Enhanced high temperature strength in near-eutectic Al–8Ce alloy through Y addition by gravity casting
Source abstract
Abstract
In this study, the heat resistant Al-8Ce-xY (x = 0, 1, 2, and 3) alloys as designed and fabricated by gravity casting. The tensile strength of the alloys at room temperature increased with the Y addition from 117.5 to 142.7 MPa, and the tensile strength at 350 °C increased significantly from 40.4 to 57.2 MPa, which is an increase of > 40%. Even after heat exposure at 350 °C for 200 h, the alloys still retain the morphology of the eutectic colony and hardness stable. The outstanding performance is primarily attributed to excellent heat stability of eutectic lamellar Al11(Ce,Y)3 phase at 350 °C and its volume fraction increased from 10.45 to 19.15% with Y additions from 0 to 3%. The increasing volume fraction of the eutectic Al11(Ce,Y)3 phase effectively improves the tensile strength of the alloys at ambient and high temperatures. Our work provides a new ternary Al-Ce-Y system which is a marvellous candidate for castable heat resistant Al alloys.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (54)
Show source-provided references
1. Recent developments in advanced aircraft aluminium alloys10.1016/j.matdes.2013.12.002 ↗
2. Superior light metals by texture engineering: optimized aluminum and magnesium alloys for automotive applications10.1016/j.actamat.2012.10.044 ↗
3. Criteria for developing castable, creep-resistant aluminum-based alloys – a review10.1515/ijmr-2006-0042 ↗
4. Cerium-based, intermetallic-strengthened aluminum casting alloy: high-volume Co-product development10.1007/s11837-016-1943-9 ↗
5. Enhanced load transfer and ductility in Al–9Ce alloy through heterogeneous lamellar microstructure design by cold rolling and annealing10.1016/j.msea.2021.141591 ↗
6. Elevated temperature ductility dip in an additively manufactured Al-Cu-Ce alloy10.1016/j.actamat.2021.117285 ↗
7. Criteria for developing castable, creep-resistant aluminum-based alloys - a review10.3139/146.101249 ↗
8. Improved tensile strength of Al-5Ce alloy by permanent magnet stirring10.1007/s11661-020-05723-2 ↗
9. High performance aluminum-cerium alloys for high-temperature applications10.1039/C7MH00391A ↗
10. Effect of (0-40) wt. % Si addition to Al on the thermal conductivity and thermal expansion of diamond/Al composites by pressure infiltration10.1016/j.jallcom.2015.12.255 ↗
11. Thermal stability of aluminum-cerium binary alloys containing the Al-Al11Ce3 eutectic10.1016/j.msea.2021.140973 ↗
12. Castability and characteristics of high cerium aluminum alloys
13. Cerium in aluminum alloys10.1007/s10853-019-03892-z ↗
14. Solid solution strengthening mechanism in high pressure die casting Al–Ce–Mg alloys10.1016/j.msea.2021.141109 ↗
15. Heterogeneous phase transformation pathways in additively manufactured Al-Ce-Mn alloys10.1016/j.jallcom.2022.168490 ↗
16. The microstructure evolution of Al-5Ce alloy prepared by strain-induced melt activation during semi-solid isothermal treatment process10.1016/j.matlet.2022.132948 ↗
17. Aging- and creep-resistance of a cast hypoeutectic Al-6.9Ce-9.3Mg (wt.%) alloy10.1016/j.msea.2020.139398 ↗
18. Beneficial effects of Sc/Zr addition on hypereutectic Al–Ce alloys: modification of primary phases and precipitation hardening10.1016/j.msea.2022.142611 ↗
19. Comparing evolution of precipitates and strength upon aging of cast and laser-remelted Al-8Ce-0.2Sc-0.1Zr (wt.%)10.1016/j.msea.2022.142990 ↗
20. Microstructure and creep properties of cast near-eutectic Al–Ce–Ni alloys10.1016/j.msea.2021.142551 ↗
21. A creep-resistant additively manufactured Al-Ce-Ni-Mn alloy10.1016/j.actamat.2022.117699 ↗
22. Improving creep resistance of Al-12 wt.% Ce alloy by microalloying with Sc10.1016/j.scriptamat.2021.113838 ↗
