journal article·2024-05Open access

Molten salt corrosion behavior of laser remelted PS-PVD YSZ thermal barrier coatings

Qijie Zhou, Jiao Wen, Yuqi Li, Jianmin Han, Bangyang Zhou, Hongbo Guo, Jiebo Li, Jian He

Abstract

Molten salt from the service environment leaches Y2O3 from yttria-stabilized zirconia (YSZ), threatening the security of thermal barrier coatings (TBCs). In this study, we compared the molten salt corrosion resistances of YSZ coatings prepared via plasma-spraying physical vapor deposition (PS-PVD) before and after laser remelting. At 1000 °C, the molten salt reacted with YSZ particulates in the PS-PVD YSZ coating and infiltrated the gaps between quasi-columnar crystals, resulting in phase transition of the coating and column breakage. A dense glazed layer was formed on the YSZ coating surface after remelting by the low-energy-density laser, which prohibited the penetration of molten salt and improved the hot corrosion resistance of the YSZ coating. By contrast, the failure of the high-energy-density laser-treated YSZ coating was accelerated due to the significant interfacial stress from the thick glazed layer and volume expansion caused by the corrosion products. Our investigation revealed the structural evolution of the PS-PVD YSZ coating under hot corrosion conditions and emphasizes the role of laser remelting. It can thus serve as a guideline for TBC modification.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Nuclear materials and radiation effects

