Corrosion behavior of steel exposed to "zero" pollution atmosphere environment for 20 years
Source abstract
Abstract
In this study, the corrosion behavior of Q235 carbon steel, 09CuPTiRE weathering steel and X60 pipeline steel after 20 years exposure in "zero" pollution atmosphere environment was investigated by corrosion rate analysis, macroscopic observation, scanning electron microscopy, X-ray diffraction, white light interferometers and electrochemical analysis were conducted to analyze. The results showed that the corrosion rate of the three kinds of steels increases first and then decreases with time, and the results indicated that the empirical formula D=Atn was suitable for corrosion kinetics of three materials, and the three kinds of steels all form a relatively dense rust layer, which can effectively protect the metal matrix, inhibit the corrosion process and reduce the rate of corrosion. Under the same exposure time and the same corrosion conditions, the corrosion degree of the three materials is: X60 pipeline steel > Q235 Carbon steel >09CuPTiRE Weathering steel, three kinds of steel corrosion products are the same, only α-FeOOH and γ-FeOOH exist in the rust layer, and the relative content of α-FeOOH is more than γ-FeOOH of each steel in both skyward side and fieldward sides. X60 Pipeline steel has the worst corrosion resistance, and 09CuPTiRE weathering steel has the best corrosion resistance, so 09CuPTiRE weathering steel has better adaptability to this environment.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Concrete Corrosion and Durability · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. A survey of the atmospheric corrosiveness of natural environments in China
2. Mossbauer spectroscopic study of rust formed on a weathering steel and a mild steel exposed for a long term in an industrial environment10.2320/matertrans.43.694 ↗
3. In-depth distribution of rusts on a plain carbon steel and weathering steels exposed to coastal-industrial atmosphere for 17 years10.1016/S0010-938X(03)00070-2 ↗
4. Atmospheric corrosion of carbon steel and weathering steel in three environments
5. Eight-year atmospheric corrosion exposure of steels in China10.5006/1.3283967 ↗
6. Atmospheric corrosion of different steels in marine, rural and industrial environments10.1016/S0010-938X(99)00005-0 ↗
7. Leiro · 20102010
8. Clarifying the effect of a small amount of Cr content on the corrosion of Ni-Mo steel in tropical marine atmospheric environment
9. Atmospheric corrosion of carbon steels in tropical and subtropical climates in Southern China
10. Atmospheric corrosion of carbon steel in Colombia10.1016/j.corsci.2009.09.006 ↗
11. Research progress of atmospheric corrosion of steels in natural environment
12. Wang · 2009
13. Development and production practice of atmospheric corrosion resisting steel 09CuPCrNi-A for railway rolling stock
14. Atmospheric corrosion of several metallic materials in CHANGBAISHAN and shenyang area
15. Study of corrosion evolution of carbon steel exposed to an industrial atmosphere10.1080/1478422X.2019.1574955 ↗
16. Initial corrosion behavior of carbon steel Q235, pipeline steel L415, and pressure vessel steel 16MnNi under high humidity and high irradiation coastal-industrial atmosphere in Zhanjiang
17. Initial corrosion behavior of carbon steel and weathering steel in Nansha marine atmosphere
18. Long term atmospheric corrosion in Mauritius10.1179/1743278214Y.0000000240 ↗
19. Yin · 2019
20. Corrosion behavior of weathering steel in marine atmosphere10.1016/S0254-0584(02)00110-4 ↗
21. Long-term atmospheric corrosion of mild steel
22. Atmospheric corrosion behavior of 30CrMnSiA high-strength steel in rural, industrial and marine atmosphere environments10.1080/1478422X.2016.1254447 ↗
23. Li · 2022
24. An attempt to classify the morphologies presented by different rust phases formed during the exposure of carbon steel to marine atmospheres
25. SEM/Micro-Raman characterization of the morphologies of marine atmospheric corrosion products formed on mild steel10.1149/2.0411608jes ↗
26. Characterisation of rust surfaces formed on mild steel exposed to marine atmospheres using XRD and SEM/Micro-Raman techniques10.1016/j.corsci.2016.04.034 ↗
27. Mechanical properties of weathering steel and the role of copper, phosphorus and rare earth elements in steel
28. Research progress of function of rare earths in steel
29. Effects of rare earth elements on corrosion behaviors of low-carbon steels and weathering steels10.1002/maco.201911150 ↗
30. Corrosion and pitting behavior of pure aluminum 1060 exposed to Nansha Islands tropical marine atmosphere10.1016/S1003-6326(22)65806-0 ↗
31. Influence of Cl- and SO2 on carbon steel Q235, pipeline steel L415 and pressure vessel steel 16MnNi corrosion behavior in industrial and marine atmosphere environment10.20964/2021.12.06 ↗
32. Song · 2020
33. Mechanism of atmospheric rusting10.1016/S0010-938X(72)90671-3 ↗
34. Pei · 2021