Anisotropic microstructure, nanomechanical and corrosion behavior of direct energy deposited Ti–13Nb–13Zr biomedical alloy
Source abstract
Abstract
The present study investigates the anisotropic microstructure, nanomechanical and corrosion behavior of Ti-13Nb-13Zr biomedical alloys, which were fabricated using the direct energy deposition method. The microstructure of the as-deposited material was studied using a field-emission scanning electron microscope (SEM), electron backscatter diffraction (EBSD) and X-ray diffraction (XRD). We found anisotropic mechanical behavior using nanoindentation from strain rate sensitivity and creep tests. For the maximum load of 50 mN, the x-y plane (normal to the building direction) shows better indentation hardness and lower strain rate sensitivity value (0.014) compared to the x-z plane (0.022) (parallel to the building direction). The difference in the indentation hardness was mainly attributed to the smaller equiaxed prior beta grains and finer α’ martensitic laths on the x-y plane. In terms of creep behavior, the x-y planes show better creep strength than the x-z plane. Meanwhile, both planes show a very high creep exponent, which signifies a similar creep mechanism, i.e., dislocation based. Moreover, we further found the anisotropic corrosion behavior using electrochemical tests. Corrosion results reveal that the x-y plane is more corrosion-resistant than the x-z plane. In summary, the x-y plane of the direct energy deposited Ti-13Nb-13Zr alloy possesses better strength and corrosion resistance due to its finer microstructure.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Additive Manufacturing Materials and Processes · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (55)
Show source-provided references
1. Bone bonding bioactivity of Ti metal and Ti-Zr-Nb-Ta alloys with Ca ions incorporated on their surfaces by simple chemical and heat treatments10.1016/j.actbio.2010.09.026 ↗
2. Mechanical and corrosion resistance of a new nanostructured Ti-Zr-Ta-Nb alloy10.1016/j.jmbbm.2011.05.012 ↗
3. Bone response to a novel Ti-Ta-Nb-Zr alloy10.1016/j.actbio.2015.03.038 ↗
4. Influence of oxygen content on microstructure and mechanical properties of Ti-Nb-Ta-Zr alloy10.1016/j.matdes.2010.11.049 ↗
5. Manufacture by selective laser melting and mechanical behavior of a biomedical Ti-24Nb-4Zr-8Sn alloy10.1016/j.scriptamat.2011.03.024 ↗
6. Titanium alloy mini-implants for orthodontic anchorage: immediate loading and metal ion release10.1016/j.actbio.2006.10.010 ↗
7. Reduced toxicity and superior cellular response of preosteoblasts to Ti-6Al-7Nb alloy and comparison with Ti-6Al-4V10.1002/jbm.a.34492 ↗
8. Multi-scale mapping for collagen-regulated mineralization in bone remodeling of additive manufacturing porous implants10.1016/j.matchemphys.2019.03.047 ↗
9. Theory-guided bottom-up design of β-titanium alloys as biomaterials based on first principles calculations: theory and experiments10.1016/j.actamat.2007.04.024 ↗
10. Effect of Zr content on phase stability, deformation behavior, and young's modulus in Ti–Nb–Zr alloys10.3390/ma13020476 ↗
11. Corrosion behavior of Ti-13Nb-13Zr alloy used as a biomaterial10.1016/j.jallcom.2008.09.026 ↗
12. Microstructure tailoring to enhance strength and ductility in Ti-13Nb-13Zr for biomedical applications10.1016/j.scriptamat.2013.08.028 ↗
13. Effect of thermomechanical processing on microstructure characteristics of a Ti-13Nb-13Zr alloy10.1016/S0925-8388(01)01604-8 ↗
14. Phase decomposition in a Ti-13Nb-13Zr alloy during aging at 600°C10.2320/matertrans.43.2956 ↗
15. An overview of Direct Laser Deposition for additive manufacturing; Part II: mechanical behavior, process parameter optimization and control
16. Microstructure and mechanical properties of selective laser melted biomaterial Ti-13Nb-13Zr compared to hot-forging10.1016/j.msea.2018.04.001 ↗
17. Study of mechanical properties of AISI 316 stainless steel processed by “selective laser melting”, following different manufacturing strategies10.1007/s00170-010-2631-5 ↗