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. Ceramic materials for thermal barrier coatings10.1016/S0955-2219(03)00129-8 ↗
2. Thermal barrier coatings for gas-turbine engine applications10.1126/science.1068609 ↗
3. Delamination resistance of thermal barrier coatings containing embedded ductile layers10.1016/j.actamat.2011.12.039 ↗
4. Novel thermal barrier coatings repel and resist molten silicate deposits10.1016/j.scriptamat.2018.12.028 ↗
5. Application of biofuel impurities and effect on the hot corrosion of yttria-stabilized zirconia thermal barrier coatings10.1016/j.surfcoat.2018.10.019 ↗
6. Advanced clean coal technology in the USA10.1179/mht.2003.002 ↗
7. Femtosecond laser polishing yttria-stabilized zirconia coatings for improving molten salts corrosion resistance10.1016/j.corsci.2021.109367 ↗
8. A review on molten sulfate salts induced hot corrosion10.1016/j.jmst.2021.03.013 ↗
9. Some aspects of the hot corrosion of thermal barrier coatings10.1007/BF02646315 ↗
10. An investigation on hot corrosion behavior of YSZ-Ta2O5 in Na2SO4+V2O5 salt at 1100°C10.1016/j.corsci.2013.06.025 ↗
11. Comparative investigation on the hot corrosion failure of YSZ and GdYb-YSZ double-ceramic-layer thermal barrier coatings under Na2SO4+V2O5 molten salts10.1016/j.ceramint.2023.02.245 ↗
12. A comparative study on hot corrosion resistance of three types of thermal barrier coatings: YSZ, YSZ+Al2O3 and YSZ/Al2O310.1016/j.msea.2007.06.001 ↗
13. Role of environment deposits and operating surface temperature in spallation of air plasma sprayed thermal barrier coatings10.1016/S0257-8972(96)02994-5 ↗
14. Effect of Al2O3 overlay on hot-corrosion behavior of yttria-stabilized zirconia coating in molten sulfate-vanadate salt10.1016/S0040-6090(03)00670-9 ↗
15. Microscopic observation of degradation behavior in yttria and ceria stabilized zirconia thermal barrier coatings under hot corrosion10.1016/j.surfcoat.2004.04.065 ↗
16. Hot corrosion behavior of dense CYSZ/YSZ bilayer coatings deposited by atmospheric plasma spray in Na2SO4+V2O5 molten salts10.1016/j.surfcoat.2021.128066 ↗
17. Vanadate hot corrosion behavior of India, yttria-stabilized zirconia10.1111/j.1151-2916.1993.tb03995.x ↗
18. Hot corrosion behavior of Sc2O3–Y2O3–ZrO2 thermal barrier coatings in presence of Na2SO4+V2O5 molten salt10.1016/j.corsci.2014.04.001 ↗
19. Phase evolution and hot corrosion behavior of Yb2O3 and CeO2 co-doping YSZ ceramics under high temperature10.1016/j.ceramint.2023.08.103 ↗
20. Hot corrosion evaluation of Gd2O3-Yb2O3 co-doped Y2O3 stabilized ZrO2 thermal barrier oxides exposed to Na2SO4+V2O5 molten salt10.1016/j.ceramint.2016.11.109 ↗
21. Degradation of CeO2 and TiO2 co-stabilized ZrO2 by the V2O5 molten salts and Na2SO4+V2O5 molten salts10.1016/j.surfcoat.2022.128352 ↗
22. Ultraviolet picosecond ultrashort pulsed laser micro glazed EB-PVD YSZ coatings for improving the molten salt (Na2SO4+V2O5) corrosion resistance10.1016/j.surfcoat.2023.129677 ↗
23. Hot corrosion behavior of APS YSZ coatings treated by laser micro glazing (LMG) under molten salts (Na2SO4+V2O5)10.1016/j.corsci.2022.110731 ↗
24. Improving the hot corrosion resistance of plasma sprayed ceria–yttria stabilized zirconia thermal barrier coatings by laser surface treatment10.1016/j.matdes.2013.12.075 ↗
25. Evaluation of laser-glazed plasma-sprayed thermal barrier coatings under high temperature exposure to molten salts10.1016/j.surfcoat.2005.10.011 ↗
26. Hot corrosion behavior of EB-PVD YSZ coatings treated by nanosecond pulsed laser10.1016/j.surfcoat.2022.128889 ↗
27. Microstructure and mechanical properties of yttria stabilized zirconia coatings prepared by plasma spray physical vapor deposition10.1016/j.ceramint.2015.02.141 ↗
28. Influence of microstructure on thermal cycling lifetime and thermal insulation properties of yttria-stabilized zirconia thermal barrier coatings for diesel engine applications10.1016/j.surfcoat.2018.07.005 ↗
29. Low-pressure plasma-induced physical vapor deposition of advanced thermal barrier coatings: microstructures, modelling and mechanisms
30. Comprehensive microstructural characterization and CMAS infiltration resistance of ytterbium disilicate coatings with lamellar and quasi-columnar structures10.1016/j.corsci.2023.111316 ↗
31. Erosion behavior of EB-PVD 7YSZ coatings under corrosion/erosion regime: effect of TBC microstructure and the CMAS chemistry10.1016/j.jeurceramsoc.2018.06.039 ↗
32. The role of the surface morphology and segmented cracks on the damage forms of laser re-melted thermal barrier coatings in presence of a molten salt (Na2SO4+V2O5)10.1016/j.corsci.2016.11.011 ↗
33. Hot corrosion behavior of Al2O3 laser clad plasma sprayed YSZ thermal barrier coatings10.1016/j.ceramint.2016.08.090 ↗
34. Evolution of hot corrosion resistance of YSZ, Gd2Zr2O7, and Gd2Zr2O7+YSZ composite thermal barrier coatings in Na2SO4+V2O5 at 1050°C10.1016/j.jeurceramsoc.2012.01.006 ↗
35. Comparison of the hot corrosion behavior of the LZ, CSZ and LZ/CSZ composite thermal barrier coating10.1016/j.surfcoat.2022.128324 ↗
36. Mechanisms governing the thermal shock and tensile fracture of PS-PVD 7YSZ TBC10.1016/j.ceramint.2017.11.190 ↗
37. Evaluation of hot corrosion behavior of plasma sprayed ceria and yttria stabilized zirconia thermal barrier coatings in the presence of Na2SO4+V2O5 molten salt10.1016/j.ceramint.2012.05.047 ↗
38. Microstructure and mechanical properties of SPS sintered Al2O3–ZrO2(3Y)–SiC ceramic composites10.1016/j.msea.2020.139197 ↗
39. Zirconia (ZrO2) embedded in carbon nanowires via electrospinning for efficient arsenic removal from water combined with DFT studies10.1021/acsami.6b06046 ↗
40. Measurement of the crystallographically transformed zone produced by fracture in ceramics containing tetragonal zirconia10.1111/j.1151-2916.1982.tb10445.x ↗
41. Raman study of yttria-stabilized zirconia interfacial coatings on NicalonTM fiber10.1016/j.jeurceramsoc.2006.04.151 ↗
42. Advanced crystallographic study of the columnar growth of YZS coatings produced by PS-PVD10.1016/j.jeurceramsoc.2017.12.054 ↗
43. Noyan · 2013
44. The influence of laser treatment on hot corrosion behavior of plasma-sprayed nanostructured yttria stabilized zirconia thermal barrier coatings10.1016/j.jeurceramsoc.2014.01.031 ↗
45. Hot corrosion behavior of YSZ, Gd2Zr2O7 and YSZ/Gd2Zr2O7 thermal barrier coatings exposed to molten sulfate and vanadate salt10.1016/j.apsusc.2017.09.047 ↗