Optimization of hatch spacing for improved build rate and high density preservation in laser powder bed fusion of pure titanium
Source abstract
Abstract
This study investigated the optimization of hatch spacing to enhance both the build rate and the density of parts produced by laser powder bed fusion of commercially pure titanium. Employing a multi-layer single track experiment, we derived the average width of melt pools, which adjusted hatch spacing to preserve the density of a part, and we proposed a modified build rate having a quadratic function of scanning speed. Nine process conditions were evaluated with a fixed laser power, while varying hatch spacing and scanning speed, to identify optimal conditions that yield a high density and maximize the build rate. The optimal process condition was a laser power of 310 W, scanning speed of 1943 mm/s, and hatch spacing of 106.7 μm. We confirmed that our process condition derived by a modified build equation could achieve higher build rate with a high density over 99.0% than prior studies. It is expected that this approach can be applied for industries requiring a high productivity of LPBF. • Hatch spacing in laser powder fusion of pure Ti was derived by multi-layer single track experiment and image processing. • Optimization of hatch spacing was performed using modified build rate modeled as a quadratic function of the scanning speed. • The influence of scanning speed and hatch spacing on the microstructures and tensile strength was investigated. • Process condition derived by modified equation achieved higher build rate with density exceeding 99% than previous studies.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Mechanical properties of SLM-printed aluminium alloys
2. Influence of SLM scan-speed on microstructure, precipitation of Al3Sc particles and mechanical properties in Sc- and Zr-modified Al-Mg alloys10.1016/j.matdes.2017.11.053 ↗
3. Effect of scanning strategies on residual stress and mechanical properties of Selective Laser Melted Ti6Al4V10.1016/j.msea.2017.11.103 ↗
4. Integrative technology evaluation model (ITEM) for selective laser melting (SLM)10.4028/www.scientific.net/AMR.337.274 ↗
5. Experimental characterization of SLM and EBM cubic lattice structures for lightweight applications10.1007/s11340-019-00481-8 ↗
6. A lightweight structure redesign method based on selective laser melting10.3390/met6110280 ↗
7. Selective laser melting of soft magnetic alloys for automotive applications, Joint Special Interest Group meeting between euspen and ASPE Advancing Precision
8. Laser metal deposition (LMD) and selective laser melting (SLM) in turbo-engine applications10.1002/latj.201090029 ↗
9. Surface comparison of three different commercial custom-made titanium meshes produced by SLM for dental applications10.3390/ma13092177 ↗
10. Custom-made titanium devices as membranes for bone augmentation in implant treatment: modeling accuracy of titanium products constructed with selective laser melting10.1016/j.jcms.2015.05.006 ↗
11. Is there a Moore's law for 3D printing? 3D Print
12. Selective laser melting of biocompatible metals for rapid manufacturing OF medical parts10.1108/13552540710776142 ↗
13. Surgical and functional outcomes in patients undergoing total knee replacement with patient-specific implants compared with “off-the shelf” implants10.1177/2325967115590379 ↗
14. Direct manufacturing of customized implants from biometals, by 3d printing
15. Additive manufacturing by selective laser melting the realizer desktop machine and its application for the dental industry10.1016/j.phpro.2010.08.082 ↗
16. Reverse effect of hot isostatic pressing on high-speed selective laser melted Ti–6Al–4V alloy10.1016/j.msea.2021.140880 ↗
17. On productivity of laser additive manufacturing10.1016/j.jmatprotec.2018.05.033 ↗
18. Influence of SLM scan-speed on microstructure, precipitation of Al3Sc particles and mechanical properties in Sc- and Zr-modified Al-Mg alloys10.1016/j.matdes.2017.11.053 ↗
19. Influence of energy density on energy demand and porosity of 316L stainless steel fabricated by selective laser melting10.1007/s40684-018-0006-9 ↗
20. Porosity formation mechanisms and fatigue response in Al-Si-Mg alloys made by selective laser melting10.1016/j.msea.2017.11.078 ↗
21. Influence of non-metallic inclusions on fatigue life in the very high cycle fatigue regime10.1016/j.ijfatigue.2015.11.001 ↗
22. Influence of defects on mechanical properties of Ti–6Al–4V components produced by selective laser melting and electron beam melting10.1016/j.matdes.2015.07.147 ↗
23. Improvement of SLM build rate of A357 alloy by optimizing fluence10.1016/j.jmapro.2021.03.043 ↗
24. Selective laser melting of stainless steel 316L with low porosity and high build rates10.1016/j.matdes.2016.05.035 ↗
25. Optimising the process parameters of selective laser melting for the fabrication of Ti6Al4V alloy10.1108/RPJ-03-2016-0045 ↗
26. SLM process parameters effects on the fatigue strength of AMed Inconel 718, Procedia Struct
27. Increasing productivity of laser powder bed fusion manufactured Hastelloy X through modification of process parameters10.1016/j.jmapro.2022.04.013 ↗
28. Selective laser melting10.1002/latj.201290018 ↗
29. Performance of high layer thickness in selective laser melting of Ti6Al4V10.3390/ma9120975 ↗
30. Selective laser melting technology: from the single laser melted track stability to 3D parts of complex shape10.1016/j.phpro.2010.08.083 ↗
31. Comparison of density of stainless steel 316L parts produced with selective laser melting using different powder grades
32. Determination of a process window with consideration of effective layer thickness in SLM process10.1007/s00170-019-04402-w ↗
33. Data analytics approach for melt-pool geometries in metal additive manufacturing10.1080/14686996.2019.1671140 ↗
34. Achieving high ductility in a selectively laser melted commercial pure-titanium via in-situ grain refinement10.1016/j.scriptamat.2020.09.023 ↗
35. Hall-Petch strengthening in nanocrystalline metals10.1016/0921-5093(93)90319-A ↗
36. Manufacture by selective laser melting and mechanical behavior of commercially pure titanium10.1016/j.msea.2013.11.038 ↗
37. Selective laser melting under the reactive atmosphere: a convenient and efficient approach to fabricate ultrahigh strength commercially pure titanium without sacrificing ductility10.1016/j.msea.2019.138078 ↗
38. Effect of laser power on oxygen and nitrogen concentration of commercially pure titanium manufactured by selective laser melting10.1016/j.matchar.2018.03.003 ↗
39. Development and mechanical characterization of porous titanium bone substitutes10.1016/j.jmbbm.2012.01.008 ↗
40. Improvement on mechanical properties and corrosion resistance of titanium-tantalum alloys in-situ fabricated via selective laser melting10.1016/j.jallcom.2019.06.307 ↗
41. Densification behavior, microstructure evolution, and wear performance of selective laser melting processed commercially pure titanium10.1016/j.actamat.2012.04.006 ↗
42. Comparative study of commercially pure titanium produced by laser engineered net shaping, selective laser melting and casting processes10.1016/j.msea.2017.08.103 ↗
43. Fabrication of porous pure titanium via selective laser melting under low-energy-density process conditions10.1016/j.matdes.2020.109035 ↗
44. Laser beam melting process based on complete-melting energy density for commercially pure titanium10.1016/j.jmapro.2019.07.031 ↗
45. Fatigue crack growth rates and tensile strength of titanium produced by means of selective laser melting10.4028/www.scientific.net/KEM.627.305 ↗
46. Efficient predictive model of part distortion and residual stress in selective laser melting