journal article·2024-05Open access

The evolution process and internal corrosion mechanisms of hot salt corrosion on TC11 titanium alloy

Mengyao Li, Daoxin Liu, Jing Yang, Xingchen Xu, Kaifa Fan, Xiaohua Zhang

Abstract

This study investigates the evolution process of hot corrosion in bi-phase Ti-6.5Al-1.5Zr-3.5Mo-0.3Si (TC11) titanium alloy induced by sodium chloride (NaCl). Through morphological progression and elemental distribution analyses, the integrated processes involved in the onset of internal corrosion during hot corrosion are elucidated, revealing intriguing phenomena that deviate from conventional mechanisms. The development of corrosion can be divided into three stages: First there is the rapid growth of the external corrosion layer induced by Cl; then a Cl and O induced internal corrosion is initiated when the external corrosion layer reaches a critical thickness, at the same time the external corrosion decreases; finally, the chlorine pressure is too low to act as the corrosion depth increases, O becomes a major contributor to deep internal corrosion, leading to O induced internal corrosion. Significant interphase selective corrosion was observed in this internal corrosion zone: the β phase was corroded while the α phase remained uncorroded, challenging the prevailing notion that the β phase is more corrosion-resistant in titanium alloys. This distinctive phenomenon results from the differences in oxygen solubility, element diffusion rates and the reactivity between the α and β phases.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Young · 2008
2. A review on molten sulfate salts induced hot corrosion10.1016/j.jmst.2021.03.013 ↗
3. Corrosion behavior of GH3535 alloy in molten LiF-BeF2 salt10.1016/j.corsci.2022.110168 ↗
4. Electrochemical study on the hot corrosion behavior of Ni16Cr13Co4Mo alloy in molten NaCl-KCl and NaCl-KCl-Na2SO410.1016/j.corsci.2022.110247 ↗
5. Achieving superior hot corrosion resistance by PVD/HVOF duplex design10.1016/j.corsci.2020.108845 ↗
6. Investigation of the mechanisms of Type-II hot corrosion of superalloy CMSX-410.1016/j.corsci.2013.11.048 ↗
7. Hot corrosion behavior of Co modified NiAl coating on nickel base superalloys10.1016/j.corsci.2012.06.027 ↗
8. Alloying effects in high temperature molten salt corrosion10.1016/j.corsci.2021.110003 ↗
9. Behaviour and mechanisms of alkali-sulphate-induced hot corrosion on composite coatings at 900°C10.1016/j.corsci.2012.01.034 ↗
10. Hot corrosion-creep interaction in IN718 under simulated marine environment: introducing strain-associated-time (SAT) plots for comprehensive understanding10.1016/j.corsci.2021.109667 ↗
11. Atypical decomposition processes of Sm2Zr2O7 + 8YSZ dual-phase TBCs during hot corrosion10.1016/j.corsci.2020.108681 ↗
12. High temperature oxidation and hot corrosion behaviors of Ti2AlNb alloy at 923 K and 1023 K10.1016/j.corsci.2021.109336 ↗
13. Corrosion behavior of the resistance sintered TiAl based intermetallics induced by two different molten salt mixture10.1016/j.corsci.2020.108819 ↗
14. Hot corrosion behaviour of Ti-6Al-4V modified by ultrasonic shot peening10.1016/j.matdes.2016.07.133 ↗
15. Effect of surface roughness on corrosion behavior of the superalloy IN718 in simulated marine environment10.1016/j.jallcom.2018.01.042 ↗
16. Effects of laser shock peening on the hot corrosion behaviour of the selective laser melted Ti6Al4V titanium alloy10.1016/j.corsci.2021.109558 ↗
17. Effect of microstructure evolution and phase precipitations on hot corrosion behavior of IN718 alloy subjected to multiple laser shock peening10.1016/j.surfcoat.2019.04.060 ↗
