journal article·2023-07Open access

The high temperature oxidation behavior of a superalloy prepared by vacuum induction melting and electron beam smelting: A comparative study

Yijiala Yiliti, Gengyi Dong, Xiaoying Liu, Xiaogang You, Wenjun Han, Liyang Dong, Yiquan Zhao, Li yi, Yinong Wang

Abstract

In this paper, the high temperature oxidation behavior of superalloys prepared by the electron beam smelting (EBS) and vacuum induction melting (VIM) at 900°C and 1000°C is investigated. Experimental results indicate that EBS alloys show better oxidation resistance and oxide layer integrity. The relationship between the growth rates of Al2O3 and Ta2O5 and the oxygen partial pressure at the oxide/substrate interface is explained by the growth model of n-type semiconductor oxides. Lower oxygen partial pressure at the oxide/substrate interface due to the higher purity of the EBS alloys. This effectively slows down the growth rate of the n-type semiconductor oxides such as Al2O3 and Ta2O5 and thickening rates of the other n-type oxides, which ultimately leads to better oxidation resistance.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · High Temperature Alloys and Creep · Metallurgical Processes and Thermodynamics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. Effects of vacuum on gas content, oxide inclusions and mechanical properties of Ni-based superalloy using electron beam button and synchrotron diffraction10.1016/j.matdes.2021.109861 ↗
2. Effect of small amounts of nitrogen and silicon on microstructure and properties of MAR-M002 nickel-base superalloy10.1179/030716984803274251 ↗
3. Effect of minor alloying additions on the carbide morphology in a single crystal Ni-base superalloy10.1016/j.scriptamat.2007.09.050 ↗
4. Crystal plasticity assessment of inclusion- and matrix-driven competing failure modes in a nickel-base superalloy10.1016/j.actamat.2019.07.024 ↗
5. Short crack propagation from cracked non-metallic inclusions in a Ni-based polycrystalline superalloy10.1016/j.actamat.2018.11.051 ↗
6. Effect of vacuum level on the interfacial reactions between K417 superalloy and Y2O3 crucibles
7. Kinetics study of nitrogen removal from liquid IN718 alloy during vacuum induction melting
8. Removal of inclusions from nickel-based superalloy by induced directional solidification during electron beam smelting10.1016/j.vacuum.2018.07.014 ↗
9. Fabrication of a turbine disk alloy by electron beam sheet lamination and investigation on the improved high temperature creep performance10.1016/j.jmst.2022.10.013 ↗
10. Fatigue deformation behavior of revert Ni-based superalloys via electron beam technology at low and middle temperature
11. Preparation of Inconel 740 superalloy by electron beam smelting10.1016/j.jallcom.2016.03.140 ↗
12. Breakaway oxidation of austenitic stainless steels induced by alloyed sulphur10.1016/j.corsci.2015.01.007 ↗
13. High-temperature performance of (Ni,Pt)Al coatings on second-generation Ni-base single-crystal superalloy at 1100 degrees C: effect of excess S impurities10.1016/j.corsci.2019.108115 ↗
14. Effect of sulfur on the cyclic oxidation behavior of a single crystalline, nickel-base superalloy10.1016/0921-5093(95)09819-4 ↗
15. Oxidation behavior of a single-crystal Ni-based superalloy over the temperature range of 850 degrees C-950 degrees C in air10.1016/j.apsusc.2019.04.089 ↗
16. Multiferroic nanoparticles of Ni doped CoCr2O4: an XPS study10.1116/1.5127349 ↗
17. High-throughput determination of interdiffusivity matrices in Ni-Al-Ti-Cr-Co-Mo-Ta-W multicomponent superalloys and their application in optimization of creep resistance
18. The influence of CrTaO4 layer on the oxidation behavior of a directionally-solidified nickel-based superalloy at 850-900 degrees C10.1016/j.jallcom.2017.07.066 ↗
19. High Temperature Oxidation Resistance of Ni-(5 similar to 13)Co-(10 similar to 16)Cr-(5 similar to 9)W-5Al-(1 similar to 1.5)Ti-(3 similar to 6)Ta Alloys10.1007/s12540-016-6305-1 ↗
20. High temperature oxidation behavior of electron beam smelted K417 superalloy
21. Film evolution and growth mechanism of a Ni-based superalloy in the two models at the different temperatures
22. Microstructural evolution of oxidation film on a single crystal nickel-based superalloy at 980 A degrees C10.1007/s11085-017-9787-4 ↗
23. Oxidation of single crystal PWA 1483 at 950 degrees C in flowing air10.1016/j.corsci.2008.06.033 ↗
24. Oxidation behavior in static air and its effect on tensile properties of a powder metallurgy EP962NP nickel-based superalloy
25. Effect of trace impurity elements on the high-temperature oxidation resistance of a high-purity nickel-based superalloy
26. Mechanism of the transition from external oxide scales to internal oxidation for Fe-Si alloys in the atmosphere with very low oxygen partial pressure10.1088/2053-1591/ab105a ↗
27. Birks · 1983
28. Sieverts law pressure exponent for hydrogen permeation through Pd-based membranes: coupled influence of non-ideal diffusion and multicomponent external mass transfer
29. High temperature oxidation behavior of electron beam refined Inconel 718 alloy
30. Research on the high temperature oxidation mechanism of Cr3C2-NiCrCoMo coating for surface remanufacturing10.1016/j.jmrt.2020.12.049 ↗
31. Evolution in microstructure and high-temperature oxidation behaviors of the laser-cladding coatings with the Si addition contents10.1016/j.jallcom.2020.154131 ↗