23. Microstructure and properties of novel Al-Ce-Sc, Al-Ce-Y, Al-Ce-Zr and Al-Ce-Sc-Y alloy conductors processed by die casting, hot extrusion and cold drawing10.1016/j.jmst.2020.03.073 ↗
24. Strengthening mechanisms in Al-Ni-Sc alloys containing Al3Ni microfibers and Al3Sc nanoprecipitates10.1016/j.actamat.2018.10.059 ↗
25. Precipitation evolution in Al–0.1Sc, Al–0.1Zr and Al–0.1Sc–0.1Zr (at.%) alloys during isochronal aging10.1016/j.actamat.2010.05.054 ↗
26. The growth of quaternary divorced eutectic in Al–Ce–Si–Mg alloys10.1007/s11661-022-06911-y ↗
27. Aluminum cast alloys based on the Al–Ce–Si–Mg system: an influence of silicon on crystallization, phase composition, and tensile properties10.1007/s11661-022-06812-0 ↗
28. Modification of hypereutectic Al–20 wt%Si alloy based on the addition of yttrium and Al–5Ti–1B modifiers mixing melt10.1007/s40962-018-0242-3 ↗
29. Influence of additives on the microstructure and tensile properties of near-eutectic Al–10.8%Si cast alloy10.1016/j.matdes.2009.05.042 ↗
30. Refining mechanism of yttrium on primary alpha-Al in semi-solid Al alloy
31. Effects of yttrium and heat treatment on the microstructure and tensile properties of Al–7.5Si–0.5Mg alloy10.1016/j.matdes.2010.08.040 ↗
32. Effect of trace yttrium addition on the microstructure and tensile properties of recycled Al–7Si–0.3Mg–1.0Fe casting alloys10.1016/j.msea.2016.04.036 ↗
33. The microstructure and mechanical characterization of Al-30%Mg2Si composite with Y inoculation addition10.1088/2053-1591/aad033 ↗
34. The varied mechanisms of yttrium (Y) modifying a hypoeutectic Al–Si alloy under conditions of different cooling rates10.1016/j.jallcom.2019.07.107 ↗
35. Internal friction and heat resistance of Al, Al–Ce, Al–Ce–Zr and Al–Ce–(Sc)–(Y) aluminum alloys with high strength and high electrical conductivity10.1016/j.jmrt.2021.07.054 ↗
36. Microstructure and mechanical properties of high performance die cast Al-8Ce-3Y aluminum alloy containing Al4(Ce,Y) phase10.1016/j.matlet.2021.130742 ↗
37. The structure and strength of unidirectionally solidified commercial purity Al-Ni composites
38. Cast near-eutectic Al-12.5 wt.% Ce alloy with high coarsening and creep resistance10.1016/j.msea.2019.138440 ↗
39. Al-Ce (Aluminum-Cerium)10.1007/s11669-011-9914-x ↗
40. The isothermal section at 500 °C of the Al–La–Y ternary system10.1016/j.intermet.2003.11.006 ↗
41. Ostwald ripening in concentrated alloys10.1016/0956-7151(94)90293-3 ↗
42. Aluminum-Yttrium
43. Evaluation of an Al-Ce alloy for laser additive manufacturing10.1016/j.actamat.2016.12.065 ↗
44. Laser powder bed fusion of Al–10 wt% Ce alloys: microstructure and tensile property10.1007/s10853-020-05037-z ↗
45. Nanostructured aluminium alloys produced by severe plastic deformation: new horizons in development10.1016/j.msea.2012.09.020 ↗
46. Strengthening mechanisms in AL alloys - an overview of natural limits and engineering possibilities10.4028/www.scientific.net/MSF.217-222.57 ↗
47. On the Al-Al11Ce3 eutectic transformation in aluminum-cerium binary alloys10.3390/ma13204549 ↗
48. Mechanical properties and yield asymmetry of Mg-Y-Zn alloys: competitive behavior of second phases10.1016/j.matchar.2020.110301 ↗
49. The Hall–Petch relation in aluminium and its dependence on the grain boundary structure10.1080/01418618608242849 ↗
50. Effect of Mg addition on the creep and yield behavior of an Al–Sc alloy10.1016/S1359-6454(03)00288-X ↗
51. Precipitation strengthening at ambient and elevated temperatures of heat-treatable Al(Sc) alloys10.1016/S1359-6454(02)00201-X ↗
52. Strengthening mechanisms in particulate metal matrix composites10.1016/0956-716X(91)90349-6 ↗
53. An additively manufactured heat-resistant Al-Ce-Sc-Zr alloy: microstructure, mechanical properties and thermal stability10.1016/j.msea.2023.144965 ↗
54. Perspective on hetero-deformation induced (HDI) hardening and back stress10.1080/21663831.2019.1616331 ↗