18. Hot corrosion behavior of TC11 titanium alloy treated by laser shock processing10.1016/j.apsusc.2013.07.017 ↗
19. The hot corrosion of 310 stainless steel with pre-coated NaCl/Na2SO4 mixtures at 750°C10.1016/j.matchemphys.2004.10.002 ↗
20. Gray · 1969 · vol. 20546
21. The mechanisms of hot salt stress corrosion cracking in titanium alloy Ti-6Al-2Sn-4Zr-6Mo10.1016/j.corsci.2018.02.025 ↗
22. The stress-corrosion cracking susceptibility of near-α titanium alloy IMI 834 in presence of hot salt10.1016/j.corsci.2014.01.013 ↗
23. A cracking oxygen story: a new view of stress corrosion cracking in titanium alloys10.1016/j.actamat.2022.117687 ↗
24. 2003
25. NaCl induced corrosion of Ti-6Al-4V alloy at high temperature10.1016/j.corsci.2016.04.016 ↗
26. Corrosion behavior of Ti60 alloy under continuous NaCl solution spraying at 600°C10.1016/j.jmst.2022.01.032 ↗
27. Effect of streaming water vapor on the corrosion behavior of Ti60 alloy under a solid NaCl deposit in water vapor at 600°C10.1016/j.corsci.2019.108177 ↗
28. Effect of Zr, Ti, Ta and Mo addition on high-temperature oxidation and hot corrosion behavior of NiAlY alloys10.1016/j.jallcom.2022.164614 ↗
29. Hot corrosion behaviour of (γ+α2)-Ti-46Al-8Nb (at.%) and α-Ti-6Al-1Mn (at.%) alloys10.1016/j.corsci.2016.11.006 ↗
30. Inter-phase selective corrosion of γ-TiAl alloy in molten salt environment at high temperature10.1016/S1002-0071(12)60064-1 ↗
31. Effect of microstructure characteristic on mechanical properties and corrosion behavior of new high strength Ti-1300 beta titanium alloy10.1016/j.jallcom.2017.08.239 ↗
32. Tuning microstructure and enhancing corrosion property of Ti-6Al-3Nb-2Zr-1Mo alloy through electron beam surface melting10.1016/j.corsci.2022.110520 ↗
33. Degradation mechanism of Ti-6Al-2Sn-4Zr-2Mo-Si alloy exposed to solid NaCl deposit at high temperature10.1016/j.corsci.2020.108611 ↗
34. Hot tensile characterization of Ti-6.5Al-3.5Mo-1.5Zr-0.3Si alloy with an equiaxed microstructure10.1016/j.matdes.2008.05.077 ↗
35. Mechanical behaviors and microstructural characteristics of TC11 alloy during hot deformation
36. Study of titanium alloy Ti6242S oxidation behaviour in air at 560°C: effect of oxygen dissolution on lattice parameters10.1016/j.corsci.2019.06.004 ↗
37. Corrosion behavior of pure Ti under a solid NaCl deposit in a wet oxygen flow at 600°C10.3390/met6040072 ↗
38. NaCl-induced hot corrosion of a titanium aluminide alloy10.1016/0921-5093(95)03345-9 ↗
39. A comparative study of the oxidation with water vapor of pure titanium and of Ti-6Al-4V10.1007/BF00614241 ↗
40. Diffusion in the Ti-Al system10.1016/S1359-6454(99)00400-0 ↗
41. 1995 · I
42. Brookite, a sometimes under evaluated TiO2 polymorph10.1039/D1RA09057G ↗
43. Non-classical growth of brookite nanorods10.1039/C9CE00682F ↗
44. Controlled synthesis of brookite and combined brookite with rutile phases of titanium di-oxide and its characterization studies10.1016/j.ceramint.2016.11.037 ↗
45. Effect of NaCl-rich environment on internal corrosion for Ti60 alloy at 600°C10.1016/j.corsci.2023.111307 ↗
46. Thermal oxidation behaviour of bulk titanium with nanocrystalline surface layer10.1016/j.corsci.2012.03.005 ↗
47. High-temperature oxidation of titanium10.1016/0022-5088(67)90017-3 ↗
48. Effective work functions of the elements10.1016/j.progsurf.2020.100583 ↗
49. Influence of surface morphology on corrosion and electronic behavior10.1016/j.actamat.2005.09.017 ↗
50. Atomic and electronic basis for the serrations of refractory high-entropy alloys10.1038/s41524-017-0024-0 ↗
51. Migration enthalpies in FCC and BCC metals10.1088/0953-8984/4/47/013 ↗