Porosity and microstructure of L-PBF printed AlSi10Mg thin tubes in laser shock peening
Source abstract
Abstract
Laser powder bed fusion (L-PBF) has emerged as one of the most promising technologies for producing complex geometries that are difficult to achieve with other methods. However, its widespread adoption is hindered by issues such as deleterious microstructure, tensile residual stresses, and porous structure, mainly while working with aluminum alloys. To address these challenges, laser shock peening (LSP) offers a potential solution by mitigating the negative effects associated with aluminum L-PBF. This study investigates the impact of the important LSP parameters, namely energy, spot size, and overlap on L-PBF printed thin AlSi10Mg tubes. A total of 17 specimens were examined by varying the mentioned parameters at three levels each. The outcome of the study was evaluated in terms of residual stresses, porosity, microstructure and surface roughness. The results have shown significant improvements in residual stresses, where a maximum improvement of over 200 % was observed and a decrease in porosity by 70 %. Furthermore, the microstructure analysis revealed grain refinement and dislocation redistribution as material reactions, aligning with the observed microhardness increase. These findings demonstrate the viability of LSP as a post-processing method for demanding applications, effectively addressing the limitations of the L-PBF process.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Surface Treatment and Residual Stress · Additive Manufacturing Materials and Processes · Laser Material Processing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. How aluminum changed the world: a metallurgical revolution through technological and cultural perspectives10.1016/j.techfore.2019.03.011 ↗
2. Technology innovation in aluminum products10.1007/s11837-001-0115-7 ↗
3. Fatigue failures in low pressure die cast AlSi10Mg cylinder heads10.1179/136404608X370747 ↗
4. Influence on microstructure, strength and ductility of build platform temperature during laser powder bed fusion of AlSi10Mg10.1016/j.actamat.2020.10.001 ↗
5. Microstructure and mechanical properties of AlSi10Mg parts produced by the laser beam additive manufacturing (AM) technology10.1007/s13632-014-0168-y ↗
6. Surface integrity of SLM manufactured meso-size gears in laser shock peening without coating10.1016/j.jmapro.2022.12.011 ↗
7. Technology advancements for channel wall nozzle manufacturing in liquid rocket engines10.1016/j.actaastro.2020.04.067 ↗
8. Design and additive manufacturing of a fatigue-critical aerospace part using topology optimization and L-PBF process10.1016/j.promfg.2021.07.037 ↗
9. Titanium based bone implants production using laser powder bed fusion technology10.1016/j.jmrt.2022.01.087 ↗
10. Laser shock peening in tooling industry
11. Laser shock processing of aluminium alloys. Application to high cycle fatigue behaviour10.1016/0921-5093(95)10084-9 ↗
12. Performance of Gen IV LSP for Thick Section Airfoil Damage Tolerance
13. High cycle fatigue life improvement of superferritic stainless steel by laser shock peening without coating10.1016/j.optlastec.2022.108083 ↗
14. Laser peening without coating as a surface enhancement technology10.2961/jlmn.2006.03.0002 ↗
15. Pathak S, Böhm M, Kaufman J, Zulić S, Brajer J, Stránský; O, et al. Method for improving surface integrity of an additive manufactured mesoscopic gear, product thereof and device carrying out the method. Luxembourg LU502626.
16. Laser shock processing of aluminium alloys. Application to high cycle fatigue behaviour10.1016/0921-5093(95)10084-9 ↗
17. Influence of shot peening on AlSi10Mg parts fabricated by additive manufacturing
18. On the effects of laser shock peening on fatigue behavior of V-notched AlSi10Mg manufactured by laser powder bed fusion10.1016/j.ijfatigue.2022.107035 ↗
19. Pore closure effect of laser shock peening of additively manufactured AlSi10Mg10.1089/3dp.2019.0064 ↗
20. In-situ laser shock peening for improved surface quality and mechanical properties of laser-directed energy-deposited AlSi10Mg alloy
21. Microstructure, residual stress and tensile properties control of wire-arc additive manufactured 2319 aluminum alloy with laser shock peening10.1016/j.jallcom.2018.02.353 ↗
22. The effect of femto-second laser shock peening on the microstructures and surface roughness of AlSi10Mg samples produced with selective laser melting (SLM)10.1016/j.procir.2022.03.017 ↗
23. Individual and synergistic effects of thermal and mechanical surface post-treatments on wear and corrosion behavior of laser powder bed fusion AlSi10Mg10.1016/j.jmatprotec.2021.117479 ↗
24. Ultrasonic peening treatment used to improve stress corrosion resistance of AlSi10Mg components fabricated using selective laser melting10.3390/met9010103 ↗
25. Effects of different mechanical and chemical surface post-treatments on mechanical and surface properties of as-built laser powder bed fusion AlSi10Mg10.1016/j.surfcoat.2022.128391 ↗
26. L. Hackel, J. Halpin, F. Harris. Laser peening of components of thin cross-section. US Patent: US 2002/0096503 A1. 1-13. https://patents.google.com/patent/US20020096503A1/en.