journal article·2024-05Open access

Modification of microstructure and mechanical properties in H13 steel by introducing oxide particles using vacuum casting

Zhixia Xiao, Honglve Yang, Rui Xu, Baoxi Liu, Jianhang Feng, Puguang Ji, Jia Liang, Guoxin Liang

Abstract

Oxide particles with suitable size can refine the microstructure and improve the strength and toughness of steel. In this study, the particles containing Al2O3 were successfully introduced into H13 steel by vacuum casting. The micro-sized Al2O3-containg particles were randomly distributed in the dendritic structure and their number was increased by almost a factor of one. The secondary dendritic arm spacing of the ingot was decreased, which might be attributed to the heterogeneous nucleation of these oxides during solidification. Meanwhile, the alloying element segregation of the ingot was also alleviated. The micro-sized primary carbides were refined as the oxide particles were introduced to H13 steel, especially for V-rich carbides. After hot rolling and heat treatment, the size of austenitic grain was reduced by up to 75% (7.2 ± 1.8 μm), which was due to the particle stimulated nucleation and Zener pinning of micro- and nanoscale oxides in the oxide-added steel. The mechanical properties were obviously modified with the ultimate tensile strength of 1835 MPa, yield strength of 1479 MPa, tensile elongation of 13.4% and impact toughness of 24 J/cm2 after the introduction of oxide particles. It is expected that the introduction of oxide particles by vacuum casting can be applied widely in other die steel for superior performance.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metallurgical Processes and Thermodynamics · Metal Alloys Wear and Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. An evaluation of H13 tool steel deformation in hot forging conditions10.1016/j.jmatprotec.2017.03.026 ↗
2. Fatigue-creep interaction based on continuum damage mechanics for AISI H13 hot work tool steel at elevated temperatures10.1007/s42243-018-0073-8 ↗
3. Modeling creep-fatigue interaction damage and H13 tool steel material response for rolling die under hot milling
4. Thermal fatigue behavior of new type high-Cr cast hot work die steel
5. Effect of Y-Ce complex modification on thermal fatigue behavior of high Cr cast hot working die steels10.2355/isijinternational.44.1762 ↗
6. Effect of primary carbide on fatigue life in die steel for cold working10.2355/tetsutohagane1955.84.1_79 ↗
7. Fractography survey on high cycle fatigue failure: crack origin characterisation and correlations between mechanical tests and microstructure in Fe-C-Cr-Mo-X alloys10.1016/j.ijfatigue.2006.06.012 ↗
8. Effect of cooling rate on the solidification microstructure and characteristics of primary carbides in H13 steel10.2355/isijinternational.ISIJINT-2018-524 ↗
9. Effects of rare earth on the microstructure and impact toughness of H13 steel10.3390/met5010383 ↗
10. Effect of cerium on the behavior of inclusions in H13 steel, Steel Res
11. Carbides evolution and tensile property of 4Cr5MoSiV1 die steel with rare earth addition10.3390/met7100436 ↗
12. Cerium addition effect on modification of inclusions, primary carbides and microstructure refinement of H13 die steel10.2355/isijinternational.ISIJINT-2020-739 ↗
13. Microstructure and obdurability improvement mechanisms of the La-microalloyed H13 steel, Steel Res
14. Effect of Mg addition on carbides in H13 steel during electroslag remelting process10.1051/metal/2018071 ↗
15. Evolution of Al2O3 inclusions by magnesium treatment in H13 hot work die steel10.1080/03019233.2016.1165498 ↗
16. Effect of trace magnesium on carbide improvement in H13 steel10.1179/1879139515Y.0000000030 ↗
17. Cerium addition effect on modification of inclusions, primary carbides and microstructure refinement of H13 die steel10.2355/isijinternational.ISIJINT-2020-739 ↗
18. Microstructure control of steels through dispersoid metallurgy using novel grain refining alloys10.2355/isijinternational.46.824 ↗
19. Effects of MgO nanoparticle additions on the structure and mechanical properties of continuously cast steel billets10.1007/s11661-015-3237-1 ↗
20. Inclusion characteristics and microstructure properties under different cooling conditions in steel with nanoparticles addition10.1080/03019233.2017.1308128 ↗
21. Wang · 2012
22. Effect of TiN nano-particles addition on micro-structure and mechanical properties of 55SiMnMo steel
23. Tian · 2018
24. Microstructures and mechanical properties of the 5Cr13 martensite stainless steel refined by oxide particles10.1002/srin.202100086 ↗
25. Microstructures and mechanical properties of alumina and/or yttrium oxides strengthened 9Cr steel fabricated by vacuum casting10.1002/srin.202200711 ↗
26. Effect of melting rate of electroslag rapid remelting on the microstructure and carbides in a hot work tool steel10.1007/s12540-020-00717-6 ↗
27. Effect of titanium and rare earth microalloying on microsegregation, eutectic carbides of M2 high speed steel during ESR process10.1016/j.jre.2019.09.009 ↗
28. Heat-transfer and solidification model of continuous slab casting: CON1D10.1007/s11663-003-0040-y ↗
29. The effect of carbide and nitride additions on the heterogeneous nucleation behavior of liquid iron10.1007/BF02642799 ↗
30. Effect of complex inclusion particles on the solidification structure of Fe-Ni-Mn-Mo alloy10.1007/s11663-012-9734-3 ↗
31. Effect of a catalyst on heterogeneous nucleation in pure and Fe-Ni alloys10.1007/s11663-003-0022-0 ↗
32. Calculation of phase equilibria between austenite and (Nb, Ti, V)(C, N) in microalloyed steels10.2355/isijinternational.41.175 ↗
33. Yu · 2021 · vol. 3 · 307
34. The double-edge effect of second-phase particles on the recrystallization behaviour and associated mechanical properties of metallic materials10.1016/j.pmatsci.2017.10.004 ↗
35. A unified theory of recovery, recrystallization and grain growth, based on the stability and growth of cellular microstructures—II. The effect of second-phase particles10.1016/S1359-6454(97)00173-0 ↗
36. The morphology and crystallography of lath martensite in alloy steels10.1016/j.actamat.2006.07.009 ↗
37. The morphology and crystallography of lath martensite in Fe-C alloys10.1016/S1359-6454(02)00577-3 ↗
38. Effect of austenite grain size on the morphology and crystallography of lath martensite in low carbon steels10.2355/isijinternational.45.91 ↗
39. Effect of Nb on segregation, primary carbides and toughness of H13 steel
40. Effect of substructure on mechanical properties and fracture behavior of lath martensite in 0.1 C-1.1 Si-1.7 Mn steel10.1016/j.jallcom.2016.03.100 ↗
41. Effect of quenching temperature on martensite multi-level microstructures and properties of strength and toughness in 20CrNi2Mo steel10.1016/j.msea.2016.08.065 ↗
42. Effect of block size on the strength of lath martensite in low carbon steels10.1016/j.msea.2005.12.048 ↗
43. Effect of concentrations of Ta and Ti on microstructure and mechanical properties of 9Cr-1W reduced activation ferritic/martensitic steel10.1016/j.fusengdes.2019.111364 ↗
44. Yu · 2021 · vol. 1 · 362
45. Analysis of size distributions of primary oxide inclusions in Fe-10 mass pct Ni-M (M= Si, Ti, Al, Zr, and Ce) alloy10.1007/s11663-999-0055-0 ↗
46. Yong · 2006 · 210