18. Anisotropic tensile behavior of Ti-6Al-4V components fabricated with directed energy deposition additive manufacturing10.1016/j.actamat.2014.12.054 ↗
19. Anisotropic response of Ti-6Al-4V alloy fabricated by 3D printing selective laser melting10.1016/j.msea.2016.11.061 ↗
20. Deformations of Ti-6Al-4V additive-manufacturing-induced isotropic and anisotropic columnar structures: insitu measurements and underlying mechanisms
21. Indentation strain rate sensitivity of laser-powder bed fused and electron beam melted Ti–6Al–4V10.1016/j.vacuum.2021.110690 ↗
22. 2014
23. In situ elaboration of a binary Ti-26Nb alloy by selective laser melting of elemental titanium and niobium mixed powders10.1016/j.msec.2016.02.033 ↗
24. Martensite formation and decomposition during traditional and am processing of two-phase titanium alloys—an overview10.3390/met11030481 ↗
25. Laser additive manufacturing of metallic components: materials, processes and mechanisms10.1179/1743280411Y.0000000014 ↗
26. Gibson · 2021
27. Lutjering · 2007
28. Additive manufacturing of Ti6Al4V alloy: a review10.1016/j.matdes.2018.107552 ↗
29. Development of strength-hardness relationships in additively manufactured titanium alloys10.1016/j.msea.2017.03.102 ↗
30. The effect of alpha platelet thickness on plastic flow during hot working of Ti-6Al-4V with a transformed microstructure10.1016/S1359-6454(01)00236-1 ↗
31. Multi-cycling instrumented nanoindentation of a Ti-23Nb-0.7Ta-2Zr-1.2O alloy in annealed condition10.1016/j.msea.2017.05.004 ↗
32. Size dependence of mechanical properties of gold at the micron scale in the absence of strain gradients10.1016/j.actamat.2004.12.031 ↗
33. Geometrically necessary dislocation and size-dependent plasticity10.1016/S1359-6462(02)00329-9 ↗
34. Indentation size effects in crystalline materials: a law for strain gradient plasticity10.1016/S0022-5096(97)00086-0 ↗
35. Slip transfer across phase boundaries in dual phase titanium alloys and the effect on strain rate sensitivity10.1016/j.ijplas.2018.01.011 ↗
36. Effect of nanocrystalline and ultrafine grain sizes on the strain rate sensitivity and activation volume: Fcc versus bcc metals10.1016/j.msea.2004.03.064 ↗
37. Strain rate dependency of dislocation plasticity
38. Nano-mechanical properties and creep behavior of ti6al4v fabricated by powder bed fusion electron beam additive manufacturing10.3390/ma14113004 ↗
39. A nanoindentation investigation of local strain rate sensitivity in dual-phase Ti alloys10.1016/j.jallcom.2016.02.146 ↗
40. Indentation creep revisited10.1557/jmr.2011.213 ↗
41. Size effects of nanoindentation creep10.1557/jmr.2004.19.2.513 ↗
42. An examination of the breakdown in creep by viscous glide in solid solution alloys at high stress levels10.1016/0001-6160(82)90139-0 ↗
43. Spherical nanoindentation creep behavior of nanocrystalline and coarse-grained CoCrFeMnNi high-entropy alloys10.1016/j.actamat.2016.02.049 ↗
44. Microstructure and nanoindentation creep behavior of CoCrFeMnNi high-entropy alloy fabricated by selective laser melting
45. Depth-sensing time-dependent response of additively manufactured Ti-6Al-4V alloy
46. Cyclic voltammetry10.1021/ed060p702 ↗
47. Pujado · 2012
48. The anisotropic corrosion behaviour of wire arc additive manufactured Ti-6Al-4V alloy in 3.5% NaCl solution10.1016/j.corsci.2018.03.047 ↗
49. Oxidation behavior of Ca-based bulk amorphous materials10.2320/matertrans.MJ200744 ↗
50. Tan · 2012
51. Corrosion behavior of selective laser melted Ti-6Al-4 V alloy in NaCl solution10.1016/j.corsci.2015.10.041 ↗
52. Comparative effect of grain size and texture on the corrosion behaviour of commercially pure titanium processed by equal channel angular pressing10.1016/j.corsci.2009.08.017 ↗
53. Corrosion resistance of ultra fine-grained Ti10.1016/j.scriptamat.2004.04.011 ↗
54. Distinction in corrosion resistance of selective laser melted Ti-6Al-4V alloy on different planes10.1016/j.corsci.2016.06.009 ↗
55. A comparison of corrosion, tribocorrosion and electrochemical impedance properties of pure Ti and Ti6Al4V alloy treated by micro-arc oxidation process10.1016/j.apsusc.2014.11.030 ↗