion of oxygen in the Al2O3 oxidation product of TiAl310.1007/s11661-000-0081-7 ↗
23. Oxidation behavior of porous NiAl prepared through reactive synthesis10.1016/j.matchemphys.2010.03.017 ↗
24. The interaction of thin NiO layers with single crystalline α-Al2O3 (1120) substrates10.1016/0039-6028(95)00063-1 ↗
25. XPS studies of SiO2-TiO2 powders prepared by sol-gel process10.1016/0169-4332(93)90433-C ↗
26. High-temperature oxidation of Ti–Al–Si alloys prepared by powder metallurgy10.1016/j.jallcom.2019.151895 ↗
27. High-temperature behaviour of Ti-Al-Si alloys produced by reactive sintering10.1016/j.jallcom.2010.05.115 ↗
28. Environmental corrosion resistance of porous TiAl intermetallic compounds10.1016/S1003-6326(08)60316-7 ↗
29. Effect of Al content on porous Ni–Al alloys10.1016/j.msea.2011.02.014 ↗
30. Open-celled porous NiAl intermetallics prepared by replication of carbamide space-holders10.1016/S1003-6326(11)60925-4 ↗
31. Rapid reactive synthesis of TiAl3 intermetallics by thermal explosion and its oxidation resistance at high temperature10.1016/j.pnsc.2019.05.002 ↗